Prediction model for time-dependent drying shrinkage of recycled coarse and fine aggregate concrete based on internal relative humidity
Source abstract
Abstract
Recycled aggregates (RAs) are characterized by large porosity and complex interfacial transition zones, leading to a more complex drying shrinkage mechanism for recycled aggregate concrete (RAC). In reporting on the mechanism of drying shrinkage of RAC, the internal relative humidity (RH) and drying shrinkage were investigated considering replacement ratios of recycled coarse aggregate (RCA) and recycled fine aggregate (RFA) of 0 %, 30 %, 50 %, 70 % and 100 %, respectively. Using empirical comparisons, the research identifies the link between the internal RH and drying shrinkage in RAC, offering an analysis of the shrinkage mechanism caused by the internal RH. Following that, the prediction model of RAC was proposed based on the internal RH, which will be implemented for evaluating the drying shrinkage of RAC considering the parameters corresponding to the RCA and RFA replacement ratios. Results showed that (1) A coupling effect between the RCA and RFA on the internal relative humidity is observed in the case of single-sided drying; (2) When all natural aggregates are replaced by RAs, the relative humidity loss ( RH loss) of concrete at by 36.4 % compared to normal concrete, while drying shrinkage increases by 94.8 %; (3) An excellent linear correlation is achieved between internal RH and drying shrinkage of the RAC. The model proposed in this study achieves accurate prediction for the drying shrinkage of RAC with the change of the internal RH, providing the theoretical basis for the quantitative analysis of the long-term performance of RAC.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Recycled Aggregate Concrete Performance · Innovative concrete reinforcement materials · Innovations in Concrete and Construction Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (57)
Show source-provided references
1. Life cycle assessment of recycled aggregate concrete on its environmental impacts: a critical review10.1016/j.conbuildmat.2021.125950 ↗
2. Comparative environmental evaluation of aggregate production from recycled waste materials and virgin sources by LCA10.1016/j.resconrec.2016.02.009 ↗
3. Research progress and engineering application of reinforced recycled aggregate concrete structure[J]
4. Relationship between internal humidity and drying shrinkage of recycled aggregate thermal insulation concrete considering recycled aggregate content10.1016/j.conbuildmat.2022.129224 ↗
5. Appropriate drying shrinkage prediction models for lightweight concrete containing coarse agro-waste aggregate
6. Autogenous shrinkage and drying shrinkage of recycled aggregate concrete: a review10.1016/j.jclepro.2021.126435 ↗
7. Creep and shrinkage of recycled aggregate concrete10.1016/j.conbuildmat.2009.02.018 ↗
8. Effects of glazed hollow beads on the drying shrinkage value and trend of recycled aggregate concrete
9. J.O. CASTAÑO, F. LOPEZ-GAYARRE, C.M. Lázaro Fernández, A. Domingo Cabo, A study on drying shrinkage and creep of recycled concrete aggregate, in: Proceedings of the Symposium of the International Association for Shell and Spatial Structures (50th. 2009. Valencia), Evolution and Trends in Design, Analysis and Construction of Shell and Spatial Structure, 2009.
10. Rheological behaviour of concrete made with fine recycled concrete aggregates – Influence of the superplasticizer10.1016/j.conbuildmat.2015.03.119 ↗
11. A systematic comparison of performance of recycled concrete fine aggregates with other alternative fine aggregates: an approach to find a sustainable alternative to river sand
12. Systematic comparison of different recycled fine aggregates from construction and demolition wastes in OPC concrete and PPC concrete
13. Prediction of the shrinkage behavior of recycled aggregate concrete: a review10.1016/j.conbuildmat.2014.12.102 ↗
14. Creep and drying shrinkage characteristics of concrete produced with coarse recycled concrete aggregate10.1016/j.cemconcomp.2011.08.004 ↗
15. Drying shrinkage model for recycled aggregate concrete accounting for the influence of parent concrete10.1016/j.engstruct.2019.109888 ↗
