journal article·2021-06

Properties of high-volume slag cement mortar incorporating circulating fluidized bed combustion fly ash and bottom ash

Salman Siddique, Hyeju Kim, Jeong Gook Jang

Publisher page

Abstract

Abstract This study investigates the incorporation of circulating fluidized bed combustion (CFBC) fly ash as an activator and CFBC bottom ash as fine aggregate in high-volume slag cement mortar. A series of investigations were carried out to analyze the influence of CFBC ash products on the properties of mortar. For comparison, control specimens of ordinary Portland cement and high-volume slag cement were considered. The results obtained from X-ray diffraction and thermogravimetric analyses revealed that the addition of CFBC fly ash activated the hydration of the slag and improved the initial strength of the mortar. Additionally, a pore size distribution test showed that the introduction of CFBC fly ash resulted in decrease of the critical pore diameter and the porosity of the high-volume slag mixes up to 28 days of curing. Similarly, it was found that the compressive strength of high-volume slag mortar manufactured with CFBC fly ash and CFBC bottom ash was improved. Furthermore, the enhanced hydration of high-volume slag mortar due to CFBC ash products resulted in decreased water absorption and fewer total voids. However, inferior resistance to chemical attack was also observed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Concrete and Cement Materials Research · Recycling and utilization of industrial and municipal waste in materials production · Rock Mechanics and Modeling

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (52)

