Abstract

Abstract This paper investigated the potential of using reactive MgO-activated ground granulated blastfurnace slag (MgO-GGBS) as a binder in cemented paste backfill (CPB) from sulphide-rich tailings. The effects of reactive MgO content of MgO-GGBS on the unconfined compressive strength (UCS) of CPB were investigated. The test results showed that the CPB achieved target strength (≧1.0 MPa) at 28 d and the UCS at 360 d showed an increasing trend when MgO-GGBS dosage was 14 wt% and reactive MgO content of MgO-GGBS was 2.5–7.5 wt%. Thermodynamic calculations and analyses of potential reactions including acid and sulphate attack have been performed. The hydration products were identified by X-ray diffraction (XRD) and thermogravimetry analysis (TG/DTG). Finally, the hydration mechanism of CPB was discussed based on the thermodynamic and experimental results. The conclusion is that MgO-GGBS will be a promising binder for tailings with sulphide.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Tailings Management and Properties · Mine drainage and remediation techniques · Mining and Resource Management

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Modern mining ideas and filling g mining
2. Geochemical study of heavy metal pollution in mine-river system
3. Zhou · 2007
4. Distribution of heavy metals in water-surface sediments in AMD, Dabao Mountain in North Guangdong Province and influential factors
5. A review on heavy metal pollution in basins near the Dabao Mountain Mining Area
6. Ranking and scoring potential environmental risks from solid mineral wastes10.1016/j.mineng.2009.09.008 ↗
7. Geotechnical properties of cemented paste backfill from Cannington Mine, Australia10.1007/s10706-006-9104-5 ↗
8. Integrated mine tailings management by combining environmental desulphurization and cemented paste backfill: application to mine Doyon, Quebec, Canada10.1016/j.mineng.2007.11.012 ↗
9. Pipe lining abrasion testing for paste backfill operations10.1016/j.mineng.2009.03.010 ↗
10. Cementitious backfill with high sulfur content: physical, chemical, and mineralogical characterization10.1016/S0008-8846(99)00023-X ↗
11. Evaluation of paste backfill mixtures consisting of sulphide-rich mill tailings and varying cement contents10.1016/j.cemconres.2004.01.018 ↗
12. Effect of properties of tailings and binder on the short and long-term strength and stability of cemented paste backfill10.1016/j.matlet.2005.06.042 ↗
13. Effect of tailings properties on paste backfill performance
14. Utilization of industrial waste products as pozzolanic material in cemented paste backfill of high sulphide mill tailings10.1016/j.jhazmat.2009.02.100 ↗
15. Cemented paste backfill of sulphide-rich tailings: Importance of binder type and dosage10.1016/j.cemconcomp.2009.01.008 ↗
16. Utilization of water-reducing admixtures in cemented paste backfill of sulphide-rich mill tailings10.1016/j.jhazmat.2010.03.096 ↗
17. Effect of natural pozzolans as mineral admixture on the performance of cemented-paste backfill of sulphide-rich tailings10.1177/0734242X09351905 ↗
18. Effect of desliming of sulphide-rich mill tailings on the long-term strength of cemented paste backfill10.1016/j.jenvman.2012.11.014 ↗
19. Utilization of granulated marble wastes and waste bricks as mineral admixture in cemented paste backfill of sulphide-rich tailings10.1016/j.conbuildmat.2015.06.042 ↗
20. Developing durable paste backfill from sulphidic tailings
21. Utilization of limestone powder and water-reducing admixture in cemented paste backfill of coarse copper mine tailings10.1016/j.conbuildmat.2016.07.055 ↗
22. Study on the strength development of cemented backfill body from lead-zinc mine tailings with sulphide
23. Effect of acid rain pH on leaching behavior of cement stabilized lead-contaminated soil10.1016/j.jhazmat.2014.02.002 ↗
24. Durability of lightweight alkali-activated ground granulated blast furnace slag (GGBS) stabilized clayey soils subjected to sulfate attack10.1016/j.clay.2018.04.014 ↗
25. Experimental investigation of influence of acid rain on leaching and hydraulic characteristics of cement-based solidified/stabilized lead contaminated clay10.1016/j.jhazmat.2012.04.072 ↗
26. A review: The comparison between alkali-activated slag (Si + Ca) and metakaolin (Si + Al) cements10.1016/j.cemconres.2010.03.020 ↗
27. Utilisation of alkali-activated blast furnace slag in paste backfill of high-sulphide mill tailings: Effect of binder type and dosage10.1016/j.mineng.2012.01.009 ↗
28. Paste backfill of high-sulphide mill tailings using alkali-activated blast furnace slag: Effect of activator nature, concentration and slag properties10.1016/j.mineng.2015.08.022 ↗
29. Effect of sodium-silicate activated slag at different silicate modulus on the strength and microstructural properties of full and coarse sulphidic tailings paste backfill10.1016/j.conbuildmat.2018.07.105 ↗
30. Strength and hydration properties of reactive MgO-activated ground granulated blastfurnace slag paste10.1016/j.cemconcomp.2014.10.007 ↗
31. J.R. Zheng, S.S. Lv, Z.B. Zhao, Method for determination of fluidity of paste slurry of whole tailings, Mining Technol. 13(5) 23–25. DOI: 10.13828/j.cnki.ckjs.2013.05.055 (in Chinese).
32. Thermodynamics and cement science10.1016/j.cemconres.2011.03.018 ↗
33. Lin · 1985
34. Thermodynamic modelling of the hydration of Portland cement10.1016/j.cemconres.2005.03.001 ↗
35. Modeling of pyrite oxidation in saturated and unsaturated subsurface flow systems10.1023/A:1006518725360 ↗
36. Temperature and common-ion effect on magnesium oxide (MgO) hydration10.1016/j.ceramint.2009.12.009 ↗
37. Effects of dosage and modulus of water glass on early hydration of alkali–slag cements10.1016/S0008-8846(01)00717-7 ↗
38. Influence of slag chemistry on the hydration of alkali-activated blast-furnace slag-part 1: effect of MgO10.1016/j.cemconres.2011.05.002 ↗
39. Synthesis and characterisation of magnesium silicate hydrate gels10.1016/j.cemconres.2004.06.022 ↗
40. Factors affecting the strength of alkali-activated slag10.1016/0008-8846(94)90026-4 ↗
41. Hydration of alkali-activated ground granulated blast furnace slag10.1023/A:1004742027117 ↗