Mitigation of efflorescence of alkali-activated slag mortars by incorporating calcium hydroxide
Source abstract
Abstract
Abstract Due to the high alkali concentration, weak binding of Na+ and relatively open microstructure, the efflorescence of alkali-activated slag (AAS) cement is a critical barrier limiting its widespread application. To reduce the efflorescence, Ca(OH)2 was added as a Ca-rich precursor into the binder with the dosage of 3, 6 and 9 wt% by slag. The efflorescence of AAS mortars was identified by visual inspection and mass weighing of efflorescence products formed on the surfaces of the mortar. Capillary porosity, water absorption rate, Na+ leaching test, XRD and TG analysis were also carried out to explain the change of microstructure and hydration products caused by the incorporation of Ca(OH)2. The results revealed that the addition of Ca(OH)2 significantly reduced the coverage areas and the amount of efflorescence products. However, visual inspection results were not consistent with that of mass weighing of efflorescence products, ion leaching, etc. If the impact of efflorescence on microstructure should be considered, visual inspection is not suitable. It can be concluded that the addition of Ca(OH)2 can mitigate the efflorescence by following reasons: firstly, the capillary porosity decreased from 16.86% to 15.22% and the water absorption rate decreased from 0.0366 mm/s1/2 to 0.0179 mm/s1/2 by adding 9% Ca(OH)2, which means that the migration pathway of the Na+ and water within the mortar was decreased. Secondly, the leaching results indicated that fewer Na+ leached from the Ca(OH)2-added samples, either from powder leaching or block leaching, which means that the addition of Ca(OH)2 may enhance the binding of Na+ by hydration products through increasing the C-A-S-H gel content.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete and Cement Materials Research · Concrete Properties and Behavior · Magnesium Oxide Properties and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (51)
Show source-provided references
1. Effect of foaming agent on physical and mechanical properties of alkali-activated slag foamed concrete10.1016/j.conbuildmat.2019.07.302 ↗
2. Effect of silicate modulus and metakaolin incorporation on the carbonation of alkali silicate-activated slags10.1016/j.cemconres.2010.02.003 ↗
3. Influence of activator type on hydration kinetics, hydrate assemblage and microstructural development of alkali activated blast-furnace slags10.1016/j.cemconres.2010.11.016 ↗
4. Effects of sodium hydroxide and sodium silicate solutions on compressive and shear bond strengths of FA–GBFS geopolymer10.1016/j.conbuildmat.2015.05.001 ↗
5. Flexural strength of notched concrete beam filled with alkali-activated binders under different types of alkali solutions10.1016/j.conbuildmat.2016.10.053 ↗
6. Alkali-activated slag mortars: mechanical strength behaviour10.1016/S0008-8846(99)00154-4 ↗
7. Factors affecting the strength of alkali-activated slag10.1016/0008-8846(94)90026-4 ↗
8. External sulfate attack on alkali-activated slag10.1016/j.conbuildmat.2013.08.013 ↗
9. Sulfate attack on alkali-activated slag concrete10.1016/S0008-8846(01)00659-7 ↗
10. Resistance of alkali-activated slag concrete to acid attack10.1016/S0008-8846(03)00125-X ↗
11. Stabilization/solidification of hazardous and radioactive wastes with alkali-activated cements10.1016/j.jhazmat.2006.05.008 ↗
12. Immobilization potential of Cr(VI) in sodium hydroxide activated slag pastes10.1016/j.jhazmat.2016.09.019 ↗
13. Effect of pore size distribution on drying shrinking of alkali-activated slag concrete10.1016/S0008-8846(00)00327-6 ↗
14. Drying shrinkage, strength and microstructure of alkali-activated high-calcium fly ash using FGD-gypsum and dolomite as expansive additive10.1016/j.cemconcomp.2020.103760 ↗
15. Study on improvement of carbonation resistance of alkali-activated slag concrete10.1016/j.conbuildmat.2018.04.117 ↗
16. Handbook of alkali-activated cements
17. Effects of red mud and Alkali-Activated Slag Cement on efflorescence in cement mortar10.1016/j.conbuildmat.2016.12.123 ↗
18. Effect of zeolite on waste based alkali-activated inorganic binder efflorescence10.1016/j.conbuildmat.2017.10.065 ↗
19. Calcium carbonate efflorescence on Portland cement and building materials10.1016/S0008-8846(02)00937-7 ↗
20. Effects of two redispersible polymer powders on efflorescence of portland cement-based decorative mortar
21. Fly ash-based geopolymers: the relationship between composition, pore structure and efflorescence10.1016/j.cemconres.2014.06.004 ↗
22. Pore solution in alkali-activated slag cement pastes. Relation to the composition and structure of calcium silicate hydrate10.1016/S0008-8846(03)00254-0 ↗
23. Alkali sorption by C-S-H and C-A-S-H gels: Part II. Role of alumina10.1016/S0008-8846(02)00753-6 ↗
24. ŠKVÁRA, A weak alkali bond in (N, K)–A–S–H gels_ evidence from leaching and modeling, (2012).
