Deterioration and mitigation of efflorescence of alkali-activated phosphorus slag
Source abstract
Abstract
To achieve the efficient application of alkali-activated phosphorus slag (AAPS), this study revealed the efflorescence mechanisms and found a feasible way to mitigate the efflorescence deterioration. The efflorescence formations were mainly constituted of Na 2CO 3·H 2O, Na 3H(CO 3) 2·2H 2O and NaHCO 3. The order of the efflorescence ability of Na species was Na f (free Na in unreacted alkali activator) > Na w (weakly bonded Na in calcium-sodium aluminosilicate hydrate (CNASH)) > Na s (strongly bonded Na in CNASH). CNASH with lower Na/Si ratios and higher polymerization degrees was harder to form efflorescence. The accelerated efflorescence not only caused the dealkalization, dealumination and polymerization shrinkage of CNASH, but also deteriorated the homogeneity of CNASH distribution in pastes, due to the uneven carbonization of the upper and lower parts of pastes. The growth of efflorescence formation and the polymerization shrinkage of CNASH caused the upper parts of pastes to crack, which deteriorated the integrity of pastes. The accelerated efflorescence deteriorated the homogeneity and integrity of pastes. An effective strategy to mitigate the efflorescence and crack of pastes resulted from the addition of aggregates, which assisted in the development of compressive strength. AAPS mortars with low Na 2O doses or moderate silicate moduli had better resistance to efflorescence.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete and Cement Materials Research · Innovative concrete reinforcement materials · Recycled Aggregate Concrete Performance
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (48)
Show source-provided references
1. New insights on dehydration at elevated temperature and rehydration of GGBS blended cement10.1016/j.cemconcomp.2023.105068 ↗
2. The effects of cations and concentration on reaction mechanism of alkali-activated blast furnace ferronickel slag10.1016/j.compositesb.2022.109825 ↗
3. One-part alkali-activated materials: A review10.1016/j.cemconres.2017.10.001 ↗
4. Alkali-activated binders: A review. Part 2. About materials and binders manufacture10.1016/j.conbuildmat.2007.03.019 ↗
5. Investigations on the rehydration of recycled blended SCMs cement10.1016/j.cemconres.2022.107036 ↗
6. The durability of alkali-activated materials in comparison with ordinary portland cements and concretes: A review
7. Effect of nano-silica on the efflorescence of waste based alkali-activated inorganic binder10.1016/j.conbuildmat.2018.02.006 ↗
8. Effect of zeolite on waste based alkali-activated inorganic binder efflorescence10.1016/j.conbuildmat.2017.10.065 ↗
9. Effect of silica fume on efflorescence formation and alkali leaching of alkali-activated slag10.1016/j.jclepro.2021.128210 ↗
10. Mitigation of efflorescence of alkali-activated slag mortars by incorporating calcium hydroxide10.1016/j.conbuildmat.2021.123873 ↗
11. Microstructure and properties of fly ash-based geopolymeric material with 5A zeolite as a filler10.1016/j.conbuildmat.2012.01.014 ↗
12. Phase changes under efflorescence in alkali activated materials with mixed activators10.1016/j.conbuildmat.2021.122678 ↗
13. Fly ash-based geopolymers: The relationship between composition, pore structure and efflorescence10.1016/j.cemconres.2014.06.004 ↗
14. Compressive strength development and shrinkage of alkali-activated fly ash-slag blends associated with efflorescence10.1617/s11527-015-0694-3 ↗
15. Effects of Si/Al ratio on the structure and properties of metakaolin based geopolymer10.1016/j.ceramint.2016.06.033 ↗
16. Efflorescence control in geopolymer binders based on natural pozzolan10.1016/j.cemconcomp.2011.07.007 ↗
17. High strength geopolymer binder based on waste-glass powder10.1016/j.apt.2016.09.034 ↗
18. Strategies for control and mitigation of efflorescence in metakaolin-based geopolymers10.1016/j.cemconres.2021.106431 ↗
19. Metakaolin-based geopolymers: Relation between formulation, physicochemical properties and efflorescence formation10.1016/j.compositesb.2019.107671 ↗