16. Recycled concrete as fine and coarse aggregates in concrete10.1680/macr.1987.39.141.214 ↗
17. J.D. Brito, R. Robles, Recycled aggregate concrete (RAC) methodology for estimating its long-term properties (2010).
18. Concrete with recycled aggregates: the Portuguese experimental research10.1617/s11527-010-9595-7 ↗
19. Structural concrete with simultaneous incorporation of fine and coarse recycled concrete aggregates: mechanical, durability and long-term properties10.1016/j.conbuildmat.2017.07.215 ↗
20. Shrinkage and creep performance of concrete with recycled aggregates from CDW plants10.1680/jmacr.17.00031 ↗
21. Time-dependent drying shrinkage model for concrete with coarse and fine recycled aggregate10.1016/j.cemconcomp.2019.103426 ↗
22. Xiao · 2018
23. Fully utilizing carbonated recycled aggregates in concrete: strength, drying shrinkage and carbon emissions analysis10.1016/j.jclepro.2022.134520 ↗
24. Compressive and shrinkage behaviors of recycled aggregate concrete containing recycled sand from weathered residual soil of granite and MgO expansion agent
25. Moisture diffusion coefficient of concrete under different conditions10.3390/buildings13102421 ↗
26. Effect of internal curing on internal relative humidity and shrinkage of high strength concrete slabs10.1016/j.conbuildmat.2014.02.060 ↗
27. Early shrinkage experiment of concrete and the development law of its temperature and humidity field in natural environment
28. Implementing capillary pressure control measures to prevent plastic shrinkage cracking in concrete10.1016/j.conbuildmat.2023.132407 ↗
29. Effect of sulfoaluminate expansive additive on mechanical properties, internal relative humidity, and shrinkage of early-age mortar
30. Hydration products, internal relative humidity and drying shrinkage of alkali activated slag mortar with expansion agents10.1016/j.conbuildmat.2017.09.162 ↗
31. X. Ge, Relationship between internal relative humidity and drying shrinkage of concrete, Harbin Institute of Technology, 2013 (in Chinese).
32. Desorption experimental analysis and modeling of drying shrinkage and relative humidity in non-saturated concrete10.4028/www.scientific.net/AMR.368-373.725 ↗
33. Prediction model of internal humidity and drying shrinkage of recycled aggregate thermal insulation concrete[J]
34. GB/T 14684-2022 · 2022
35. GB/T 14685-2022 · 2022
36. Influence of the pre-saturation of recycled coarse concrete aggregates on concrete properties10.1680/macr.2011.63.8.617 ↗
37. Ministry of Housing and Urban–Rural Development of the People’s Republic of China · 2011
38. Prediction of the elastic modulus and the splitting tensile strength of concrete incorporating both fine and coarse recycled aggregate10.1016/j.conbuildmat.2019.04.212 ↗
39. The effect of superplasticisers on the workability and compressive strength of concrete made with fine recycled concrete aggregates10.1016/j.conbuildmat.2011.10.050 ↗
40. Optimization on proportion for recycled aggregate in concrete using two-stage mixing approach10.1016/j.conbuildmat.2006.05.040 ↗
41. Ministry of Housing and Urban-Rural Development of the People's Republic of China · 2016
42. Ministry of Housing and Urban-Rural Development of the People's Republic of China · 2019
43. Ministry of Housing and Urban-Rural Development of the People's Republic of China · 2009
44. Influence of moisture conditioning of recycled aggregates on the properties of fresh and hardened concrete10.1016/j.jclepro.2013.05.009 ↗
45. Performance enhancement of recycled concrete aggregate – A review10.1016/j.jclepro.2015.08.057 ↗
46. Effect of residual mortar on compressive properties of modeled recycled coarse aggregate concrete10.1016/j.conbuildmat.2023.132511 ↗
47. Rheology of recycled fine aggregate concrete and its effect on strength and durability
48. Relative humidity evolution of high performance concrete caused by self-desiccation and moisture diffusion[J]
49. Tests and prediction model for time-dependent internal relative humidity of recycled aggregate concrete due to self-desiccation10.1016/j.conbuildmat.2022.129024 ↗
50. Use of recycled fine clay brick aggregate as internal curing agent for low water to cement ratio mortar10.1016/j.conbuildmat.2020.120280 ↗
51. Long-term shrinkage and mechanical properties of fully recycled aggregate concrete: testing and modelling10.1016/j.cemconcomp.2022.104527 ↗
52. Effects of printing paths and recycled fines on drying shrinkage of 3D printed mortar10.1016/j.conbuildmat.2022.128007 ↗
53. Time-dependent behaviour of structural concrete made with recycled coarse aggregates. Creep and shrinkage10.1016/j.conbuildmat.2016.06.050 ↗
54. Effect of internal curing with super absorbent polymers on autogenous shrinkage of concrete at early age10.1016/j.conbuildmat.2015.12.115 ↗
55. The elastic constants of a solid containing spherical holes10.1088/0370-1301/63/1/302 ↗
56. Relationship between autogenous deformation and internal relative humidity of high-strength expansive concrete10.1007/s11595-010-0032-0 ↗
57. Microstructure-based modelling of drying shrinkage and microcracking of cement paste at high relative humidity10.1016/j.conbuildmat.2016.09.066 ↗