Relation between activator ratio, hydration products and mechanical properties of alkali-activated slag
Source abstract
Abstract
The use of cement substitute, such as alkali-activated slag, is of great interest in the field of earth-based construction materials to preserve their environmental benefit. Nonetheless, the cationic activity of clayey particles of earth-based materials induces new issues by affecting the alkaline conditions in which slag is activated. This work aims to present how alkaline conditions modify the nature and the amount of hydrates formed, the kinetics for reaction and the resulting mechanical properties. A minimum of 5 wt.% of activator with respect to the slag was needed to trigger consolidation of the samples within the first 24 hours, while an activator content of 15% led to an excess of sodium, especially remarkable at early age. Besides, hydration kinetics were followed in situ during the first 3 days by infrared spectroscopy. The formation of portlandite and hydrotalcite-like hydrates were only observable from 10% of activator and the presence of hydrotalcite is correlated with an increase in mechanical properties. Finally, these results are of interest for the formulation of earth-based materials by predicting hydrated phases formed during slag activation depending on alkaline conditions.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete and Cement Materials Research · Recycling and utilization of industrial and municipal waste in materials production · Magnesium Oxide Properties and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (82)
Show source-provided references
1. F. Pacheco-Torgal, Z. Abdollahnejad, A.F. Camões, M. Jamshidi, Y. Ding, Durability of alkali-activated binders: A clear advantage over Portland cement or an unproven issue?, 30 (2012) 400–405. https://doi.org/10.1016/j.conbuildmat.2011.12.017.10.1016/j.conbuildmat.2011.12.017 ↗
2. Can Portland cement be replaced by low-carbon alternative materials? A study on the thermal properties and carbon emissions of innovative cements10.1016/j.jclepro.2018.02.138 ↗
3. Alexandre · 1988
4. The development of alkali-activated mixtures for soil stabilisation
5. Stabilisation of clayey soils with industrial by-products: Part B
6. Pozzolanic consolidation of stabilized soft clays10.1016/j.clay.2014.03.020 ↗
7. Properties of ion leaching of alkali-activated blast furnace slag at early hydration10.1680/jadcr.15.00073 ↗
8. A. Gruskovnjak, Hydration mechanisms of activated blast furnace slag, Berne, Suisse, 2006. https://www.dora.lib4ri.ch/empa/islandora/object/empa%3A12253/datastream/PDF/view (accessed May 13, 2019).
9. Mécanisme de la prise du laitier granulé sous activation alcaline, Laboratoire des Ponts et Chaussées
10. Effect of activator mix on the hydration and strength behaviour of alkali-activated slag cements10.1680/adcr.2003.15.3.129 ↗
11. Impact of chemical variability of ground granulated blast-furnace slag on the phase formation in alkali-activated slag pastes10.1016/j.cemconres.2016.09.003 ↗
12. S. Wang, X. Pu, K.L. Scrivener, P.L. Pratt, Alkali-activated slag cement and concrete : a review of properties and problems, (1995) 93–102.10.1680/adcr.1995.7.27.93 ↗
13. Thermodynamic modelling of alkali-activated slag cements10.1016/j.apgeochem.2015.06.006 ↗
14. Influence of slag chemistry on the hydration of alkali-activated blast-furnace slag — Part I: Effect of MgO10.1016/j.cemconres.2011.05.002 ↗
15. Influence of slag chemistry on the hydration of alkali-activated blast-furnace slag — Part II: Effect of Al2O310.1016/j.cemconres.2011.08.005 ↗
