Abstract Slag is activated with alkali-silicate solutions made with nano-silica and waterglass. The reaction kinetics and the reaction products formed are evaluated for different silica and sodium contents. Isothermal calorimetric measurements with in-situ mixing reveal increased early reactivity with added silica, while the main hydration reaction is delayed. The presence of Na with dissolved silica in the activating solution does not influence the initial dissolution and early reactivity of slag. At the same time, it has an accelerating effect on the main hydration peak of slag. Dissolution studies of slag in alkaline solution with added silica indicate the immediate formation of calcium silicate hydrates after dissolution contributes to the early reactivity. The enhanced early reaction product formation in the presence of dissolved silica leads to the very rapid development of the internal structure. Rheological measurements indicate an early loss of workability due to increased early reactivity. The increase in time for the main hydration reaction of slag in the presence of added silica, however, delays the setting behavior. The primary reaction product in alkali-activated slag is calcium silicate hydrate with aluminum uptake, C-(A)-S-H. The addition of silica in the activating solution leads to its larger incorporation in the C-(A)-S-H and higher compressive strength. The sodium content in the activating solution does not contribute to the ultimate strength. The sodium in the alkali-activated slag is present in the form of a water-soluble amorphous product.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Concrete and Cement Materials Research · CO2 Sequestration and Geologic Interactions · Magnesium Oxide Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (64)

Show source-provided references
1. Shi · 2006
2. Early stage dissolution characteristics of aluminosilicate glasses with blast furnace slag- and fly-ash-like compositions10.1111/jace.14716 ↗
3. A critical review on application of alkali activated slag as a sustainable composite binder
4. Understanding the roles of activators towards setting and hardening control of alkali-activated slag cement10.1016/j.compositesb.2019.04.024 ↗
5. Sodium silicate-based, alkali-activated slag mortars - Part I. Strength, hydration and microstructure10.1016/S0008-8846(02)00717-2 ↗
6. Alkali-activated slag cement and concrete: a review of properties and problems10.1680/adcr.1995.7.27.93 ↗
7. Hydration products of alkali activated slag cement10.1016/0008-8846(95)00045-E ↗
8. Alkali-activated cements Opportunities and challenges10.1016/S0008-8846(98)00093-3 ↗
9. 29Si and 27Al NMR study of alkali-activated slag10.1016/S0008-8846(02)01044-X ↗
10. Characterization of alkali activated slag–fly ash blends containing nano-silica10.1016/j.conbuildmat.2015.08.086 ↗
11. A calorimetric study of early hydration of alkali-slag cements10.1016/0008-8846(95)00126-W ↗
12. Some factors affecting early hydration of alkali-slag cements10.1016/S0008-8846(96)85031-9 ↗
13. Influence of activator type on hydration kinetics, hydrate assemblage and microstructural development of alkali activated blast-furnace slags10.1016/j.cemconres.2010.11.016 ↗
14. Influence of slag chemistry on the hydration of alkali-activated blast-furnace slag — Part I: Effect of MgO10.1016/j.cemconres.2011.05.002 ↗
15. Influence of slag chemistry on the hydration of alkali-activated blast-furnace slag - Part II: Effect of Al2O310.1016/j.cemconres.2011.08.005 ↗
16. Hydration Products and Reactivity of Blast-Furnace Slag Activated by Various Alkalis10.1111/j.1151-2916.2003.tb03623.x ↗
17. Alkali-activated slag mortars: Mechanical strength behaviour10.1016/S0008-8846(99)00154-4 ↗
18. Effect of activator mix on the hydration and strength behaviour of alkali-activated slag cements10.1680/adcr.2003.15.3.129 ↗
19. Composition design and performance of alkali-activated cements10.1617/s11527-017-1048-0 ↗
20. Temperature and activator effect on early-age reaction kinetics of alkali-activated slag binders10.1016/j.conbuildmat.2016.03.098 ↗
21. Reaction kinetics, gel character and strength of ambient temperature cured alkali activated slag–fly ash blends10.1016/j.conbuildmat.2015.01.065 ↗
22. Investigation on a green olivine nano-silica source based activator in alkali activated slag-fly ash blends: Reaction kinetics, gel structure and carbon footprint10.1016/j.cemconres.2017.06.007 ↗
23. Sodium silicate solution – structure, properties and problems10.1002/zfch.19880280202 ↗
24. Effect of activator type and content on properties of alkali-activated slag mortars10.1016/j.compositesb.2013.10.001 ↗
25. Effect of alkali dosage and silicate modulus on carbonation of alkali-activated slag mortars10.1016/j.cemconres.2018.07.005 ↗
26. Microstructural changes in alkali-activated slag mortars induced by accelerated carbonation10.1016/j.cemconres.2017.07.008 ↗
27. Influence of starting material on the early age hydration kinetics, microstructure and composition of binding gel in alkali activated binder systems10.1016/j.cemconcomp.2013.11.010 ↗
28. Compatibility studies between N-A-S-H and C-A-S-H gels. Study in the ternary diagram Na2O-CaO-Al2O3-SiO2-H2O10.1016/j.cemconres.2011.05.006 ↗
29. Effects of dosage and modulus of water glass on early hydration of alkali–slag cements10.1016/S0008-8846(01)00717-7 ↗
30. Workability Loss and Compressive Strength Development of Cementless Mortars Activated by Combination of Sodium Silicate and Sodium Hydroxide10.1061/(ASCE)0899-1561(2009)21:3(119) ↗
31. Mechanical and thermal characterisation of geopolymers based on silicate-activated metakaolin/slag blends10.1007/s10853-011-5490-z ↗
32. BIS (Bureau of Indian Standards), Specification for granulated slag for the manufacture of Portland slag cement [CED 2: Cement and Concrete]. IS 12089 (1987), Manak Bhavan, New Delhi, India.
