journal article·2024-08

Early performance modification of a waste-derived super-sulfated cement from arsenic-containing bio-oxidation waste via calcium aluminate and calcium sulfoaluminate cement

Jin Hongmei, Yu Hongwen, Fu Zhiyong, Shan Longhui, Zhang Shiyu, Zhao Yingliang

Publisher page

Abstract

The study investigated the effects of calcium aluminate cement (CAC) and calcium sulfoaluminate cement (CSA) on the early hydration kinetics of super-sulfated cement (SSC) derived from arsenic-containing bio-oxidation waste (BW) to enhance its early strength development. The results demonstrated that the minor addition of both CAC and CSA significantly promoted SSC hydration, leading to improved early-age strength, with CAC showing superior performance. The incorporation of 0.5 wt% CAC (CAC10) resulted in a substantial increase in compressive strength at 1 d and 3 d by approximately 37.2 % and 22.5 %, respectively, which was attributed to the in-situ formation of ettringite (AFt) serving as nucleation sites for further precipitation. Nano-indentation analysis indicated that C-S-H gels formed in the presence of CAC demonstrated increased values of elastic modulus and hardness, which contributed to favorable conditions for SSC strength development. However, a higher dosage of CAC and CSA imposed restrictions on the early reaction of SSC, which were linked to reduced alkalinity and limitations in blast furnace slag (BFS) dissolution. Moreover, effective arsenic immobilization in SSC from BW was observed, and the life cycle assessment (LCA) indicated lower environmental impacts compared to ordinary Portland cement (OPC).
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Concrete and Cement Materials Research · Recycling and utilization of industrial and municipal waste in materials production · Recycled Aggregate Concrete Performance

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (57)

