Effect of soda-lime glass powder on alkali-activated binders: Rheology, strength and microstructure characterization
Source abstract
Abstract
Abstract Alkali-activated binders (AABs) have the potential to consume various types of cementitious waste materials, including coal ashes, municipal solid waste incinerator ash, palm-oil fuel ash, steel slags, mine tailings, cement kiln dust, ceramic tile residue, rice husk ash, and waste glass. This paper presents a study of alkali-activated cement paste produced with the substitution of the cementitious waste material soda-lime glass, which makes up the major proportion of the general glass waste stream. In the alkali-activated cement paste, crushed soda-lime glass powder (CG) was used as a replacement for class F fly ash (FA) from 0 to 30% by total solid weight, keeping the ground granulated blast furnace slag (GGBFS) content constant at 50%. The influence of activator molarity (4–8 M), alkaline liquid/solid binder (L/S) ratio (0.4–0.5) and different curing conditions (ambient air curing, wet curing, and short-term heat curing) on the rheology, strength, and microstructure of CG-substituted AABs was investigated and optimum conditions are suggested. According to the experimental results, both the workability and strength (compressive and tensile) of the AAB gradually increased with increasing level of substitution of FA by CG. Significant improvement in flow and setting time was seen with the addition of CG, even in mixtures with a low L/S ratio of 0.4. Both ambient and wet curing had more influence on the strength gain of AABs, especially after 28 days. Short-term heat curing resulted in high early strength gain. The dissolution of CG increased with increasing molarity (from 4 to 8 M) of the alkaline solution, which improved both strength and microstructure with curing time. Morphological and elemental analysis indicated an improvement of the microstructure of AABs due to the increased formation of calcium-dominant hydration products and hence reduced porosity with the substitution of CG. However, undissolved large-sized CG particles agglomerated in the binder without participating in the alkaline reactions. These agglomerated particles may induce micro-cracks due to weak bonding between the cement matrix and the smooth CG interface, which reduces the durability of AABs. Therefore, the inclusion of waste soda-lime glass powder with a mean diameter of 10–15 µm as a precursor in FA/GGBFS-based AAB as a replacement for FA is feasible and provides a good solution for waste material recycling.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete and Cement Materials Research · Magnesium Oxide Properties and Applications · Innovative concrete reinforcement materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (48)
Show source-provided references
1. Utilization of cement kiln dust (CKD) to enhance mine tailings-based geopolymer bricks10.1016/j.conbuildmat.2012.11.069 ↗
2. Development of geopolymer mortar under ambient temperature for in situ applications10.1016/j.conbuildmat.2016.05.085 ↗
3. Glass waste as supplementary cementing materials: The effects of glass chemical composition10.1016/j.cemconcomp.2014.07.020 ↗
4. Geopolymer cement: A review
5. Physico-chemical and mechanical characterization of high volume fly ash incorporated and engineered cement system towards developing greener cement10.1016/j.jclepro.2016.03.118 ↗
6. The influence of curing methods on the strength of MSWI bottom ash-based alkali-activated mortars: The role of leaching of OH− and free alkali10.1016/j.conbuildmat.2018.07.224 ↗
7. Effect of metakaolin replaced granulated blast furnace slag on fresh and early strength properties of geopolymer mortar10.1016/j.asej.2016.11.011 ↗
8. Influence of different curing temperatures and alkali activators on properties of GBFS geopolymer mortars containing fly ash and palm-oil fuel ash10.1016/j.conbuildmat.2016.08.153 ↗
9. Properties of ceramic tile waste based alkali-activated mortars incorporating GBFS and fly ash10.1016/j.conbuildmat.2019.04.154 ↗
10. Quantification of thermally-induced microcracks in granite using X-ray CT imaging and analysis10.1016/j.geothermics.2019.04.007 ↗
11. Waste glass powder as partial replacement of cement for sustainable concrete practice10.1016/j.ijsbe.2016.10.005 ↗
12. Waste glass in the production of cement and concrete–A review10.1016/j.jece.2014.03.016 ↗
13. Preparation conditions for the synthesis of alkali-activated binders using tungsten mining waste10.1061/(ASCE)MT.1943-5533.0002029 ↗
