journal article·2023-11

Mechanisms and differences between sodium and magnesium sulfate attacks on alkali-activated phosphorus slag

Ruiquan Jia, Qiang Wang, Ting Luo

Publisher page

Abstract

To promote the application of alkali-activated phosphorus slag (AAPS), a new type of alkali-activated cement (AAC), this study revealed the mechanisms and differences between Na 2SO 4 and MgSO 4 attacks. During Na 2SO 4 exposure, the deterioration of AAPS was caused by the expansion of calcium-sodium aluminosilicate hydrate (C-N-A-S-H). The dealkalization of C-N-A-S-H was accelerated by the formation of (NaOH) 0, which promoted the polymerization shrinkage of C-N-A-S-H and improved the volume stability of AAPS. During MgSO 4 exposure, the deterioration of AAPS was caused by C-N-A-S-H deterioration and Mg(OH) 2 expansion, but the Mg(OH) 2 layer protected the AAPS from MgSO 4 attack. The dealkalization, decalcification and dealumination of C-N-A-S-H was accelerated by the formation of Mg(OH) 2 and (NaSO 4) −, transforming C-N-A-S-H into magnesium-sodium aluminosilicate hydrate (M-N-A-S-H). The resistance of AAPS to Na 2SO 4 was excellent, but its resistance to MgSO 4 was poorer. These differences were caused by the different binding capacities of Mg 2+ and Na + with OH − and the different degrees of forward movement of the dissolution equilibrium of C-N-A-S-H caused by Na 2SO 4 and MgSO 4.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Concrete and Cement Materials Research · Recycled Aggregate Concrete Performance · Magnesium Oxide Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (55)

