Effect of nano-silica on the efflorescence of waste based alkali-activated inorganic binder
Source abstract
Abstract
Abstract The efflorescence caused by carbonate weathering is one of the dominant causes of deterioration of alkali-activated inorganic materials. In order to inhibit the efflorescence of waste based alkali-activated inorganic binder, the effects of nano -silica on the compressive strength, carbonate ions concentration, hydration rate and pore size distribution of the obtained alkali-activated inorganic binder have been investigated, and the efflorescence inhibition mechanism has been also analyzed. The results revealed that compressive strength and microstructural properties could be further developed with inclusion of nano-silica in alkali-activated inorganic binder. In addition, the efflorescence decreased with increasing nano-silica content and decreasing of the nano-silica particle size. Besides, the hydration rate results indicated that the hydration of waste based alkali-activated inorganic binder was accelerated before hydration for 3d with the incorporation of nano-silica. The suggested inhibition mechanisms discussed were mainly; micro-aggregate filling effect, induced nucleation, and accelerated hydration effects of nano-silica.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete and Cement Materials Research · Magnesium Oxide Properties and Applications · Recycling and utilization of industrial and municipal waste in materials production
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (73)
Show source-provided references
1. GEOPOLYMER Inorganic polymerie new materials10.1007/BF01912193 ↗
2. Utilisation of fly ash in a geopolymeric material10.1016/S0883-2927(02)00005-7 ↗
3. Investigation of early compressive strength of fly ash-based geopolymer concrete10.1016/j.conbuildmat.2016.03.008 ↗
4. Mechanical performance and hydration mechanism of geopolymer composite reinforced by resin10.1016/j.msea.2010.06.069 ↗
5. Strength and drying shrinkage of alkali-activated slag paste and mortar10.1155/2012/579732 ↗
6. Artificial pozzolanic cement pastes containing burnt clay with and without silica fume10.1007/s10973-011-1676-5 ↗
7. Reactivity of dealuminated kaolin and burnt kaolin using cement kiln dust or hydrated lime as activators10.1016/j.conbuildmat.2013.06.078 ↗
8. Freeze–thaw cycle test and damage mechanics models of alkali-activated slag concrete10.1016/j.conbuildmat.2010.12.006 ↗
9. Resistance of alkali-activated slag concrete to acid attack10.1016/S0008-8846(03)00125-X ↗
10. Corrosion resistance of alkali-activated slag cement10.1680/adcr.2003.15.2.77 ↗
11. Properties and durability of alkali-activated slag pastes immersed in sea water10.1016/j.ceramint.2012.01.024 ↗
12. J. Davidovits, 30 Years of Successes and Failures in Geopolymer Applications. Market Trends and Potential Breakthroughs, in: Geopolymer 2002 Conference, 2002, pp. 1–16.
13. H. Ma JY, Y. Ren, F. Ling, Mineral polymer: current developments and prospects, Earth Sci. Front. 9 (2002) 397–407.
14. Geopolymer technology: the current state of the art10.1007/s10853-006-0637-z ↗
15. Multi-scale modeling and experimental investigations of geopolymeric gels at elevated temperatures10.1016/j.compstruc.2013.01.005 ↗
16. Preparation and thermal properties of fire resistant metakaolin-based geopolymer-type coatings10.1016/j.jnoncrysol.2010.09.063 ↗
17. Thermal resistance, microstructure and mechanical properties of type I Portland cement pastes containing low-cost nanoparticles10.1007/s10973-016-5863-2 ↗
18. Influence of carbon nanotubes, nanosilica and nanometakaolin on some morphological-mechanical properties of oil well cement pastes subjected to elevated water curing temperature and regular room air curing temperature10.1016/j.conbuildmat.2017.04.124 ↗
19. Effects of nano-TiO2 on strength, shrinkage and microstructure of alkali activated slag pastes10.1016/j.cemconcomp.2014.11.009 ↗
20. Effect of Carbonation on Alkali-Activated Slag Paste10.1111/j.1551-2916.2006.01214.x ↗
21. Fly ash-based geopolymers: the relationship between composition, pore structure and efflorescence10.1016/j.cemconres.2014.06.004 ↗
22. Effect of nano-SiO2 on the alkali-activated characteristics of metakaolin-based geopolymers10.1016/j.conbuildmat.2013.07.027 ↗
23. The effect of adding nano-SiO2 and nano-Al2O3 on properties of high calcium fly ash geopolymer cured at ambient temperature10.1016/j.matdes.2013.09.049 ↗
24. Effects of nano-SiO2 particles on the mechanical and microstructural properties of ultra-high performance cementitious composites10.1016/j.cemconcomp.2014.11.001 ↗
25. Physico-chemical characterisation of bricks all through the manufacture process in relation to efflorescence salts10.1016/j.jeurceramsoc.2008.11.015 ↗
26. FPG. Calcium carbonate efflorescence on Portland cement and building materials10.1016/S0008-8846(02)00937-7 ↗
27. Efflorescence-mechanism of occurrence and possibilities of prevention
28. Efflorescence control in geopolymer binders based on natural pozzolan10.1016/j.cemconcomp.2011.07.007 ↗
29. Microstructure and properties of fly ash-based geopolymeric material with 5A zeolite as a filler10.1016/j.conbuildmat.2012.01.014 ↗
30. Effects of Si/Al ratio on the structure and properties of metakaolin based geopolymer10.1016/j.ceramint.2016.06.033 ↗