14. Performance evaluation of concrete incorporating glass powder and glass sludge wastes as supplementary cementing material10.1016/j.jclepro.2017.09.133 ↗
15. Management and recycling of waste glass in concrete products: Current situations in Hong Kong10.1016/j.resconrec.2012.10.006 ↗
16. An overview on the reuse of waste glasses in alkali-activated materials10.1016/j.resconrec.2019.02.007 ↗
17. Fresh properties of cement pastes or mortars incorporating waste glass powder and cullet10.1016/j.conbuildmat.2016.11.011 ↗
18. Use of waste glass in alkali activated cement mortar10.1016/j.conbuildmat.2017.11.080 ↗
19. Utilisation of alkali activated glass powder in binary mixtures with Portland cement, slag, fly ash and hydrated lime10.1617/s11527-016-0922-5 ↗
20. Geopolymer as well cement and the variation of its mechanical behavior with curing temperature10.1002/ghg.39 ↗
21. Geopolymer as well cement and its mechanical integrity under deep down-hole stress conditions: application for carbon capture and storage wells10.1007/s40948-016-0034-2 ↗
22. Effect of GGBFS on setting, workability and early strength properties of fly ash geopolymer concrete cured in ambient condition10.1016/j.conbuildmat.2014.05.080 ↗
23. Effect of different superplasticizers and activator combinations on workability and strength of fly ash based geopolymer10.1016/j.matdes.2014.01.064 ↗
24. Waste glass from end-of-life fluorescent lamps as raw material in geopolymers10.1016/j.wasman.2016.04.003 ↗
25. Olivier · 2013
26. Influence of curing conditions on properties of high calcium fly ash geopolymer containing Portland cement as additive10.1016/j.matdes.2013.07.018 ↗
27. Effects of sodium hydroxide and sodium silicate solutions on compressive and shear bond strengths of FA–GBFS geopolymer10.1016/j.conbuildmat.2015.05.001 ↗
28. Use of glass waste as an activator in the preparation of alkali-activated slag. Mechanical strength and paste characterisation10.1016/j.cemconres.2013.12.005 ↗
29. Recent advances in alkaline cement binders: A review10.1016/j.jclepro.2019.04.103 ↗
30. Geopolymers obtained from bottom ash as source of aluminosilicate cured at room temperature10.1016/j.conbuildmat.2017.09.111 ↗
31. A review on the use of waste glasses in the production of cement and concrete10.1016/j.resconrec.2007.01.013 ↗
32. Utilization of municipal solid waste (MSW) ash in cement and mortar10.1016/j.resconrec.2010.05.002 ↗
33. Comparison of metakaolin-based geopolymer cements from commercial sodium waterglass and sodium waterglass from rice husk ash10.1007/s10971-016-3983-6 ↗
34. Geopolymer binders from metakaolin using sodium waterglass from waste glass and rice husk ash as alternative activators: A comparative study10.1016/j.conbuildmat.2016.03.184 ↗
35. Effect of mechanical activation of fly ash on the properties of geopolymer cured at ambient temperature10.1016/j.jmatprotec.2009.03.016 ↗
36. Compressive strength and microstructure analysis of geopolymer paste using waste glass powder and fly ash10.1016/j.jclepro.2017.11.125 ↗
37. Use of Vietnamese rice husk ash for the production of sodium silicate as the activator for alkali-activated binders10.1016/j.jclepro.2018.08.025 ↗
38. Fly ash-based geopolymers containing added silicate waste10.1016/j.ceramint.2017.07.221 ↗
39. Extensive reuse of soda-lime waste glass in fly ash-based geopolymers10.1016/j.conbuildmat.2018.08.096 ↗
40. Waste glass in the geopolymer preparation. Mechanical and microstructural characterisation10.1016/j.jclepro.2014.11.074 ↗
41. Technical and environmental performance of lower carbon footprint cement mortars containing biomass fly ash as a secondary cementitious material10.1016/j.resconrec.2018.03.004 ↗
42. Carbon dioxide equivalent (CO2-e) emissions: A comparison between geopolymer and OPC cement concrete10.1016/j.conbuildmat.2013.01.023 ↗
43. Production of sodium silicate powder from waste glass cullet for alkali activation of alternative binders10.1016/j.cemconres.2018.11.008 ↗
44. Upcycling of waste materials: Green binder prepared with pure coal fly ash10.1061/(ASCE)MT.1943-5533.0001414 ↗
45. Synthesis factors affecting mechanical properties, microstructure, and chemical composition of red mud–fly ash based geopolymers10.1016/j.fuel.2014.05.058 ↗
46. Waste glass as partial mineral precursor in alkali-activated slag/fly ash system10.1016/j.cemconres.2017.08.012 ↗
47. Effectiveness of novel and traditional methods to incorporate industrial wastes in cementitious materials—An overview10.1016/j.resconrec.2013.03.003 ↗
48. Conversion of local industrial wastes into greener cement through geopolymer technology: a case study of high-magnesium nickel slag10.1016/j.jclepro.2016.09.147 ↗