25. F. Škvára, L. Kopecky, L. Myskova, V. Smilauer, L. Alberovská, L. Vinšová, Aluminosilicate polymers - Influence of elevated temperatures, efflorescence, 2009.
26. Characterisation of pore structure development of alkali-activated slag cement during early hydration using electrical responses10.1016/j.cemconcomp.2018.02.016 ↗
27. Compressive strength development and shrinkage of alkali-activated fly ash–slag blends associated with efflorescence10.1617/s11527-015-0694-3 ↗
28. Efflorescence and subflorescence induced microstructural and mechanical evolution in fly ash-based geopolymers10.1016/j.cemconcomp.2018.06.010 ↗
29. The role of sodium during the hydration of alkali-activated slag10.1680/adcr.2000.12.2.65 ↗
30. J.S.J.v.D. P. Duxson, Effect of alkali cations on aluminum incorporation Geopolymeric Gels, (2005).10.1021/ie0494216 ↗
31. Effect of nano-silica on the efflorescence of waste based alkali-activated inorganic binder10.1016/j.conbuildmat.2018.02.006 ↗
32. Pore solution composition and alkali diffusion in inorganic polymer cement10.1016/j.cemconres.2010.04.008 ↗
33. Effect of Ca(OH)2 on shrinkage characteristics and microstructures of alkali-activated slag concrete10.1016/j.conbuildmat.2018.04.180 ↗
34. Strength development and durability of alkali-activated fly ash mortar with calcium carbide residue as additive10.1016/j.conbuildmat.2017.12.034 ↗
35. Porous medium coffee ring effect and other factors affecting the first crystallisation time of sodium chloride at the surface of a drying porous medium10.1063/1.4834356 ↗
36. Discrete salt crystallization at the surface of a porous medium10.1103/PhysRevLett.108.054502 ↗
37. Experimental study of the effect of sodium chloride on drying of porous media: the crusty–patchy efflorescence transition10.1016/j.ijheatmasstransfer.2012.09.045 ↗
38. Effect of nano-SiO2 on the efflorescence of an alkali-activated metakaolin mortar10.1016/j.conbuildmat.2020.118952 ↗
39. S. Geoffroy, M. Prat, A Review of Drying Theory and Modelling Approaches, 2014.10.1007/978-3-319-04531-3_7 ↗
40. Methods to control efflorescence in alkali-activated cement-based materials, in: F. Pacheco-Torgal, J.A. Labrincha, C. Leonelli, A. Palomo, P. Chindaprasirt (Eds.), Handbook of Alkali-Activated Cements, Mortars and Concretes, Woodhead Publishing, Oxford, 2015, pp. 463–483.10.1533/9781782422884.3.463 ↗
41. Influence of physico-chemical characteristics on the carbonation of cement paste at high replacement rates of metakaolin10.1016/j.conbuildmat.2017.10.021 ↗
42. Microcracking and strength development of alkali activated slag concrete10.1016/S0958-9465(01)00003-8 ↗
43. Salt weathering of concrete by sodium carbonate and sodium chloride
44. Hong Sung-Yoon, P.F. Glasser, Alkali binding in cement pastes: Part I. The C-S-H phase, Cem. Concr. Res. (1999).10.1016/S0008-8846(99)00187-8 ↗
45. Alkali uptake in calcium alumina silicate hydrate (C-A-S-H), Cem. Concr. Res. 85 (2016) 122–136.10.1016/j.cemconres.2016.03.009 ↗
46. Effects of sodium/calcium cation exchange on the mechanical properties of calcium silicate hydrate (CSH)10.1016/j.conbuildmat.2020.118283 ↗
47. A thermodynamic model for C-(N-)A-S-H gel: CNASH_ss. Derivation and validation10.1016/j.cemconres.2014.07.005 ↗
48. Strength and drying shrinkage of slag paste activated by sodium carbonate and reactive MgO10.1016/j.conbuildmat.2015.01.082 ↗
49. Enhancement of reactivity of calcium hydroxide-activated slag mortars by the addition of barium hydroxide10.1016/j.conbuildmat.2009.09.001 ↗
50. Hydration products and strength development of calcium hydroxide-based alkali-activated slag mortars10.1016/j.conbuildmat.2011.10.063 ↗
51. Effects of type and dosage of alkaline activator and temperature on the properties of alkali-activated slag mixtures10.1016/j.conbuildmat.2006.07.002 ↗