Effect of Alloying Powders on Microstructure and Mechanical Properties of Aluminum Alloy Arc Additive Manufacturing
Source abstract
Abstract
Cold metal transfer arc additive manufacturing technique was used to produce 5356 aluminum alloy by adding refining agents to solve the problems of coarse grains and poor performance. Metallic powders (Ti, TiH, and Ti+B 4 C) were used to refine the grain size and promote the mechanical properties of the alloy. The effects of refining agents on the microstructure and mechanical properties of straight wall samples (SWSs) were studied. Samples with Ti+B 4 C addition had a profound impact on morphology. However, the TiH added sample revealed uneven transition between sediment layers, unstable precipitation process, unstable wall height and wall width, poor morphology, and defects. All SWSs with powder addition revealed the formation of the Al 3 Ti phase. Moreover, the columnar grains between the layers were transformed into equiaxed grains and finer grains at the center of the layers. There was a significant effect of TiH on the grain refinement. The samples with Ti demonstrated superior mechanical properties. The tensile strength and elongation of the SWSs increased by 28 MPa and 4.6% in the parallel additive direction and by 37 MPa and 8.9% in the vertical direction. The addition of Ti also contributed to the even distribution of the mechanical properties in both directions.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
School of Material Science and Engineering, Hebei University of Science and Technology, Shijiazhuang, China.
Hebei Key Laboratory of Material Near-Net Forming Technology, Shijiazhuang, China.
School of Sciences, Hebei University of Science and Technology, Shijiazhuang, China.
School of Engineering, University of Waikato, Hamilton, New Zealand.
School of Mechanical Engineering, Hebei University of Science and Technology, Shijiazhuang, China.
References (42)
Show source-provided references
1. 10.1016/j.matlet.2017.11.11110.1016/j.matlet.2017.11.111 ↗
2. Xu CX. Study on Synthesis and Grain-Refining Efficiency of Al-Ti-C Based Master Alloy. Taiyuan: Taiyuan University of Technology 2010.
3. 10.1089/3dp.2019.017610.1089/3dp.2019.0176 ↗
4. 10.1016/j.matdes.2012.03.05610.1016/j.matdes.2012.03.056 ↗
5. 10.1016/j.jmrt.2020.04.06210.1016/j.jmrt.2020.04.062 ↗
6. Bai JY, , Wang JH, , Shi JH, et al. Microstructure and mechanical properties of 4043-A1 alloy thin-walled components produced by additive manufacturing with TIG welding. Weld, 2015; 10:23–26.
7. Shi JH. Numerical Simulation and Microstructure Analysis of 5183 Aluminum Alloy TIG Additive Manufacturing. Harbin: Harbin Institute of Technology 2016.
8. 10.1016/j.msea.2017.11.11310.1016/j.msea.2017.11.113 ↗
9. 10.1016/j.msea.2015.12.10110.1016/j.msea.2015.12.101 ↗
10. 10.1016/j.jmatprotec.2018.04.01410.1016/j.jmatprotec.2018.04.014 ↗
11. 10.1007/BF0270863010.1007/BF02708630 ↗
12. 10.1016/j.matchar.2017.12.00410.1016/j.matchar.2017.12.004 ↗
13. Sun XY. Study on Refinement Mechanism of Al-Ti-B and Al-Ti-C Master Alloys in Aluminum and Its Alloys. Beijing: Tsinghua University 2011.
14. Hei YD, , Zhang XM. Refinement mechanism of trace Cr, Mn, Ti and Zr as cast 7A55 alloys. Chin J Nonferrous Met, 2005; 10:118–125.
15. 10.1007/BF0339742410.1007/BF03397424 ↗
16. Wang Q. Study on the Microstructure and Mechanical Properties of Aluminum Alloys Modified and Refined by the New Composite Inoculants. Tianjin: Hebei University of Technology 2017.
17. 10.1179/09506600122500104910.1179/095066001225001049 ↗
18. 10.1016/j.phpro.2011.03.01610.1016/j.phpro.2011.03.016 ↗
19. 10.1179/13621719910153803010.1179/136217199101538030 ↗
20. 10.1016/j.jallcom.2010.09.04610.1016/j.jallcom.2010.09.046 ↗
21. Yang CG, , Ji HG, , Huang ZB, et al. Effect of Ti, Zr elements on microstructure and mechanical properties of 2A12 aluminum alloy weld. Hot Working Technol, 2018; 3:210–212.
22. 10.1016/j.jmatprotec.2014.10.02310.1016/j.jmatprotec.2014.10.023 ↗
23. Janakiram GD, , Mitra TK, , Shankar V, et al. Microstructural refinement through inoculation of type 7020 Al-Zn-Mg alloy welds and its effect on hot cracking and tensile properties. J Mater Process Technol, 2003; 142:1174–1181.
24. 10.1016/j.optlastec.2018.09.03610.1016/j.optlastec.2018.09.036 ↗
25. 10.1016/j.optlastec.2020.10654010.1016/j.optlastec.2020.106540 ↗
26. 10.1016/j.matlet.2019.01.11710.1016/j.matlet.2019.01.117 ↗
27. 10.1016/j.addma.2020.10120010.1016/j.addma.2020.101200 ↗
28. 10.1016/j.jallcom.2016.11.04910.1016/j.jallcom.2016.11.049 ↗
29. 10.1016/j.msea.2020.14055710.1016/j.msea.2020.140557 ↗
30. 10.1016/j.jmapro.2020.10.00710.1016/j.jmapro.2020.10.007 ↗
31. Zhou Dk, , Chen XH. The removal of aluminum from alcohol. Chin J Hosp Pharm, 1982; 06:57.
32. 10.1016/j.matdes.2019.10835710.1016/j.matdes.2019.108357 ↗
33. Rui FA, , St A, , Ji A, et al. Hot-wire arc additive manufacturing of aluminum alloy with reduced porosity and high deposition rate. Mater Design, 2020; 199:109370.
34. 10.1016/j.jmatprotec.2015.11.00610.1016/j.jmatprotec.2015.11.006 ↗
35. Ma MW, , Wang L, , Tang BH, et al. Kinetics of hydrogen desorption from titanium hydride under isothermal conditions. Int J Hydrogen Energ, 2017; 3:1577–1586.
36. Gao Y. Interaction mechanisms between low-angle grain boundaries and dislocations in face centered cubic metals: molecular dynamics simulations. Shanghai: Shanghai Jiaotong University 2017.
37. 10.1016/j.ijrmhm.2015.01.01410.1016/j.ijrmhm.2015.01.014 ↗
38. Zeng Z, , Cong BQ, , Oliveira JP, et al. Wire and arc additive manufacturing of a Ni-rich NiTi shape memory alloy: Microstructure and mechanical properties. Addit Manuf, 2020:101051.
39. 10.1016/j.scriptamat.2019.12.01210.1016/j.scriptamat.2019.12.012 ↗
40. 10.1088/0370-1301/64/9/30310.1088/0370-1301/64/9/303 ↗
41. Petch NJ. The cleavage strength of polycrystals. J Iron Steel Inst, 1953; 174:25–28.
42. 10.1016/j.matdes.2009.05.04210.1016/j.matdes.2009.05.042 ↗