journal article·2021-10Open access

Experimental research on the spalling behaviour of ultra-high performance concrete under fire conditions

Hao Qin, Jiacheng Yang, Kai Yan, Jeung-Hwan Doh, Kun Wang, Xin Zhang

Abstract

Explosive spalling is a severe risk for ultra-high performance concrete (UHPC) structures exposed to fire, fundamentally obstructing the comprehensive study of fire safety and the extensive engineering application of UHPC. In contrast to previous studies on the optimisation of components and mixture properties, this paper proposes a new curing regime, two-stage hot air curing (THAC), to inhibit the explosive spalling of UHPC in a high stress state and under an extreme heating rate. Two hundred and twenty-eight UHPC cubes with variations in parameters such as curing regime, fibre type, and water-binder ratio were tested under the ISO 834 fire standard. The influence of THAC on the mechanical properties and explosive spalling of the samples was investigated, and scanning electron microscopy (SEM) was utilised to observe the microstructures of the tested cubes. On this basis, twelve full-scale UHPC beams with various curing regimes and load ratios were tested under thermal–mechanical coupling conditions. The explosive spalling behaviour of the beams was observed, and the influence of spalling on the fire resistance was analysed. The test results indicated that UHPC formed a dense microstructure during the first stage of 50 °C curing. With hot air curing at 150 °C, further hydration and pozzolanic reaction of residual cement and mineral admixtures could be activated, generating massive calcium-silica-hydrate (C-S-H) gels. Moreover, almost all the free water could be consumed and evaporated after THAC curing, dramatically improving the explosive spalling resistance of UHPC. THAC could completely prevent the fire-induced explosive spalling of UHPC of different sizes and with varying stress states and improve the mechanical properties. This occurred despite conventional curing such as standard curing, water curing, and steam curing potentially leading to more serious spalling and a significant reduction in fire resistance, even possibly affecting the failure mode of UHPC beams.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Fire effects on concrete materials · Engineering and Material Science Research · Fire dynamics and safety research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. E. Fehling, M. Schmidt, J. Walraven, T. Leutbecher, S. Fröhlich, Ultra-high performance concrete UHPC: fundamentals, design, examples, John. Wiley. Sons. (2015), https://onlinelibrary.wiley.com/doi/book/10.1002/9783433604076.10.1002/9783433604076 ↗
2. A review on structural behavior, design, and application of ultra-high-performance fiber-reinforced concrete10.1007/s40069-016-0143-x ↗
3. Chinses standard, T/CCPA 7-2018, Fundamental characteristics and test methods of ultra-high performance concrete (in Chinese).
4. AFGC, Ultra high performance fibre-reinforced concretes-interim recommendations, AFGC Publication, 2002.
5. ASTM C1856/C1856M-17, Standard practice for fabricating and testing specimens of ultra-high performance concrete.
6. JSCE, Recommendations for design and construction of ultra high strength fiber reinforced concrete structures (Draft), Japan Society of Civil Engineers, 2006.
7. Effects of steel fiber and strain rate on the dynamic compressive stress-strain relationship in reactive powder concrete10.1016/j.conbuildmat.2018.03.101 ↗
8. Cyclic behavior of ultra-high performance fiber reinforced concrete beam column joint10.1002/suco.201800025 ↗
9. Investigation on thermophysical properties of reactive powder concrete10.1007/s11431-011-4536-4 ↗
10. Comparative fire behavior of reinforced RPC and NSC simply supported beams10.1016/j.engstruct.2019.01.097 ↗
11. Mechanical and permeability properties of the interface between normal concrete substrate and ultra high performance fiber concrete overlay10.1016/j.conbuildmat.2012.06.013 ↗
12. Explosive spalling of ultra-high performance fibre reinforced concrete beams under fire10.1108/JSFE-12-2016-023 ↗
13. Experimental behavior of ultra high performance fiber reinforced concrete beams under fire conditions10.1016/j.engstruct.2020.110316 ↗
14. Critical factors governing the fire performance of high strength concrete systems10.1016/j.firesaf.2006.10.006 ↗
15. Experimental study on the spalling behaviour of ultra-high strength concrete in fire10.1016/j.conbuildmat.2020.120334 ↗
16. Combined curing as a novel approach to improve resistance of ultra-high performance concrete to explosive spalling under high temperature and its mechanical properties10.1016/j.cemconres.2018.04.011 ↗
17. Experimental research on fire resistance of reactive powder concrete10.1155/2012/860303 ↗
18. Effect of strength and fiber reinforcement on fire resistance of high-strength concrete columns10.1061/(ASCE)0733-9445(2003)129:2(253) ↗
19. Study of mechanisms of explosive spalling in high-strength concrete at high temperatures using acoustic emission10.1016/j.conbuildmat.2012.06.070 ↗
20. Quantifying curing and composition effects on compressive and tensile strength of 160–250 MPa RPC10.1016/j.conbuildmat.2019.117987 ↗
21. Microstructure and mechanical properties of RPC containing PP fibres at elevated temperatures10.1680/macr.13.00232 ↗
22. ISO 834-1:1999. (2020, January 15). Retrieved from https://www.iso.org/standard/2576.html.
23. Spalling and pore pressure in HPC at high temperatures10.1016/S0008-8846(00)00384-7 ↗
24. Effect of lateral restraint and inclusion of polypropylene and steel fibers on spalling behavior, pore pressure, and thermal stress in ultra-high-performance concrete (UHPC) at elevated temperature10.1016/j.conbuildmat.2020.121879 ↗
25. Effect of fire insulation on fire resistance of hybrid-fiber reinforced reactive powder concrete beams10.1016/j.compstruct.2018.10.073 ↗
26. Compressive behaviour of steel fiber reinforced reactive powder concrete at elevated temperatures10.1166/sam.2016.2758 ↗
27. Investigation on spalling resistance of ultra-high-strength concrete under rapid heating and rapid cooling
28. Shear strength of fiber reinforced reactive powder concrete prestressed girders without stirrups10.3151/jact.4.123 ↗
29. Microstructure of fire-damaged concrete. A case study10.1016/j.cemconcomp.2004.02.022 ↗
30. Effect of curing temperature on the behaviour of UHPFRC at elevated temperatures10.1016/j.conbuildmat.2018.06.163 ↗
31. Spalling behavior of metakaolin-fly ash based geopolymer concrete under elevated temperature exposure10.1016/j.cemconcomp.2019.103483 ↗
32. Chinses standard, GB/T 31387-2015, Reactive powder concrete (in Chinese).
33. The effect of curing conditions on compressive strength of ultra high strength concrete with high volume mineral admixtures10.1016/j.buildenv.2006.03.013 ↗
34. Influence of curing regime on properties of reactive powder concrete containing waste steel fibers10.1016/j.conbuildmat.2019.117129 ↗
35. Shear capacity of T-section girders made of reactive powder concrete10.1061/(ASCE)BE.1943-5592.0001253 ↗
36. Experimental research on mechanical performance of normal section of reinforced reactive powder concrete beam
37. BS Institution, BS EN 1363-1:2012, Fire resistance tests-Part 1: General requirements.