journal article·2020-08

Effects of zeolite and silica fume substitution on the microstructure and mechanical properties of mortar at high temperatures

Mehrdad Abdi Moghadam, Ramezan Ali Izadifard

Publisher page

Abstract

Abstract The exposure of concrete to high temperatures leads to mechanical and chemical changes, and the performance of concrete is extremely dependent on its mortar specification. In this study, the compressive and tensile strength of mortar in a temperature range of 28–800 °C is investigated in hot conditions. The microstructure characterization is examined by X-ray diffraction test, thermal gravity analysis, and scanning electronic microscopy test. To minimize the environmental impacts of cement consumption, the possibility of partial replacement of cement with pozzolans is investigated. The results indicate that partial replacement of cement with zeolite and silica fume in the mixing plan of the concrete structure exposed to high-temperature meet both engineering and environmental consideration. Furthermore, the XRD and the TGA results provide valuable information about the prediction of the order of strength and the temperature history of the concrete members. The results pave the way for a better understanding of the high-temperature behavior of pozzolanic mortars.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Fire effects on concrete materials · Concrete and Cement Materials Research · Concrete Properties and Behavior

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (48)

Show source-provided references
1. A study on the mechanical properties of self-compacting concrete at high temperature and after cooling10.1617/s11527-012-9839-9 ↗
2. Mechanical properties of concrete composites subject to elevated temperature10.1016/j.firesaf.2017.10.010 ↗
3. Fire response of hybrid fiber reinforced concrete to high temperature10.1016/j.proeng.2017.02.123 ↗
4. Influence of high temperature on steel fiber reinforced concrete
5. Evaluation of mechanical properties of steel-fibre-reinforced concrete exposed to high temperatures by double-punch test10.1016/j.conbuildmat.2015.01.042 ↗
6. The effect of high temperature on the compressive strength of mortars10.1016/j.conbuildmat.2012.02.082 ↗
7. Behavior of blended cement mortars containing nano-metakaolin at elevated temperatures10.1016/j.conbuildmat.2012.04.099 ↗
8. Meyer · 2004
9. The concrete conundrum
10. Sustainability of the concrete industry: Current trends and future outlook10.5937/tehnika1701038T ↗
11. Sustainable development and climate change initiatives10.1016/j.cemconres.2007.09.008 ↗
12. Environmental assessment of green concrete containing natural zeolite on the global warming index in marine environments10.1016/j.jclepro.2013.07.055 ↗
13. Isothermal calorimetry and in-situ XRD study of the NaOH activated fly ash, metakaolin and slag10.1016/j.cemconres.2017.10.004 ↗
14. Supplementary cementitious materials: New sources, characterization, and performance insights10.1016/j.cemconres.2019.05.008 ↗
15. 618–05: Specifications for Coal Fly Ash and Raw or Calcined Natural Pozzolan for Use in Concrete
16. Comparing a natural pozzolan, zeolite, to metakaolin and silica fume in terms of their effect on the durability characteristics of concrete: A laboratory study10.1016/j.conbuildmat.2012.11.054 ↗
17. Markiv · Optimization of Concrete Composition With Addition of Zeolitic Tuff · 2014 · 116
18. Influence of pumice and zeolite on compressive strength, transport properties and resistance to chloride penetration of high strength self-compacting concretes10.1016/j.conbuildmat.2017.06.071 ↗
19. An experimental study on durability properties of concrete containing zeolite as a highly reactive natural pozzolan10.1016/j.conbuildmat.2012.04.038 ↗
20. Development of a high-temperature-resistant mortar by using slag and pumice10.1016/j.firesaf.2008.02.001 ↗