16. The characterization of hardened alkali-activated blast-furnace slag pastes and the nature of the calcium silicate hydrate (C-S-H) phase10.1016/0008-8846(94)90002-7 ↗
17. Very early-age reaction kinetics and microstructural development in alkali-activated slag10.1016/j.cemconcomp.2014.09.001 ↗
18. Hydration and properties of sodium sulfate activated slag10.1016/j.cemconcomp.2012.12.010 ↗
19. S.-D. Wang, K.L. Scrivener, P.L. Pratt, Factors Affecting the Strength of Alkali-Activated Slag, Cem. Concr. Res. 24 (1994) 1033–1043. https://api-istex-fr.docelec.insa-lyon.fr/document/FFA64EE047DDAE2185FB5D20293A7165B4BB547B/fulltext/pdf?auth=ip,fede&sid=ebsco,istex-view (accessed December 20, 2018).10.1016/0008-8846(94)90026-4 ↗
20. Alkali-activated slag mortars Mechanical strength behaviour10.1016/S0008-8846(99)00154-4 ↗
21. Pacheco-Torgal · 2015
22. Hydration of alkali-activated slag: thermodynamic modelling10.1680/adcr.2007.19.2.81 ↗
23. Phase diagrams for alkali-activated slag binders10.1016/j.cemconres.2017.02.006 ↗
24. MgO content of slag controls phase evolution and structural changes induced by accelerated carbonation in alkali-activated binders10.1016/j.cemconres.2013.12.003 ↗
25. Effect of slag chemistry on the hydration of alkali-activated blast-furnace slag10.1617/s11527-014-0461-x ↗
26. Houzé · 2013
27. Early stage dissolution characteristics of aluminosilicate glasses with blast furnace slag-and fly-ash-like compositions10.1111/jace.14716 ↗
28. Etude de la réactivité des ciments riches en laitier, à basse température et à temps court, sans ajout chloruré
29. Activation of blast furnace slag by a new method10.1016/j.cemconres.2009.05.012 ↗
30. Hydration of Alkali Activated Slag : Comparison with Ordinary Portland Cement10.1680/adcr.2006.18.3.119 ↗
31. Influence of activator type on hydration kinetics, hydrate assemblage and microstructural development of alkali activated blast-furnace slags10.1016/j.cemconres.2010.11.016 ↗
32. Structure of Calcium Silicate Hydrates Formed in Alkaline-Activated Slag: Influence of the Type of Alkaline Activator10.1111/j.1151-2916.2003.tb03481.x ↗
33. An environmental evaluation of geopolymer based concrete production: Reviewing current research trends10.1016/j.jclepro.2011.03.012 ↗
34. M. Weil, K. Dombrowski, A. Buchwald, Life-cycle analysis of geopolymers, in: J.L. Provis, J.S.J.B.T.-G. van Deventer (Eds.), Geopolymers. Struct. Process. Prop. Ind. Appl., Woodhead Publishing Series in Civil and Structural Engineering, Cambridge, UK, 2009: pp. 194–210. https://doi.org/https://doi.org/10.1533/9781845696382.2.194.10.1533/9781845696382.2.194 ↗
35. I. Garcia-Lodeiro, A. Palomo, A. Fernández-Jiménez, Crucial insights on the mix design of alkali-activated cement-based binders, in: Handb. Alkali-Activated Cem. Mortars Concr., Elsevier Inc., 2014: pp. 49–73. https://doi.org/10.1533/9781782422884.1.49.10.1533/9781782422884.1.49 ↗
36. Properties of cementless mortars activated by sodium silicate10.1016/j.conbuildmat.2007.07.003 ↗
37. Effects of dosage of alkali-activated solution and curing conditions on the properties and durability of alkali-activated slag concrete10.1016/j.conbuildmat.2012.04.005 ↗
38. S.-D. Wang, K.L. Scrivener, Hydration Products of Alkali Activated Slag Cement, Cem. End Concr. Res. 25 (1995) 561–571. https://api-istex-fr.docelec.insa-lyon.fr/document/31C4FFC95DF244378C520D09D9738551159626E5/fulltext/pdf?auth=ip,fede&sid=ebsco (accessed October 12, 2017).10.1016/0008-8846(95)00045-E ↗
39. A model for the C-A-S-H gel formed in alkali-activated slag cements10.1016/j.jeurceramsoc.2011.04.036 ↗
