In this work, quantitative assessment of surface damage in terms of parameters like surface crack density and recast layer thickness in wire electrical discharge machining (WEDM) process has been undertaken. The effect of processing conditions on crack formation is studied using scanning electron microscope. Surface crack density and recast layer thickness analysis in terms of machining parameters such as pulse on time, pulse off time, peak current, spark gap voltage significantly deteriorate the microstructure of machined samples, which produces the deeper, wider overlapping craters, pock marks, globules of debris and micro cracks. The microstructure analysis of WEDM surface was based upon the theory of electrical discharge phase and metallurgical physics. It is found that the pulse on time, pulse off time and peak current are the most dominating parameters for both surface crack density and recast layer thickness.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced Machining and Optimization Techniques · Advanced Surface Polishing Techniques · Advanced machining processes and optimization

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. Ekmekci B. · Metallurgical and Materials Transactions B: Metallurgy and Materials Processing Science · 40 · 7010.1007/s11663-008-9220-0 ↗
2. 10.1081/MST-20005124410.1081/MST-200051244 ↗
3. 10.1007/s11668-011-9487-310.1007/s11668-011-9487-3 ↗
4. 10.1177/095440541246277810.1177/0954405412462778 ↗
5. 10.1016/j.jmapro.2012.05.00310.1016/j.jmapro.2012.05.003 ↗
6. 10.1016/j.apsusc.2007.05.03110.1016/j.apsusc.2007.05.031 ↗
7. 10.1016/j.jmatprotec.2007.02.04810.1016/j.jmatprotec.2007.02.048 ↗
8. 10.1016/j.jmatprotec.2005.04.07810.1016/j.jmatprotec.2005.04.078 ↗
9. 10.1080/135281603100007497310.1080/1352816031000074973 ↗
10. 10.1016/j.msea.2003.10.27710.1016/j.msea.2003.10.277 ↗
11. Kumar J. · Journal of the Brazilian Society of Mechanical Sciences and Engineering · 30 · 231
12. Kumar J. · International Journal of Machining and Machinability of Materials · 5 · 347
13. 10.1504/IJMR.2010.03162910.1504/IJMR.2010.031629 ↗
14. Kumar A. · International Journal of Advance Manufacturing Technology · 68 · 2645
15. 10.1177/095440541347979110.1177/0954405413479791 ↗
16. 10.1155/2013/84787610.1155/2013/847876 ↗
17. 10.1080/10910344.2014.86363210.1080/10910344.2014.863632 ↗
18. 10.1177/095440541351301310.1177/0954405413513013 ↗
19. 10.1080/10910344.2011.55796610.1080/10910344.2011.557966 ↗
20. 10.1016/S0924-0136(03)00547-810.1016/S0924-0136(03)00547-8 ↗
21. 10.1016/j.msea.2003.08.04610.1016/j.msea.2003.08.046 ↗
22. 10.1016/0924-0136(92)90162-L10.1016/0924-0136(92)90162-L ↗
23. 10.1080/1042691080193857710.1080/10426910801938577 ↗
24. 10.1016/S0924-0136(00)00539-210.1016/S0924-0136(00)00539-2 ↗
25. 10.1016/0378-3804(87)90047-710.1016/0378-3804(87)90047-7 ↗
26. 10.1007/s00170-004-2331-010.1007/s00170-004-2331-0 ↗
27. 10.1179/sur.1989.5.2.15810.1179/sur.1989.5.2.158 ↗
28. 10.1016/S0890-6955(02)00158-X10.1016/S0890-6955(02)00158-X ↗
29. 10.1007/s00170-004-2496-610.1007/s00170-004-2496-6 ↗
30. 10.1243/09544054JEM155910.1243/09544054JEM1559 ↗
31. 10.1007/s00170-004-2203-710.1007/s00170-004-2203-7 ↗
32. 10.1007/s00170-011-3340-410.1007/s00170-011-3340-4 ↗
33. Tao J. · Journal of Manufacturing Science and Engineering · 50 · 431
34. Wood, R.A.; Favor, R.J. (1972)Titanium Alloys Handbook. Air Force Materials Laboratory, Ohio, 45433, 45–46.
35. 10.1016/j.apsusc.2011.01.08310.1016/j.apsusc.2011.01.083 ↗