33. The viscosity properties of sodium silicate solutions10.1007/s10953-007-9214-6 ↗
34. BIS (Bureau of Indian Standards). 1988. Methods of physical tests for hydraulic cement. Part-6: Determination of compressive strength of hydraulic cement other than masonry cement. IS 4031 (1988). Manak Bhavan, New Delhi, India.
35. BIS (Bureau of Indian Standards), Method of Tests for Strength of Concrete [CED 2: Cement and Concrete]. IS 516 (1959), Manak Bhavan, New Delhi, India.
36. An investigation of microstructure evolution in cement paste through setting using ultrasonic and rheological measurements10.1016/j.cemconres.2009.09.018 ↗
37. Ultrasonic monitoring of capillary porosity and elastic properties in hydrating cement paste10.1016/j.cemconcomp.2010.11.001 ↗
38. The origins of thixotropy of fresh cement pastes10.1016/j.cemconres.2011.09.004 ↗
39. The influence of wall slip on yield stress and viscoelastic measurements of cement paste10.1016/S0008-8846(00)00440-3 ↗
40. International Centre for Diffraction Data (ICDD), Powder Diffraction File (PDF-2013), 12 Campus Boulevard, Newtown Square, PA, 19073-3273, USA.
41. Direct decomposition X-ray diffraction method for amorphous phase quantification and glassy phase determination in binary blends of siliceous fly ash and hydrated cement
42. Quantitative phase analysis of slag hydrating in an alkaline environment10.1107/S1600576720001399 ↗
43. Quantitative Analysis of Phase Assemblage and Chemical Shrinkage of Alkali-Activated Slag10.3151/jact.14.245 ↗
44. Effects of activator characteristics on the reaction product formation in slag binders activated using alkali silicate powder and NaOH10.1016/j.cemconcomp.2012.03.006 ↗
45. Stoichiometry of Slag Hydration with Calcium Hydroxide10.1111/j.1151-2916.2002.tb00197.x ↗
46. Selective dissolution of hydrated blast furnace slag cements10.1016/0008-8846(87)90110-4 ↗
47. Degrees of reaction of the slag in some blends with Portland cements10.1016/0008-8846(95)00190-5 ↗
48. Methods for determination of degree of reaction of slag in blended cement pastes10.1016/j.cemconres.2011.11.010 ↗
49. Reactivity of blast-furnace slag in Portland cement blends hydrated under different conditions10.1016/S0008-8846(01)00587-7 ↗
50. Pore solution chemistry of alkali-activated ground granulated blast-furnace slag10.1016/S0008-8846(98)00212-9 ↗
51. High-resolution Nanoprobe X-ray fluorescence characterization of heterogeneous calcium and heavy metal distributions in alkali-activated fly ash10.1021/la901560h ↗
52. Pore solution composition of alkali-activated slag/fly ash pastes10.1016/j.cemconres.2018.10.010 ↗
53. Setting of alkali-activated slag cement. Influence of activator nature10.1680/adcr.2001.13.3.115 ↗
54. Rheological characterization of low-calcium fly ash suspensions in alkaline silicate colloidal solutions for geopolymer concrete production10.1016/j.jclepro.2019.06.124 ↗
55. Thixotropic investigation on cement paste: Experimental and numerical approach10.1016/j.jnnfm.2005.10.007 ↗
56. Suitability of commercial superplasticizers for one-part alkali-activated blast-furnace slag mortar
57. The hydration of slag, part 1: Reaction models for alkali-activated slag10.1007/s10853-006-0873-2 ↗
58. In situ imaging of ground granulated blast furnace slag hydration10.1007/s10853-006-0941-7 ↗
59. Cell dimensions and composition of nanocrystalline calcium silicate hydrate solid solutions. Part 1: synchrotron-based x-ray diffraction10.1111/j.1551-2916.2008.02484.x ↗
60. Structural characterization of C-S-H and C-A-S-H samples-Part II: Local environment investigated by spectroscopic analyses10.1016/j.jssc.2009.09.024 ↗
61. Pore solution in alkali-activated slag cement pastes. Relation to the composition and structure of calcium silicate hydrate10.1016/S0008-8846(03)00254-0 ↗
62. Structure of Calcium Silicate Hydrates Formed in Alkaline-Activated Slag: Influence of the Type of Alkaline Activator10.1111/j.1151-2916.2003.tb03481.x ↗
63. Structure of Calcium Silicate Hydrate (C-S-H): Near-, Mid-, and Far-Infrared Spectroscopy10.1111/j.1151-2916.1999.tb01826.x ↗
64. The role of sodium during the hydration of alkali-activated slag10.1680/adcr.2000.12.2.65 ↗