40. R. Fernández, E. Torres, A.I. Ruiz, J. Cuevas, M. Cruz Alonso, J. Luis García Calvo, E. Rodríguez, M. Jesús Turrero, Interaction processes at the concrete-bentonite interface after 13 years of FEBEX-Plug operation. Part II: Bentonite contact, Phys. Chem. Earth. 99 (2017) 49–63. https://doi.org/10.1016/j.pce.2017.01.009.10.1016/j.pce.2017.01.009 ↗
41. C. Shi, R.L. Day, A Calorimetric Study of Early Hydration of Alkali-Sag Cements, Cem. Connete Res. 25 (1995) 1333–1346. https://api-istex-fr.docelec.insa-lyon.fr/document/C4768A62F7F1B411A20A4CD6DF8202B1992A6C4A/fulltext/pdf?auth=ip,fede&sid=ebsco (accessed October 12, 2017).10.1016/0008-8846(95)00126-W ↗
42. Infrared Spectra and Characteristic Frequencies of Inorganic Ions Their Use in Qualitative Analysis10.1021/ac60068a007 ↗
43. H. Wijnja, C.P. Schulthess, ATR-FTIR and DRIFT spectroscopy of carbonate species at the aged k-Al 2 O 3 /water interface, Spectrochim. Acta Part A. 55 (1999) 861–872. https://api-istex-fr.docelec.insa-lyon.fr/ark:/67375/6H6-W2250PT4-Z/fulltext.pdf?auth=ip,fede&sid=ebsco,istex-view (accessed June 6, 2019).10.1016/S1386-1425(98)00236-4 ↗
44. M.A. Trezza, A.E. Lavat, Analysis of the system 3CaO.Al2O3 - CaSO4.2H2O - CaCO3 - H2O by FT-IR spectroscopy, Cem. Concr. Res. 31 (2001) 869–872. https://api-istex-fr.docelec.insa-lyon.fr/ark:/67375/6H6-0TRL2L4V-4/fulltext.pdf?auth=ip,fede&sid=ebsco,istex-view (accessed September 2, 2019).10.1016/S0008-8846(01)00502-6 ↗
45. Early hydration and setting of Portland cement monitored by IR, SEM and Vicat techniques10.1016/j.cemconres.2009.01.017 ↗
46. M. Horgnies, J.J. Chen, C. Bouillon, Overview about the use of Fourier Transform Infrared spectroscopy to study cementitious materials, in: C.A. Brebbia, A. Klemm (Eds.), Mater. Characterisation VI. Comput. Methods Exp., WIT Press, Southampton, U.K, 2013: p. 364. https://doi.org/10.2495/MC130221.10.2495/MC130221 ↗
47. FTIR analysis of water structure and its significance in the flotation of sodium carbonate and sodium bicarbonate salts10.1016/S0927-7757(03)00317-0 ↗
48. K. Nakamoto, M. Margoshes, R.E. Rundlb Yol, B. Kazuo Nakamoto, R.E. Rundle, N. Cl, Stretching Frequencies as a Function of Distances in Hydrogen Bonds, J. Am. Chem. Soc. 77 (1955) 6480–86. https://pubs.acs.org/sharingguidelines (accessed September 2, 2019).10.1021/ja01629a013 ↗
49. Coupled thermodynamic modelling and experimental study of sodium hydroxide activated slag10.1016/j.conbuildmat.2018.08.087 ↗
50. FT-Raman and FT-IR spectroscopic study of synthetic Mg/Zn/Al-hydrotalcites10.1002/jrs.1244 ↗
51. Incorporation of Al in C-A-S-H gels with various Ca/Si and Al/Si ratio: Microstructural and structural characteristics with DTA/TG, XRD, FTIR and TEM analysis10.1016/j.conbuildmat.2017.08.091 ↗
52. Structure of Calcium Silicate Hydrate (C-S-H): Near-, Mid-, and Far-Infrared Spectroscopy10.1111/j.1151-2916.1999.tb01826.x ↗
53. A. Gmira, Etude structurale et thermodynamique d’hydrates modèles du ciment, Université d’Orléans, 2003. https://tel.archives-ouvertes.fr/tel-00006001/document (accessed May 18, 2018).
54. Effect of alkalis on fresh C-S–H gels. FTIR analysis10.1016/j.cemconres.2009.01.003 ↗
55. Analysis of Slag Chemistry by FTIR-RAS and Raman Spectroscopy: Effect of Water Vapor Content in H 2 –H 2 O-CO–CO 2 Mixtures Relevant to a Novel Green Ironmaking Technology10.1002/srin.201400186 ↗
56. C. Kedziora, Propriétés d’usage et mécanismes d’hydratation du système ternaire [Ciment Alumineux – Sulfate de Calcium – Laitier de Haut Fourneau] à haute teneur en sulfate de calcium : de l’approche expérimentale à la modélisation, Institut National des Sciences Appliquées de Lyon, 2015. http://theses.insa-lyon.fr/publication/2015ISAL0047/these.pdf (accessed April 24, 2019).