20. Efflorescence and subflorescence induced microstructural and mechanical evolution in fly ash-based geopolymers10.1016/j.cemconcomp.2018.06.010 ↗
21. Rheology of activated phosphorus slag with lime and alkaline salts10.1016/j.cemconres.2018.07.010 ↗
22. Understanding the acting mechanism of NaOH adjusting the transformation of viscoelastic properties of alkali activated phosphorus slag10.1016/j.conbuildmat.2020.119488 ↗
23. Understanding the workability of alkali-activated phosphorus slag pastes: Effects of alkali dose and silicate modulus on early-age hydration reactions10.1016/j.cemconcomp.2022.104649 ↗
24. Reaction kinetics and kinetics models of alkali activated phosphorus slag10.1016/j.conbuildmat.2019.117728 ↗
25. Rheology and apparent activation energy of alkali activated phosphorous slag10.1016/j.conbuildmat.2018.03.130 ↗
26. Alkali-activated phosphorous slag performance under different curing conditions: compressive strength, hydration products, and microstructure10.1061/(ASCE)MT.1943-5533.0002101 ↗
27. The effect of NaOH content on rheological properties, microstructures and interfacial characteristic of alkali activated phosphorus slag fresh pastes10.1016/j.conbuildmat.2020.119132 ↗
28. Effect of fly ash microsphere on the rheology and microstructure of alkali-activated fly ash/slag pastes10.1016/j.cemconres.2018.04.008 ↗
29. GB/T 17671-2021, Test method of cement mortar strength (ISO method), Standardization Administration, Beijing, 2021.
30. Effect of alkali dosage and silicate modulus on carbonation of alkali-activated slag mortars10.1016/j.cemconres.2018.07.005 ↗
31. Clarifying and quantifying the immobilization capacity of cement pastes on heavy metals10.1016/j.cemconres.2022.106945 ↗
32. Mechanisms of enhancement in early hydration by sodium sulfate in a slag-cement blend-Insights from pore solution chemistry10.1016/j.cemconres.2020.106110 ↗
33. Phase evolution of C-(N)-A-S-H/N-A-S-H gel blends investigated via alkali-activation of synthetic calcium aluminosilicate precursors10.1016/j.cemconres.2016.08.010 ↗
34. Morphology-structural change of C-A-S-H gel in blended cements10.1016/j.cemconres.2023.107156 ↗
35. Operando visualisation of battery chemistry in a sodium-ion battery by 23Na magnetic resonance imaging10.1038/s41467-020-15938-x ↗
36. Generalized structural description of calcium-sodium aluminosilicate hydrate gels: The cross-linked substituted tobermorite model10.1021/la4000473 ↗
37. Salt weathering of concrete by sodium carbonate and sodium chloride
38. Carbonation in the pore solution of metakaolin-based geopolymer10.1016/j.cemconres.2016.05.008 ↗
39. Influence of activator type on hydration kinetics, hydrate assemblage and microstructural development of alkali activated blast-furnace slags10.1016/j.cemconres.2010.11.016 ↗
40. Influence of slag chemistry on the hydration of alkali-activated blast-furnace slag - Part II: Effect of Al2O310.1016/j.cemconres.2011.08.005 ↗
41. A.M. Kaja, K. Schollbach, S. Melzer, et al., Hydration of potassium citrate-activated BOF slag, Cement Concrete Res. 140 (2021) 106291.10.1016/j.cemconres.2020.106291 ↗
42. Characterization of novel blast-furnace slag cement pastes and mortars activated with a reactive mixture of MgO-NaOH10.1016/j.cemconres.2018.01.002 ↗
43. Structure of calcium silicate hydrates formed in alkaline-activated slag: influence of the type of alkaline activator10.1111/j.1151-2916.2003.tb03481.x ↗
44. Hydration degree of alkali-activated slags: A 29Si NMR study10.1111/j.1551-2916.2011.04828.x ↗
45. Multiscale micromechanical analysis of alkali-activated fly ash-slag paste10.1016/j.cemconres.2020.106141 ↗
46. Modification of phase evolution in alkali-activated blast furnace slag by the incorporation of fly ash10.1016/j.cemconcomp.2013.09.006 ↗
47. Nanoscale chemical degradation mechanisms of sulfate attack in alkali-activated slag10.1021/acs.jpcc.7b11270 ↗
48. Effects of pH on the nano/micro structure of calcium silicate hydrate (C-S-H) under sulfate attack10.1016/j.cemconres.2020.106306 ↗