Durability study of AAMs: Sulfate attack resistance
Source abstract
Abstract
Abstract This paper is a part of works intended to determine more appropriate durability test methods for alkali activated materials (AAMs). Indeed, the current methods used to characterize durability of AAMs are those initially developed for ordinary Portland cement (OPC) and blended OPC. As the chemistry that governs both AAMs and OPC systems is completely different, using OPC durability methods for AAMs could induce inaccurate results. This work aims to study sulfate resistance of alkali activated slag (AAS), alkali activated fly ash (AAFA) and OPC (used as reference) to propose appropriate sulfate resistance test for AAMs by using ASTM C1012 as a basis. Both temperature of curing and sodium sulfate concentration were studied. Expansion of samples was evaluated over time. Results showed that all the OPC bars exceeded the limit compliance with less expansion for those precured at 35 °C. The expansion was attributed in all cases to gypsum and ettringite formation. AAS samples underwent expansion that remains below the limit compliance. At high curing temperature, an initial high expansion attributed to water absorption by the formed porosity was observed. For AAFA systems, no expansion was detected whatever the curing regime and the sulfate concentration, showing a great resistance of such systems to sodium sulfate attack.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete and Cement Materials Research · Magnesium Oxide Properties and Applications · Recycling and utilization of industrial and municipal waste in materials production
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. J.L. Provis, J.S.J. van Deventer, Alkali Activated Materials: State-of-the-Art Report, RILEM TC 224-AAM, 2014. doi:10.1007/978-94-007-7672-2.10.1007/978-94-007-7672-2 ↗
2. F. Pacheco-Torgal, Handbook of alkali-activated cements, mortars and concretes, Woodhead P, 2004. doi:https://doi.org/10.1016/C2013-0-16511-7.10.1016/C2013-0-16511-7 ↗
3. Durability of alkali-activated materials: progress and perspectives10.1111/jace.12831 ↗
4. Durability test methods and their application to AAMs: case of sulfuric-acid resistance10.1617/s11527-016-0904-7 ↗
5. Practical investigation of the sulfate resistance of concrete from construction units
6. Chemical stability of cementitious materials based on metakaolin10.1016/S0008-8846(99)00074-5 ↗
7. Geopolymer materials based on fly ash
8. Alkaline cement mortars. Chemical resistance to sulfate and seawater attack10.3989/mc.2002.v52.i267.326 ↗
9. Sulfate attack on alkali-activated slag concrete10.1016/S0008-8846(01)00659-7 ↗
10. Evaluation of accelerated degradation test methods for cementitious composites subject to sulfuric acid attack; application to conventional and alkali-activated concretes10.1016/j.cemconcomp.2017.12.015 ↗
11. Sulphuric acid exposure of conventional concrete and alkali-activated concrete: assessment of test methodologies10.1016/j.conbuildmat.2018.11.166 ↗
12. Development of microstructures in plain cement pastes hydrated at different temperatures10.1016/0008-8846(91)90044-I ↗
13. Effect of hydration temperature on the solubility behavior of Ca-, S-, Al-, and Si-bearing solid phases in Portland cement pastes10.1016/S0008-8846(03)00224-2 ↗
14. Effect of temperature on the pore solution, microstructure and hydration products of Portland cement pastes10.1016/j.cemconres.2006.11.016 ↗
15. 29Si magic-angle-spinning nuclear magnetic resonance study of hydrated cement paste and mortar10.1111/j.1151-2916.1990.tb06582.x ↗
16. Effect of curing temperature on cement hydration
17. Effect of elevated temperature curing on properties of alkali-activated slag concrete10.1016/S0008-8846(99)00143-X ↗
18. Strength and drying shrinkage of alkali-activated slag paste and mortar10.1155/2012/579732 ↗
19. Alkali-activated slag mortars: mechanical strength behaviour10.1016/S0008-8846(99)00154-4 ↗
20. Alkali-activated fly ashes A cement for the future10.1016/S0008-8846(98)00243-9 ↗
21. The effect of temperature on the geopolymerization process of a metakaolin-based geopolymer10.1016/j.matlet.2010.12.049 ↗
22. Geopolymeric materials prepared using Class F fly ash and elevated temperature curing10.1016/j.cemconres.2004.06.031 ↗
23. Effect of curing temperature on geopolymerization of metakaolin-based geopolymers10.1016/j.clay.2014.06.024 ↗
24. Eglinton · 2003
25. Hydration products of alkali activated slag cement10.1016/0008-8846(95)00045-E ↗
26. Hydration of alkali-activated slag: comparison with ordinary Portland cement10.1680/adcr.2006.18.3.119 ↗
27. External sulfate attack on alkali-activated slag10.1016/j.conbuildmat.2013.08.013 ↗
28. C. euro-international du beton CEB, Durable concrete structures - Design Guide 1989.
29. Hydration, setting and hardening of portland cement
30. A state-of-the-art review on delayed ettringite attack on concrete10.1016/S0958-9465(02)00080-X ↗
31. A new method for evaluating the risk of DEF10.1520/CCA11864 ↗
32. DEF: Una forma de ataque por sulfatos DEF: as a form of sulfate attack10.3989/mc.1996.v46.i244.519 ↗
33. Alkali activation of Australian slag cements10.1016/S0008-8846(98)00170-7 ↗
34. Workability and mechanical properties of alkali activated slag concrete10.1016/S0008-8846(98)00236-1 ↗
35. Effect of shrinkage-reducing admixtures on the properties of alkali-activated slag mortars and pastes10.1016/j.cemconres.2006.11.021 ↗
36. Factors affecting the strength of alkali-activated slag10.1016/0008-8846(94)90026-4 ↗
37. Influence of slag chemistry on the hydration of alkali-activated blast-furnace slag – Part II: effect of Al2O310.1016/j.cemconres.2011.08.005 ↗
38. MgO content of slag controls phase evolution and structural changes induced by accelerated carbonation in alkali-activated binders10.1016/j.cemconres.2013.12.003 ↗
39. The role of sodium during the hydration of alkali-activated slag10.1680/adcr.2000.12.2.65 ↗
40. Properties and durability of alkali-activated slag concrete
41. Microstructural changes in alkali activated fly ash/slag geopolymers with sulfate exposure10.1617/s11527-012-9906-2 ↗
42. Composition and microstructure of alkali activated fly ash binder: effect of the activator10.1016/j.cemconres.2005.03.003 ↗
43. Durability of alkali-activated fly ash cementitious materials10.1007/s10853-006-0584-8 ↗
44. S. Wallah, B.V. Rangan, Low-calcium fly ash-based geopolymer concrete: Long-term properties, 2006. https://espace.curtin.edu.au/handle/20.500.11937/34322 (accessed February 22, 2019).
45. Durability of geopolymer materials in sodium and magnesium sulfate solutions10.1016/j.cemconres.2004.09.002 ↗