Effect of diatomite on the reaction kinetics, early-age chemical shrinkage and microstructure of alkali-activated slag cements
Source abstract
Abstract
Understanding and revealing the relationship between the early-age chemical shrinkage, reaction characteristic and microstructure of alkali-activated slag (AAS) pastes are of importance for the application of this cementitious material. This study investigates the effect of diatomite on the early-age compressive strength and the first 72-h chemical shrinkage of AAS pastes. A novel approach is proposed based on isothermal conduction calorimetry and 1H low-field nuclear magnetic resonance analyses to identify the internal correlation between chemical shrinkage and reaction situation. Results show that the early-age chemical shrinkage is dominated by the reaction process and reaction degree of AAS pastes. The incorporation of diatomite makes a great contribution to the control of chemical shrinkage even though it slightly sacrifices the development of compressive strength. This suggests the controls in the reaction process and chemical shrinkage of AAS pastes can be achieved by incorporating diatomite. The proposed approach can be used to assess chemical shrinkage of AAS, which contributes more to deeper understanding in the early-age volume change of alkali-activated cements.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete and Cement Materials Research · Concrete Properties and Behavior · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (70)
Show source-provided references
1. Advances in understanding alkali-activated materials10.1016/j.cemconres.2015.04.013 ↗
2. Engineering properties of alkali activated materials reactive powder concrete10.1016/j.conbuildmat.2020.121550 ↗
3. Advances in alkali-activation of clay minerals10.1016/j.cemconres.2020.106050 ↗
4. Beneficial use of boiler ash in alkali-activated bricks10.1016/j.resconrec.2017.09.013 ↗
5. Shrinkage mitigation, strength enhancement and microstructure improvement of alkali-activated slag/fly ash binders by ultrafine waste concrete powder10.1016/j.compositesb.2021.109570 ↗
6. Antimicrobial performance and biodeterioration mechanisms of alkali-activated slag10.1016/j.cemconres.2022.106844 ↗
7. Effect of curing time on the chloride diffusion of alkali-activated slag
8. Alkali-activated slag (AAS) paste: Correlation between durability and microstructural characteristics10.1016/j.conbuildmat.2020.120886 ↗
9. On the mechanisms of shrinkage reducing admixture in alkali activated slag binders
10. Autogenous shrinkage of alkali activated slag mortars: Basic mechanisms and mitigation methods10.1016/j.cemconres.2018.04.004 ↗
11. On the mechanism of plastic shrinkage cracking in fresh cementitious materials10.1016/j.cemconres.2018.10.015 ↗
12. Shrinkage behavior of fly ash based geopolymer pastes with and without shrinkage reducing admixture10.1016/j.cemconcomp.2019.02.007 ↗
13. Shrinkage mechanisms and shrinkage-mitigating strategies of alkali-activated slag composites: A critical review10.1016/j.conbuildmat.2021.125993 ↗
14. Effect of internal curing by superabsorbent polymers – Internal relative humidity and autogenous shrinkage of alkali-activated slag mortars10.1016/j.conbuildmat.2016.07.007 ↗
15. Cracking potential of alkali-activated slag and fly ash concrete subjected to restrained autogenous shrinkage10.1016/j.cemconcomp.2020.103767 ↗
16. Mitigating shrinkage of alkali activated slag with biofilm10.1016/j.cemconres.2020.106234 ↗
17. Shrinkage mitigation strategies in alkali-activated slag10.1016/j.cemconres.2017.08.025 ↗
18. Shrinkage characteristics of heat-treated ultra-high performance concrete and its mitigation using superabsorbent polymer based internal curing method10.1016/j.cemconcomp.2018.03.003 ↗
19. Use of recycled aggregates as internal curing agent for alkali-activated slag system10.1016/j.conbuildmat.2017.10.110 ↗
20. Internal curing by superabsorbent polymers in alkali-activated slag10.1016/j.cemconres.2020.106123 ↗
21. A review on shrinkage-reducing methods and mechanisms of alkali-activated/geopolymer systems: Effects of chemical additives
22. Shrinkage behavior and mechanical properties of alkali activated mortar incorporating nanomaterials and polypropylene fiber10.1016/j.ceramint.2022.04.297 ↗
23. Drying shrinkage in alkali-activated binders – A critical review10.1016/j.conbuildmat.2018.09.125 ↗
24. Mechanisms of autogenous shrinkage of alkali-activated fly ash-slag pastes cured at ambient temperature within 24 h10.1016/j.conbuildmat.2018.03.155 ↗
25. Early age volume changes in metakaolin geopolymers: Insights from molecular simulations and experiments10.1016/j.cemconres.2021.106428 ↗
26. Accurate determination of the “time-zero” of autogenous shrinkage in alkali-activated fly ash/slag system10.1016/j.compositesb.2019.107367 ↗
27. Shrinkage characteristics of alkali-activated fly ash/slag paste and mortar at early ages10.1016/j.cemconcomp.2014.07.007 ↗
28. On the use of diatomite as antishrinkage additive in the preparation of monolithic carbon aerogels10.1016/j.carbon.2015.11.017 ↗
29. Humidity control materials prepared from diatomite and volcanic ash10.1016/j.conbuildmat.2012.09.040 ↗
30. A novel synthesis of lightweight and high-strength green geopolymer foamed material by rice husk ash and ground-granulated blast-furnace slag10.1016/j.resconrec.2021.105922 ↗
31. Additive manufacturing of inorganic components using a geopolymer and binder jetting
32. Fully reacted high strength geopolymer made with diatomite as a fumed silica alternative10.1016/j.ceramint.2017.07.222 ↗