21. An experimental study of different curing regimes on the mechanical properties and sorptivity of self-compacting mortars with fly ash and silica fume10.1016/j.conbuildmat.2017.03.228 ↗
22. Fire resistance of high-volume fly ash mortars with nanosilica addition10.1016/j.conbuildmat.2012.05.028 ↗
23. Effect of elevated temperatures on geopolymer paste, mortar and concrete10.1016/j.cemconres.2009.10.017 ↗
24. Effect of pumice and fly ash incorporation on high temperature resistance of cement based mortars10.1016/j.cemconres.2007.02.005 ↗
25. The effect of acid treatment on the reactivity of natural zeolites used as supplementary cementitious materials10.1016/j.cemconres.2015.08.007 ↗
26. Recent advances in understanding the role of supplementary cementitious materials in concrete10.1016/j.cemconres.2015.03.018 ↗
27. Self-compacting concrete containing different powders at elevated temperatures–Mechanical properties and changes in the phase composition of the paste10.1016/j.tca.2010.12.007 ↗
28. Application of micro X-ray diffraction to investigate the reaction products formed by the alkali–silica reaction in concrete structures10.1016/j.cemconres.2015.07.012 ↗
29. Microstructure of concrete subjected to elevated temperatures: physico-chemical changes and analysis techniques10.1590/s1983-41952017000400004 ↗
30. Performance of lightweight concrete with silica fume after high temperature10.1016/j.conbuildmat.2007.07.017 ↗
31. Characterization of high strength mortars with nano alumina at elevated temperatures10.1016/j.cemconres.2013.08.003 ↗
32. Standard Practice for Mechanical Mixing of Hydraulic Cement Pastes and Mortars of Plastic Consistency
33. Mechanical properties and spalling at elevated temperature of high performance concrete made with reactive and waste inert powders10.1016/j.jestch.2016.12.004 ↗
34. 109M–02, Stand. Test Method Compressive Strength Hydraul. Cem. Mortars (Using 2-in. or [50-Mm]
35. Designation · 2012
36. Effect of temperature on phase composition and microstructure of artificial pozzolana-cement pastes containing burnt kaolinite clay10.1016/S0008-8846(98)00083-0 ↗
37. Behaviour of cement concrete at high temperature
38. S. Lim, Effects of elevated temperature exposure on cement-based composite materials, (2015).
39. Investigation of the structure of heated Portland cement paste by using various techniques10.1016/j.conbuildmat.2012.09.071 ↗
40. The properties of reactive powder concrete using PP fiber and pozzolanic materials at elevated temperature10.1016/j.jobe.2016.09.010 ↗
41. M. Abdi Moghadam, R.A. Izadifard, Experimental investigation on the effect of silica fume and zeolite on mechanical and durability properties of concrete at high temperatures, SN Appl. Sci. 1 (2019) 682. doi:10.1007/s42452-019-0739-2.10.1007/s42452-019-0739-2 ↗
42. Effects of steel and glass fibers on mechanical and durability properties of concrete exposed to high temperatures10.1016/j.firesaf.2020.102978 ↗
43. Evaluation of shear strength of plain and steel fibrous concrete at high temperatures10.1016/j.conbuildmat.2019.04.136 ↗
44. R.A. Izadifard, M. Abdi Moghadam, Experimental Study on the shear strength of normal strength concrete at high temperatures, InBook of Abstracts 2019 Aug 20 (p. 44).10.1016/j.conbuildmat.2019.04.136 ↗
45. C. Castillo, Effect of transient high temperature on high-strength concrete, (1987).
46. Tayfun Uygunoğlu İlker Bekir Topçu Effect of aggregate type on linear thermal expansion of self-consolidating concrete at elevated temperatures 19 3 2012 10.1515/secm-2012-0015 https://www.degruyter.com/view/j/secm.2012.19.issue-3/secm-2012-0015/secm-2012-0015.xml10.1515/secm-2012-0015 ↗
47. Experimental study on the thermal expansion property and mechanical performance of oil well cement with carbonaceous admixtures10.1039/C7RA03504G ↗
48. Thermal expansion of Portland cement paste, mortar and concrete at high temperatures10.1002/fam.810040203 ↗