Show source-provided references
1. Mechanism underlying early hydration kinetics of carbonated recycled concrete fines-ordinary portland cement (CRCF-OPC) paste10.1016/j.cemconcomp.2023.105275 ↗
2. An innovative strategy for maximizing CO2 reduction in concrete through preparing carbon sequestration precursors by accelerated carbonation10.1016/j.cemconcomp.2024.105618 ↗
3. Highly reactive carbonated recycled concrete fines prepared via mechanochemical carbonation: influence on the early performance of cement composites10.1016/j.cemconcomp.2024.105636 ↗
4. Study of strength and microstructure of a new sustainable concrete incorporating pozzolanic materials
5. Enhancement fracture behavior of sustainable cementitious composites using synergy between fly ash (FA) and nanosilica (NS) in the assessment based on digital image processing procedure10.1016/j.tafmec.2024.104442 ↗
6. Assessing of water absorption on concrete composites containing fly ash up to 30% in regards to structures completely immersed in water
7. Research status of super sulfate cement10.1016/j.jclepro.2021.126228 ↗
8. Examining the hydration mechanism of supersulfated cements made with high and low-alumina slags10.1016/j.cemconcomp.2019.05.001 ↗
9. Effect of NaOH content on hydration, mineralogy, porosity and strength in alkali/sulfate-activated binders from ground granulated blast furnace slag and phosphogypsum10.1016/j.cemconres.2020.106054 ↗
10. Application of lime neutralised phosphogypsum in supersulfated cement10.1016/j.jclepro.2020.122660 ↗
11. The influence of two types of alkali activators on the microstructure and performance of supersulfated cement concrete: mitigating the strength and carbonation resistance10.1016/j.cemconcomp.2021.103947 ↗
12. Influence of the calcination temperature of phosphogypsum on the performance of supersulfated cements10.1016/j.conbuildmat.2020.119961 ↗
13. Hydration mechanism of calcium sulfoaluminate-activated supersulfated cement10.1016/j.jclepro.2021.130094 ↗
14. Novel low emissions supersulfated cements of pumice in concrete; mechanical and electrochemical characterization10.1016/j.jclepro.2020.122520 ↗
15. On the retardation mechanisms of citric acid in ettringite-based binders10.1016/j.cemconres.2020.106315 ↗
16. Recycling of arsenic-containing biohydrometallurgy waste to produce a binder for cemented paste backfill: mix proportion optimization10.1016/j.powtec.2022.117155 ↗
17. Recycling of arsenic-containing biohydrometallurgy waste to produce a binder for cemented paste backfill: influence of additives
18. Studies on the influence of spent FCC catalyst on hydration of calcium aluminate cements at ambient temperature10.1007/s10973-011-1303-5 ↗
19. Kurdowski W. Chemistry of cement and concrete. Polski Cement, Kraków 2010.
20. Microstructure development in mixes of calcium aluminate cement with silica fume or fly ash10.1007/s10973-007-8439-3 ↗
21. Scientific aspects of high alumina cement
22. The effect of temperature on the formation of the hydrated calcium aluminate cement structure10.1016/j.proeng.2013.04.015 ↗
23. Studies of conversion progress of calcium aluminate cement hydrates by thermal analysis method10.1007/s10973-014-3804-5 ↗
24. Understanding expansion in calcium sulfoaluminate–belite cements10.1016/j.cemconres.2011.07.010 ↗
25. Advances in alternative cementitious binders10.1016/j.cemconres.2010.11.012 ↗
26. Mechanism of hydration reactions in the system C4A3S-CS-CaO-H2O referred to hydration of sulphoaluminate cements10.1016/0008-8846(89)90038-0 ↗
27. Comparison on early hydration of Portland cement and sulphoaluminate cement in the presence of nano ettringite10.1016/j.conbuildmat.2022.129516 ↗
28. Removal and immobilization of arsenic from copper smelting wastewater using copper slag by in situ encapsulation with silica gel10.1016/j.cej.2020.124833 ↗
29. Efficient removal of arsenic from “dirty acid” wastewater by using a novel immersed multi-start distributor for sulphide feeding10.1016/j.seppur.2014.12.029 ↗
30. Physicochemical properties of arsenic-bearing lime–ferrate sludge and its leaching behaviors10.1016/S1003-6326(17)60140-7 ↗
31. Immobilization capacity assessment of a binder from arsenic-containing biohydrometallurgy waste: effects of halloysite nanotubes and biochar addition
32. Increasing arsenic immobilization capacity of a binder prepared by arsenic-containing biohydrometallurgy waste: effects of ferric/ferrous salts addition10.1016/j.jece.2023.110206 ↗
33. Calorimetric study of ternary binder of calcium aluminate cement, Portland-limestone cement and FGD gypsum10.1007/s10973-009-0542-1 ↗
34. Scrivener KarenA practical guide to microstructural analysis of cementitious materials Taylor Fr. Group (ed.) , 2016.
35. Recycling of arsenic-containing biohydrometallurgy waste to produce a binder for cemented paste backfill: Co-treatment with oil shale residue10.1016/j.jenvman.2022.115621 ↗
36. An insight of carbonation-hydration kinetics and microstructure characterization of cement paste under accelerated carbonation at early age10.1016/j.cemconcomp.2022.104763 ↗
37. Mechanisms of carbonation hydration hardening in Portland cements10.1016/j.cemconres.2021.106687 ↗
38. Mechanism of hydration reactions in the system C4A3S CS CaO H2O referred to hydration of sulphoaluminate cements10.1016/0008-8846(89)90038-0 ↗
39. Hydration of ordinary Portland cement and calcium sulfoaluminate cement blends10.1016/j.cemconcomp.2014.11.005 ↗
40. Influence of calcium sulfate and calcium hydroxide on the hydration of calcium sulfoaluminate clinker
41. Insights on the molecular structure evolution for tricalcium silicate and slag composite: from 29Si and 27Al NMR to molecular dynamics10.1016/j.compositesb.2020.108401 ↗
42. Blast furnace slag cement: a 29Si and 27Al NMR study10.1016/j.crci.2004.02.004 ↗
43. Recycling utilization of phosphogypsum in eco excess-sulphate cement: synergistic effects of metakaolin and slag additives on hydration, strength and microstructure10.1016/j.jclepro.2022.131901 ↗
44. Supersulfated cements based on pumice with quicklime, anhydrite and hemihydrate: characterization and environmental impact10.1016/j.cemconcomp.2021.104236 ↗
45. Carbonation of C–S–H and C–A–S–H samples studied by 13C, 27Al and 29Si MAS NMR spectroscopy10.1016/j.cemconres.2015.01.019 ↗
46. Enhancing the corrosion resistance of recycled aggregate concrete by incorporating waste glass powder10.1016/j.cemconcomp.2022.104909 ↗
47. The nanogranular behavior of CSH at elevated temperatures (up to 700C)10.1016/j.cemconres.2006.09.006 ↗
48. A multi-technique investigation of the nanoporosity of cement paste10.1016/j.cemconres.2006.03.021 ↗
49. The elastic moduli of calcium hydroxide10.1016/0008-8846(95)00154-9 ↗
50. The mechanisms of heavy metal immobilization by cementitious material treatments and thermal treatments: a review10.1016/j.jenvman.2017.02.026 ↗
51. Assessment of arsenic immobilization in synthetically prepared cemented paste backfill specimens10.1016/j.jenvman.2011.08.015 ↗
52. Competition behaviour of metal uptake in cementitious systems: an XRD and EXAFS investigation of Nd- and Zn-loaded 11Å tobermorite10.1016/j.pce.2014.01.001 ↗
53. Effective reuse of red mud as supplementary material in cemented paste backfill: durability and environmental impact10.1016/j.conbuildmat.2022.127002 ↗
54. Hydration of calcium sulfoaluminate cements — experimental findings and thermodynamic modelling10.1016/j.cemconres.2009.08.014 ↗
55. Recent progress and technical challenges in using calcium sulfoaluminate (CSA) cement10.1016/j.cemconcomp.2022.104908 ↗
56. The influence of calcium sulfate content on the hydration of belite-calcium sulfoaluminate cements with different clinker phase compositions10.1617/s11527-021-01811-w ↗
57. Effect of calcium sulfate source on the hydration of calcium sulfoaluminate eco-cement10.1016/j.cemconcomp.2014.08.003 ↗