31. Influence of sodium carbonate addition on the thermal reactivity of tungsten mine waste mud based binders10.1016/j.conbuildmat.2009.08.018 ↗
32. High strength geopolymer binder based on waste-glass powder10.1016/j.apt.2016.09.034 ↗
33. A study on the effect of nano silica on compressive strength of high volume fly ash mortars and concretes10.1016/j.matdes.2014.04.025 ↗
34. Effects of nano-silica on the strength development of geopolymer cured at room temperature10.1016/j.conbuildmat.2015.10.044 ↗
35. The effects of TiO2 nanoparticles on physical, thermal and mechanical properties of concrete using ground granulated blast furnace slag as binder10.1016/j.msea.2010.11.070 ↗
36. AF-J. Mineralogical and microstructural characterisation of alkali-activated fly ash slag pastes10.1016/S0958-9465(02)00059-8 ↗
37. The role of SiO2 nanoparticles and ground granulated blast furnace slag admixtures on physical, thermal and mechanical properties of self compacting concrete10.1016/j.msea.2010.11.064 ↗
38. Effects SiO2/Na2O molar ratio on mechanical properties and the microstructure of nano-SiO2 metakaolin-based geopolymers10.1016/j.conbuildmat.2013.12.003 ↗
39. Influence of mixing methods of nano silica on the microstructural and mechanical properties of flax fabric reinforced geopolymer composites10.1016/j.conbuildmat.2016.07.049 ↗
40. Effect of nano-silica on strength and durability of fly ash based geopolymer mortar10.1016/j.conbuildmat.2014.07.093 ↗
41. Silicates
42. Influence of nano-silica agglomeration on microstructure and properties of the hardened cement-based materials10.1016/j.conbuildmat.2012.08.006 ↗
43. The influence of different preparation methods on the aggregation status of pyrogenic nanosilicas used in concrete
44. Effects of colloidal nanoSiO2 on fly ash hydration10.1016/j.cemconcomp.2012.06.013 ↗
45. Effects of colloidal nanosilica on rheological and mechanical properties of fly ash–cement mortar10.1016/j.cemconcomp.2012.08.027 ↗
46. Effects of the pozzolanic reactivity of nanoSiO2 on cement-based materials10.1016/j.cemconcomp.2014.09.014 ↗
47. GB/T 20472–2006: Sulfoaluminate cement
48. Effect of granulated lead smelter slag on strength of fly ash-based geopolymer concrete10.1016/j.conbuildmat.2015.03.009 ↗
49. Efflorescence pathway diagram: understanding salt weathering10.1016/j.conbuildmat.2004.02.003 ↗
50. Influence of limestone and slag on the pore structure of cement paste based on mercury intrusion porosimetry and water vapour sorption measurements10.1016/j.conbuildmat.2013.11.022 ↗
51. Estimation of Water Retention Curve from Mercury Intrusion Porosimetry and van Genuchten Model
52. Use of analytical techniques for identification of inorganic polymer gel composition10.1007/s10853-010-4257-2 ↗
53. Effect of nano-clay on alkali activated water-cooled slag geopolymer10.9734/BJAST/2013/2690 ↗
54. The effects of nanoparticles on early age compressive strength of ash-based geopolymers10.1016/j.ceramint.2012.02.021 ↗
55. A comprehensive overview about the effect of nano-SiO2 on some properties of traditional cementitious materials and alkali-activated fly ash10.1016/j.conbuildmat.2013.10.101 ↗
56. Kinetics of geopolymerization: role of Al2O3 and SiO210.1016/j.cemconres.2007.01.003 ↗
57. Medium-term phase stability of Na2O–Al2O3–SiO2–H2O geopolymer systems10.1016/j.cemconres.2007.10.003 ↗
58. The role of Al2O3, SiO2 and Na2O on the amorphous crystalline phase transformation in geopolymer systems
59. Role of water in the synthesis of calcined kaolin-based geopolymer10.1016/j.clay.2008.09.003 ↗
60. Composite geopolymers of metakaolin and geothermal nanosilica waste10.1016/j.conbuildmat.2016.03.002 ↗
61. Z. Wu HL, High Performance Concrete, China Railway Press, Beijing, 1999.
62. Experimental study of XRD, FTIR and TGA techniques in geopolymeric materials
63. Factors affecting the performance of metakaolin geopolymers exposed to elevated temperatures10.1007/s10853-007-2205-6 ↗
64. A comprehensive overview about the influence of different additives on the properties of alkali-activated slag – A guide for Civil Engineer10.1016/j.conbuildmat.2013.04.011 ↗
65. Fresh and hardened properties of alkali-activated fly ash/slag pastes with superplasticizers10.1016/j.conbuildmat.2013.09.048 ↗
66. Z. Lin, Inorganic Metalloid Materials Technics, third ed., Wuhan University of Technology Press, 2008.
67. Effects of colloidal nanoBoehmite and nanoSiO2 on fly ash cement hydration10.1016/j.conbuildmat.2015.10.038 ↗
68. Dissolution processes, hydrolysis and condensation reactions during geopolymer synthesis: Part I—Low Si/Al ratio systems10.1007/s10853-006-0820-2 ↗
69. 29Si and 27Al MAS-NMR of NaOH-Activated Blast-Furnace Slag10.1111/j.1151-2916.1994.tb04606.x ↗
70. Studies on early stage hydration of tricalcium silicate incorporating silica nanoparticles: part I10.1016/j.conbuildmat.2014.08.046 ↗
71. Effects of nano-limestone on hydration properties of tricalcium silicate10.1007/s10973-017-6123-9 ↗
72. Utilization of carbonated and granulated steel slag aggregate in concrete10.1016/j.conbuildmat.2015.03.008 ↗
73. Microstructure, strength, and reaction products of ground granulated blast-furnace slag activated by highly concentrated NaOH solution10.1557/JMR.1994.0188 ↗