Show source-provided references
1. Compressive strength and microstructure of alkali-activated waste glass-slag cements
2. One-part alkali-activated materials: A review10.1016/j.cemconres.2017.10.001 ↗
3. Boosting the performance of low-carbon alkali activated slag with APEG PCEs: a comparison with ordinary Portland cement
4. Electrochemical oxidation of recycled carbon fibers for an improved interaction toward alkali-activated composites10.1016/j.jclepro.2022.133093 ↗
5. Effect of superabsorbent polymers and expansive additives on the shrinkage of alkali-activated slag10.1016/j.cemconcomp.2021.104218 ↗
6. Effects of alkali dosage and silicate modulus on alkali-silica reaction in alkali-activated slag mortars10.1016/j.cemconres.2018.06.005 ↗
7. Efflorescence and subflorescence induced microstructural and mechanical evolution in fly ash-based geopolymers10.1016/j.cemconcomp.2018.06.010 ↗
8. Effect of alkali dosage and silicate modulus on carbonation of alkali-activated slag mortars10.1016/j.cemconres.2018.07.005 ↗
9. Resistance of alkali-activated slag concrete to acid attack10.1016/S0008-8846(03)00125-X ↗
10. Influence of activator composition on the chloride binding capacity of alkali-activated slag10.1016/j.cemconcomp.2019.103368 ↗
11. External sulfate attack on alkali-activated slag10.1016/j.conbuildmat.2013.08.013 ↗
12. Durability of low-calcium fly ash based geopolymer concrete culvert in a saline environment10.1016/j.cemconres.2017.07.010 ↗
13. Mechanism of sulfate attack on alkali-activated slag: The role of activator composition10.1016/j.cemconres.2019.105868 ↗
14. Microstructural changes in alkali activated fly ash/slag geopolymers with sulfate exposure10.1617/s11527-012-9906-2 ↗
15. Expansion behavior and microstructure change of alkali-activated slag grouting material in sulfate environment10.1016/j.conbuildmat.2020.119909 ↗
16. The long-term failure mechanisms of alkali-activated slag mortar exposed to wet-dry cycles of sodium sulphate10.1016/j.cemconcomp.2020.103893 ↗
17. Insights to the sulfate resistance and microstructures of alkali-activated metakaolin/slag pastes10.1016/j.clay.2020.105968 ↗
18. Modification of phase evolution in alkali-activated blast furnace slag by the incorporation of fly ash10.1016/j.cemconcomp.2013.09.006 ↗
19. Rheology of activated phosphorus slag with lime and alkaline salts10.1016/j.cemconres.2018.07.010 ↗
20. Understanding the acting mechanism of NaOH adjusting the transformation of viscoelastic properties of alkali activated phosphorus slag10.1016/j.conbuildmat.2020.119488 ↗
21. Understanding the workability of alkali-activated phosphorus slag pastes: Effects of alkali dose and silicate modulus on early-age hydration reactions10.1016/j.cemconcomp.2022.104649 ↗
22. Rheology and apparent activation energy of alkali activated phosphorous slag10.1016/j.conbuildmat.2018.03.130 ↗
23. The effect of NaOH content on rheological properties, microstructures and interfacial characteristic of alkali activated phosphorus slag fresh pastes10.1016/j.conbuildmat.2020.119132 ↗
24. Effect of fly ash microsphere on the rheology and microstructure of alkali-activated fly ash/slag pastes10.1016/j.cemconres.2018.04.008 ↗
25. GB/T 17671-2021, Test method of cement mortar strength (ISO method), Standardization Administration, Beijing, 2021, p. 10-11.
26. Durability of phosphogypsum-based supersulfated cement mortar against external attack by sodium and magnesium sulfate
27. P. Li, S. Liu, Y. Bai, et al., Research on rheology performance and sealing effect of alkali-activated GGBS paste used for tunnel leakage plugging, J. Sustain. Cem-Based, (2023).10.1080/21650373.2023.2219256 ↗
28. Effect of slag content and activator dosage on the resistance of fly ash geopolymer binders to sulfuric acid attack10.1016/j.cemconres.2018.06.011 ↗
29. Phase evolution of C-(N)-A-S-H/N-A-S-H gel blends investigated via alkali-activation of synthetic calcium aluminosilicate precursors10.1016/j.cemconres.2016.08.010 ↗
30. Gel nanostructure in alkali-activated binders based on slag and fly ash, and effects of accelerated carbonation10.1016/j.cemconres.2013.06.007 ↗
31. Generalized structural description of calcium-sodium aluminosilicate hydrate gels: The cross-linked substituted tobermorite model10.1021/la4000473 ↗
32. Atomic structure and phase assemblages in novel M-(N)-A-S-H materials10.1016/j.cemconres.2020.106336 ↗
33. Crystal structure of magnesium silicate hydrates (M-S-H): The relation with 2:1 Mg-Si phyllosilicates10.1016/j.cemconres.2015.03.014 ↗
34. Effect of magnesium silicate hydrate (M-S-H) formation on the local atomic arrangements and mechanical properties of calcium silicate hydrate (C-S-H): In situ X-ray scattering study10.1016/j.cemconres.2022.106869 ↗
35. Pore solution composition of alkali-activated slag/fly ash pastes10.1016/j.cemconres.2018.10.010 ↗
36. Influence of limestone on the hydration of Portland cements10.1016/j.cemconres.2008.01.002 ↗
37. Advances in understanding alkali-activated materials10.1016/j.cemconres.2015.04.013 ↗
38. Influence of activator type on hydration kinetics, hydrate assemblage and microstructural development of alkali activated blast-furnace slags10.1016/j.cemconres.2010.11.016 ↗
39. Influence of slag chemistry on the hydration of alkali-activated blast-furnace slag-Part II: Effect of Al2O310.1016/j.cemconres.2011.08.005 ↗
40. Hydration properties of steel slag under autoclaved condition10.1007/s10973-015-4397-3 ↗
41. Sulfate resistance of ferrochrome slag based geopolymer concrete10.1016/j.ceramint.2015.09.058 ↗
42. Nanoscale chemical degradation mechanisms of sulfate attack in alkali-activated slag10.1021/acs.jpcc.7b11270 ↗
43. Metakaolin-based geopolymers: Relation between formulation, physicochemical properties and efflorescence formation10.1016/j.compositesb.2019.107671 ↗
44. Strategies for control and mitigation of efflorescence in metakaolin-based geopolymers10.1016/j.cemconres.2021.106431 ↗
45. Early stage dissolution characteristics of aluminosilicate glasses with blast furnace slag- and fly-ash-like compositions10.1111/jace.14716 ↗
46. Reaction kinetics and kinetics models of alkali activated phosphorus slag10.1016/j.conbuildmat.2019.117728 ↗
47. Mechanisms of enhancement in early hydration by sodium sulfate in a slag-cement blend-Insights from pore solution chemistry10.1016/j.cemconres.2020.106110 ↗
48. Modeling of aqueous species interaction energies prior to nucleation in cement-based gel systems10.1016/j.cemconres.2020.106266 ↗
49. Effects of pH on the nano/micro structure of calcium silicate hydrate (C-S-H) under sulfate attack10.1016/j.cemconres.2020.106306 ↗
50. Hydration of potassium citrate-activated BOF slag10.1016/j.cemconres.2020.106291 ↗
51. Characterization of novel blast-furnace slag cement pastes and mortars activated with a reactive mixture of MgO-NaOH10.1016/j.cemconres.2018.01.002 ↗
52. Effect of NaOH content on hydration, mineralogy, porosity and strength in alkali/sulfate-activated binders from ground granulated blast furnace slag and phosphogypsum10.1016/j.cemconres.2020.106054 ↗
53. Gel composition and molecular structure of alkali-activated metakaolin-limestone cements10.1016/j.cemconres.2020.106211 ↗
54. Multiscale micromechanical analysis of alkali-activated fly ash-slag paste10.1016/j.cemconres.2020.106141 ↗
55. Strength and hydration properties of reactive MgO-activated ground granulated blastfurnace slag paste10.1016/j.cemconcomp.2014.10.007 ↗