33. Very early-age reaction kinetics and microstructural development in alkali-activated slag10.1016/j.cemconcomp.2014.09.001 ↗
34. Alkali-activated blends of calcium aluminate cement and slag/diatomite10.1016/j.ceramint.2013.05.031 ↗
35. Toward an indexing approach to evaluate fly ashes for geopolymer manufacture10.1016/j.cemconres.2016.04.007 ↗
36. Preparation and characteristics of porous magnesium phosphate cement modified by diatomite10.1016/j.matchemphys.2019.121742 ↗
37. Low field NMR relaxation as a probe to study the effect of activators and retarders on the alkali-activated GGBFS setting process10.1016/j.cemconcomp.2019.103399 ↗
38. Surface relaxation and permeability of cement pastes with hydrophobic agent: Combining 1H NMR and BET10.1016/j.conbuildmat.2021.125264 ↗
39. A novel method for semi-quantitative analysis of hydration degree of cement by 1H low-field NMR10.1016/j.cemconres.2020.106329 ↗
40. Isothermal calorimetry and in-situ XRD study of the NaOH activated fly ash, metakaolin and slag10.1016/j.cemconres.2017.10.004 ↗
41. Reaction kinetics in sodium silicate powder and liquid activated slag binders evaluated using isothermal calorimetry10.1016/j.tca.2012.07.010 ↗
42. Estimation of reaction kinetics of geopolymers at early ages10.1016/j.cemconres.2020.105971 ↗
43. The use of raw and calcined diatomite in cement production10.1016/j.cemconcomp.2007.08.003 ↗
44. Curing process and pore structure of metakaolin-based geopolymers: Liquid-state 1H NMR investigation10.1016/j.cemconres.2021.106394 ↗
45. Effect of water-binding ability of amorphous gel on the rheology of geopolymer fresh pastes with the different NaOH content at the early age10.1016/j.conbuildmat.2020.120529 ↗
46. Water distribution and transport-kinetics model in fresh cement-based mixtures containing superabsorbent polymers based on 1H low-field NMR10.1016/j.cemconcomp.2021.104396 ↗
47. Surface relaxation and chemical exchange in hydrating cement pastes: a two-dimensional NMR relaxation study
48. Probing the microstructure and water phases in composite cement blends10.1016/j.cemconres.2006.10.007 ↗
49. 1H-NMR relaxation and state evolvement of evaporable water in cement pastes
50. New insights into the effect of gypsum on hydration and elasticity development of C3S paste during setting10.1016/j.cemconres.2022.106860 ↗
51. Degradation mechanisms of alkali-activated binders in sulfuric acid: The role of calcium and aluminum availability10.1016/j.conbuildmat.2020.118477 ↗
52. Mercury porosimetry: An inappropriate method for the measurement of pore size distributions in cement-based materials10.1016/S0008-8846(00)00370-7 ↗
53. Influence of evaporation rate on pore size distribution, water loss, and early-age drying shrinkage of cement paste after the initial setting10.1016/j.conbuildmat.2019.07.143 ↗
54. Evolutions in the properties and microstructure of cement mortars containing hydroxyethyl methyl cellulose after controlling the air content10.1016/j.cemconcomp.2022.104487 ↗
55. Reuse of waste glass powder in alkali-activated metakaolin/fly ash pastes: Physical properties, reaction kinetics and microstructure10.1016/j.resconrec.2021.105721 ↗
56. Microstructure and durability performance of sustainable cementitious composites containing high-volume regenerative biosilica10.1016/j.resconrec.2021.106038 ↗
57. Pore structure evolution mechanism of cement mortar containing diatomite subjected to freeze-thaw cycles by multifractal analysis10.1016/j.cemconcomp.2020.103731 ↗
58. Investigation of particle characteristics and enhancing the pozzolanic activity of diatomite by grinding
59. Effect of drying procedures on pore structure and phase evolution of alkali-activated cements10.1016/j.cemconcomp.2018.12.003 ↗
60. Reusing waste red brick powder as partial mineral precursor in eco-friendly binders: Reaction kinetics, microstructure and life-cycle assessment10.1016/j.resconrec.2022.106523 ↗
61. Effect of elevated temperature on alkali-activated geopolymeric binders compared to Portland cement-based binders10.1016/j.cemconres.2016.09.013 ↗
62. Experimental study on humidity control performance of diatomite-based building materials10.1016/j.applthermaleng.2016.11.203 ↗
63. A comparison study of Portland cement hydration kinetics as measured by chemical shrinkage and isothermal calorimetry10.1016/j.cemconcomp.2013.03.007 ↗
64. Characterization of one-part alkali-activated slag with rice straw ash10.1016/j.conbuildmat.2022.128403 ↗
65. Absorption kinetics of superabsorbent polymers (SAP) in various cement-based solutions10.1016/j.cemconres.2017.03.009 ↗
66. Early age shrinkage and heat of hydration of cement-fly ash-slag ternary blends10.1016/j.conbuildmat.2017.07.138 ↗
67. Insight into the catalytic properties zeolitized kaolinite/diatomite geopolymer as an environmental catalyst for the sustainable conversion of spent cooking oil into biodiesel; optimization and kinetics
68. Insight into the role of the zeolitization process in enhancing the adsorption performance of kaolinite/diatomite geopolymer for effective retention of Sr (II) ions; batch and column studies10.1016/j.jenvman.2021.112984 ↗
69. Metal-organic framework MIL-100(Fe) as a novel moisture buffer material for energy-efficient indoor humidity control10.1016/j.buildenv.2018.09.027 ↗
70. Preparation and characterization of composite scallop shell powder-based and diatomite-based hygroscopic coating materials with metal-organic framework for indoor humidity regulation