57. Phase evolution of C-(N)-A-S-H/N-A-S-H gel blends investigated via alkali-activation of synthetic calcium aluminosilicate precursors10.1016/j.cemconres.2016.08.010 ↗
58. Evaluation of slag characteristics on the reaction kinetics and mechanical properties of Na2CO3 activated slag10.1016/j.conbuildmat.2016.11.074 ↗
59. E. L ’hôpital, B. Lothenbach, K. Scrivener, D.A. Kulik, E. L’Hôpital, B. Lothenbach, K. Scrivener, D.A. Kulik, E. L ’hôpital, B. Lothenbach, K. Scrivener, D.A. Kulik, Alkali uptake in calcium alumina silicate hydrate (C-A-S-H), Cem. Concr. Res. 85 (2016) 122–136. https://doi.org/10.1016/j.cemconres.2016.03.009.10.1016/j.cemconres.2016.03.009 ↗
60. (Micro)-structural comparison between geopolymers, alkali-activated slag cement and Portland cement10.1016/j.jeurceramsoc.2005.12.021 ↗
61. Handbook of thermal analysis of construction materials, William Andrew Publishing, Norwich, New, York
62. Thermal stability of C-S-H phases and applicability of Richardson and Groves’ and Richardson C-(A)-S-H(I) models to synthetic C-S-H10.1016/j.cemconres.2016.12.005 ↗
63. X-ray diffraction : a powerful tool to probe and understand the structure of nanocrystalline calcium silicate hydrates10.1107/S2052519213021155 ↗
64. The evolution of strength and crystalline phases for alkali-activated ground blast furnace slag and fly ash-based geopolymers10.1016/j.cemconres.2009.10.010 ↗
65. The role of Al in cross-linking of alkali-activated slag cements10.1111/jace.13360 ↗
66. The role of Al in C-S-H: NMR, XRD, and compositional results for precipitated samples10.1016/j.cemconres.2005.03.002 ↗
67. Crystal structures of calcium hemicarboaluminate and carbonated calcium hemicarboaluminate from synchrotron powder diffraction data10.1107/S010876811203042X ↗
68. Crystal Chemistry of Iron Containing Cementitious AFm Layered Hydrates10.2174/1877944105666150420235831 ↗
69. Use of CaO as an activator for producing a price-competitive non-cement structural binder using ground granulated blast furnace slag10.1016/j.cemconres.2013.09.011 ↗
70. Differential scanning calorimetry study of the hydration products in portland cement pastes with metakaolin replacement
71. Structural evolution of an alkali sulfate activated slag cement10.1016/j.jnucmat.2015.11.016 ↗
72. 27AI and 25Mg Solid-state Magic-angle Spinning Nuclear Magnetic Resonance Study of Hydrotalcite and its Thermal Decomposition Sequence10.1039/jm9930301263 ↗
73. Wilkinson · Stabilisation of clayey soils with industrial by-products: part A · 2010 · 3 · 149
74. Jolivet · 1994
75. Iler · 1979
76. I.G. Richardson, The nature of C-S-H in hardened cements, 1999. https://api-istex-fr.docelec.insa-lyon.fr/ark:/67375/6H6-3KRV35PR-T/fulltext.pdf?auth=ip,fede&sid=ebsco,istex-view (accessed April 26, 2019).
77. S.A. Bernal, R. San Nicolas, J.S. J van Deventer, J.L. Provis Professor, Alkali-activated slag cements produced with a blended sodium carbonate/sodium silicate activator, (n.d.). https://doi.org/10.1680/jadcr.15.00013.10.1680/jadcr.15.00013 ↗
78. A thermodynamic model for C-(N-)A-S-H gel: CNASH_ss. Derivation and validation10.1016/j.cemconres.2014.07.005 ↗
79. The System Na20-Ca0-SiOrH2010.1111/j.1151-2916.1990.tb06475.x ↗
80. Calcium silicate hydrates: Solid and liquid phase composition10.1016/j.cemconres.2015.03.019 ↗
81. Myers · 2015
82. Nanoscale Charge-Balancing Mechanism in Alkali-Substituted Calcium–Silicate–Hydrate Gels10.1021/acs.jpclett.6b02233 ↗