Show source-provided references
1. The effect of curing conditions on compressive strength of ultra high strength concrete with high volume mineral admixtures10.1016/j.buildenv.2006.03.013 ↗
2. Utilization of high volume of industrial slag in self compacting concrete10.1016/j.jclepro.2015.08.039 ↗
3. Mercury intrusion porosimetry characterization of micropore structures of high-strength cement pastes incorporating high volume ground granulated blast-furnace slag10.1016/j.conbuildmat.2017.01.076 ↗
4. Effect of gypsum on the properties of composite binder containing high-volume slag and iron tailing powder10.1016/j.conbuildmat.2020.119023 ↗
5. Influence of nano-CaCO3 addition on the compressive strength and microstructure of high volume slag and high volume slag-fly ash blended pastes10.1016/j.jobe.2019.100929 ↗
6. Use of nano-silica to increase early strength and reduce setting time of concretes with high volumes of slag10.1016/j.cemconcomp.2012.02.005 ↗
7. The synergistic effect of nano-silica with blast furnace slag in cement based materials10.1016/j.conbuildmat.2016.09.078 ↗
8. Effect of nano silica on compressive strength and microstructures of high volume blast furnace slag and high volume blast furnace slag-fly ash blended pastes
9. Characterization of lime activated recycled aggregate concrete with high-volume ground granulated blast furnace slag10.1016/j.conbuildmat.2020.119882 ↗
10. Examining the potential of calcined oyster shell waste as additive in high volume slag cement10.1016/j.conbuildmat.2019.116973 ↗
11. Sulfation phenomena in fluidized bed combustion systems10.1016/S0360-1285(00)00021-6 ↗
12. Utilization of circulating fluidized bed combustion ash in producing controlled low-strength materials with cement or sodium carbonate as activator10.1016/j.conbuildmat.2017.08.158 ↗
13. Effect of CFBC ash as partial replacement of PCC ash in alkali-activated material10.1016/j.conbuildmat.2020.118383 ↗
14. Characteristics of CFBC fly ash and properties of cement-based composites with CFBC fly ash and coal-fired fly ash10.1016/j.conbuildmat.2014.05.057 ↗
15. Blast furnace slag addition effects on delayed ettringite formation in heat-cured mortars10.1007/s12205-017-0642-6 ↗
16. The effect of the partial cement substitution with fly ash on Delayed Ettringite Formation in heat-cured mortars10.1007/s12205-016-0778-9 ↗
17. Influence of circulating fluidized bed combustion (CFBC) fly ash on properties of modified high volume low calcium fly ash (HVFA) cement paste10.1016/j.conbuildmat.2015.05.075 ↗
18. Synthesis and characterization of mortars with circulating fluidized bed combustion fly ash and ground granulated blast-furnace slag10.1016/j.conbuildmat.2016.07.071 ↗
19. Use of circulating fluidized bed combustion bottom ash as a secondary activator in high-volume slag cement10.1016/j.conbuildmat.2019.117240 ↗
20. ASTMC150, Standard Specification for Portland Cement, ASTM International, West Conshohocken, PA, 2020.
21. ASTMC989, Standard Specification for Slag Cement for Use in Concrete and Mortars, ASTM International, West Conshohocken, PA, 2018.
22. ASTMC109, Standard Test Method for Compressive Strength of Hydraulic Cement Mortars (Using 2-in. or [50 mm] Cube Specimens), ASTM International, West Conshohocken, PA, 2020.
23. ASTMC642, Standard Test Method for Density, Absorption, and Voids in Hardened Concrete, ASTM International, West Conshohocken, PA, 2013.
24. ASTMC1403, Standard Test Method for Rate of Water Absorption of Masonry Mortars, ASTM International West Conshohocken, PA, 2015.
25. ASTMC267, Standard Test Methods for Chemical Resistance of Mortars, Grouts, and Monolithic Surfacings and Polymer Concretes, ASTM International, West Conshohocken, PA, 2012.
26. Self-cementitious properties of fly ashes from CFBC boilers co-firing coal and high-sulphur petroleum coke10.1016/j.cemconres.2007.03.013 ↗
27. Investigations of anhydrite in CFBC fly ash as cement retarders10.1016/j.conbuildmat.2012.11.056 ↗
28. The zeta-potential of blast furnace slag and fly ash10.1016/0008-8846(89)90052-5 ↗
29. Possibilities of utilizing solid residues from pressured fluidized bed coal combustion (PSBC) for the production of blended cements10.1016/S0008-8846(97)00258-5 ↗
30. Microstructural densification and CO2 uptake promoted by the carbonation curing of belite-rich Portland cement10.1016/j.cemconres.2016.01.001 ↗
31. Optimization of gypsum and slag contents in blended cement containing slag10.1016/j.cemconcomp.2020.103674 ↗
32. Influence of water to cement ratio on CO2 uptake capacity of belite-rich cement upon exposure to carbonation curing10.1016/j.cemconcomp.2020.103616 ↗
33. Strength development of solely ground granulated blast furnace slag geopolymers10.1016/j.conbuildmat.2020.118720 ↗
34. Differential scanning calorimetry study of ordinary Portland cement10.1016/S0008-8846(99)00128-3 ↗
35. Differential scanning calorimetry study of ordinary Portland cement paste containing metakaolin and theoretical approach of metakaolin activity10.1016/S0958-9465(00)00090-1 ↗
36. The AFm phase in Portland cement10.1016/j.cemconres.2006.10.010 ↗
37. Pore size analyses of cement paste exposed to external sulfate attack and delayed ettringite formation10.1016/j.cemconres.2019.05.011 ↗
38. Experimental study and modelling of sulfate sorption on calcium silicate hydrates
39. Use of power plant bottom ash as fine and coarse aggregates in high-strength concrete10.1016/j.conbuildmat.2010.06.065 ↗
40. G. Nader, B. Jeffrey, Properties of high-calcium dry bottom ash for structural concrete, ACI Mater. J. 94(2).
41. Delayed ettringite formation10.1016/S0008-8846(01)00466-5 ↗
42. Durability properties of bone china ceramic fine aggregate concrete10.1016/j.conbuildmat.2018.03.262 ↗
43. D.D. Double, A. Hellawell, S.J. Perry, P.B. Hirsch, The hydration of Portland cement, Proc. Royal Soc. London. A. Math. Phys. Sci. 359(1699) (1978) 435–451.10.1098/rspa.1978.0050 ↗
44. The confused world of sulfate attack on concrete10.1016/j.cemconres.2004.04.004 ↗
45. Magnesium-sodium sulfate attack in plain and blended cements10.1061/(ASCE)0899-1561(1994)6:2(201) ↗
46. Sulfate attack research — whither now?10.1016/S0008-8846(01)00510-5 ↗
47. Damage evolution of cement mortar with high volume slag exposed to sulfate attack10.1016/j.conbuildmat.2020.118626 ↗
48. Development of synthetic aggregate using off-ASTM specification ashes10.1016/j.conbuildmat.2012.09.009 ↗
49. Improvement of the properties of a mortar with 5% of kaolin fillers in sand combined with metakaolin, brick waste and glass powder in cement10.1016/j.conbuildmat.2017.07.062 ↗
50. Influence of chlorides on magnesium sulphate attack for mortars with Portland cement and slag based binders10.1016/j.conbuildmat.2017.07.201 ↗
51. Evaluating resistance of fine bone china ceramic aggregate concrete to sulphate attack10.1016/j.conbuildmat.2018.07.138 ↗
52. Investigation of sulfuric acid attack upon cement mortars containing silicon carbide powder10.1016/j.powtec.2019.10.026 ↗