Enhancing behavior of large volume underground concrete structure using expansive agents
Source abstract
Abstract
Abstract Many underground concrete structures suffer from issues of concrete cracking due to shrinkage during hydration, which furthermore results in water leakage. In order to improve the anti-crack ability of concrete, expansive agents were used to compensate for concrete shrinkage. This paper investigates enhancing the behavior of large volume underground concrete structures with expansive agents. Field measurements of strain and laboratory specimen tests were conducted. The results of concrete specimen in laboratory curing condition indicate that the restrained expansion ratio of concrete with expansive agents rapidly increases within the first 3 days. Restrained expansion ratio reaches the peak value after 14 days and then decreases with the elapsed time. The restrained expansion ratio was found to maintain a value of approximately 0.030% after 28 days. The developing trend of restrained expansion ratio of the field cured specimen was found to be similar as that of the specimen cured in laboratory. However, the peak value and average value of restrained expansion ratio of the field cured specimen was found to be smaller than those of the laboratory cured specimen. The field test results indicate that the post-poured strips and post-poured expansive reinforcing band with expansive agents can effectively increase the expansive strain of concrete, which furthermore indicates that expansive agents can enhance the crack prevention behavior of concrete structure in the field.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete Properties and Behavior · Concrete and Cement Materials Research · Innovative concrete reinforcement materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. Effects of shrinkage reducing admixtures on restrained shrinkage cracking of concrete
2. Interactions between shrinkage reducing admixtures (SRA) and cement10.1016/j.cemconres.2007.12.005 ↗
3. Shrinkage reducing admixtures and early-age desiccation in cement pastes and mortars10.1016/S0008-8846(01)00519-1 ↗
4. Numerical evaluation of land subsidence induced by groundwater pumping in Shanghai10.1139/t11-049 ↗
5. Assessment of internal forces for interior anchorage zone of post-tensioned concrete structure10.1016/j.conbuildmat.2014.04.085 ↗
6. Long-term settlement behavior of the metro tunnel in Shanghai10.1016/j.tust.2013.10.013 ↗
7. Evaluation of hydraulic conductivity for both marine and deltaic deposit based on piezocone test10.1016/j.oceaneng.2015.10.011 ↗
8. Longitudinal structural modelling of shield tunnels considering shearing dislocation between segmental rings10.1016/j.tust.2015.08.001 ↗
9. Evaluation of hydraulic parameter based on groundwater pumping test of multi-aquifer system of Tianjin10.1016/j.compgeo.2015.03.011 ↗
10. Characteristics of groundwater seepage with cutoff wall in gravel aquifer. I: field observations10.1139/cgj-2014-0285 ↗
11. Characteristics of groundwater seepage with cutoff wall in gravel aquifer. II: numerical analysis10.1139/cgj-2014-0289 ↗
12. Evaluation of the blocking effect of retaining walls on groundwater seepage in aquifers with different insertion depths10.1016/j.enggeo.2014.08.023 ↗
13. Structural behaviors of large underground earth-retaining systems in Shanghai. I: unpropped circular diaphragm wall
14. Structural behaviors of large underground earth-retaining systems in Shanghai. II: multipropped rectangular diaphragm wall10.1061/(ASCE)CF.1943-5509.0000535 ↗
15. Mitigation strategies for autogenous shrinkage cracking10.1016/S0958-9465(03)00045-3 ↗
16. Influence of temperature on autogenous deformation and relative humidity change in hardening cement paste10.1016/S0008-8846(99)00021-6 ↗
17. Combined effect of expansive and shrinkage reducing admixtures to control autogenous shrinkage in self-compacting concrete10.1016/j.conbuildmat.2013.11.033 ↗
18. Autogenous deformation and RH-change in perspective10.1016/S0008-8846(01)00501-4 ↗
19. Autogenous relative humidity change and autogenous shrinkage of high-performance cement pastes10.1016/j.cemconres.2004.06.028 ↗
20. Synthesis and evaluation of shrinkage-reducing admixture for cementitious materials10.1016/j.cemconres.2004.07.009 ↗
21. Influence of ring size on the restrained shrinkage behavior of ultra-high performance fiber reinforced concrete10.1617/s11527-013-0119-0 ↗
22. Plastic shrinkage cracking in cementitious repairs and overlays10.1617/s11527-008-9403-9 ↗
23. Plastic shrinkage cracking and evaporation formulas
24. Lea · 1976 · 533
25. Modification on FIP design model for interior anchorage zones of post-tensioned concrete structures10.1007/s12205-011-0835-3 ↗
26. Reducing the drying shrinkage of cement paste by admixture surface treatments10.1016/S0008-8846(99)00239-2 ↗
27. Shrinkage reducing admixtures
28. The effect of hybrid fibers and expansive agent on the shrinkage and permeability of high-performance concrete10.1016/S0008-8846(00)00479-8 ↗
29. Effects of shrinkage reducing admixture in shrinkage compensating concrete under non-wet curing conditions10.1016/j.cemconcomp.2004.09.020 ↗
30. Combined effect of expansive and shrinkage reducing admixtures to obtain stable and durable mortars10.1016/j.cemconres.2004.11.021 ↗
31. Formation and expansion of ettringite crystals10.1016/0008-8846(94)90092-2 ↗
32. Mechanism of sulphate expansion I. Thermodynamic principle of crystallization pressure10.1016/0008-8846(92)90015-N ↗
33. Mechanism of expansion of concrete due to the presence of dead burnt CaO and MgO10.1016/0008-8846(94)00111-B ↗
34. Mechanism of expansion associated with ettringite formation10.1016/0008-8846(73)90056-2 ↗
35. Self-healing behavior for crack closing of expansive agent via granulation/film coating method10.1016/j.conbuildmat.2014.08.045 ↗
36. The influence of expansive agent on the performance of fibre reinforced10.1016/j.conbuildmat.2015.05.002 ↗
37. Influence of a combination of expansive and shrinkage-reducing admixture on autogenous deformation and self-stress of silica fume high-performance concrete10.1016/j.conbuildmat.2010.06.033 ↗
38. Structural behavior of FRP enclosed shrinkage-compensating concrete (SHCC) beams made with different expansive agents10.1016/j.conbuildmat.2014.11.045 ↗
39. Expansive Synergic Effect of ettringite from pozzolan (metakaolin) and from OPC, co-precipitating in a common plaster-bearing solution: Part I: by cement pastes and mortars10.1016/j.conbuildmat.2010.02.009 ↗