Influence of curing methods and concentration of NaOH on strength of the synthesized alkaline activated ground slag-ultrafine palm oil fuel ash mortar/concrete

Moruf Olalekan Yusuf, Megat Azmi Megat Johari, Zainal Arifin Ahmad, Mohammed Maslehuddin

Publisher page

Abstract

Abstract Efficiency in energy-utilization in the adoption of curing methods and effects of NaOH aq concentration towards achieving a better strength performance in the synthesis of alkaline activated ground-steel-slag (GSS) with ultrafine palm-oil-fuel ash (UPOFA) – (AAGU) mortars and concrete prompted this study. AAGU samples were prepared with the combined activators (Na 2 SiO 3aq + NaOH aq : (Na 2 SiO 3aq + NaOH aq )/(GSS + UPOFA) = 0.5) while different curing methods namely: oven-cured (60 °C for 24 h), water-ponding and room-cured (25 °C) were also investigated. The findings showed that 76% and 50% of 28-day strength in the oven-cured mortars could be attained in water-ponding and room-curing, respectively. Regardless of the curing methods, GSS/(GSS+UPOFA) and Na 2 SiO 3aq /NaOH aq -ratios could significantly affect the strength development in AAGU mortars. The strength development in AAGU concrete depends on the NaOH aq concentration (NC). X-ray diffractogram (XRD), Fourier-transform infrared (FTIR) spectra, and scanning-electron-microscope coupled with energy-dispersive-spectroscopy (SEM + EDS) showed that strong alkali (10 M-NaOH aq ) influenced the microstructural-density, reduced carbonation and improved binder amorphousity than the mild alkali (4 M-NaOH aq ).
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Concrete and Cement Materials Research · Magnesium Oxide Properties and Applications · Innovative concrete reinforcement materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. Resistance to chloride penetration of blended Portland cement mortar containing palm oil fuel ash, rice husk ash and fly ash10.1016/j.conbuildmat.2006.12.001 ↗
2. Strength, drying shrinkage, and water permeability of concrete incorporating ground palm oil fuel ash10.1016/j.cemconcomp.2010.08.008 ↗
3. Use of ground palm oil fuel ash to improve strength, sulfate resistance, and water permeability of concrete containing high amount of recycled concrete aggregates10.1016/j.matdes.2012.04.054 ↗
4. Engineering and transport properties of high-strength green concrete containing high volume of ultrafine palm oil fuel ash10.1016/j.conbuildmat.2011.12.007 ↗
5. Synthesis of geopolymer from large amounts of treated palm oil fuel ash: application of the Taguchi method in investigating the main parameters affecting compressive strength10.1016/j.conbuildmat.2013.11.039 ↗
6. Evolution of alkaline activated ground blast furnace slag-ultrafine palm oil fuel ash based concrete10.1016/j.matdes.2013.09.047 ↗
7. Strength and microstructure of alkali-activated binary blended binder containing palm oil fuel ash and ground blast-furnace slag10.1016/j.conbuildmat.2013.11.012 ↗
8. Effects of addition of Al(OH)3 on the strength of alkaline activated ground blast furnace slag-ultrafine palm oil fuel ash (AAGU) based binder10.1016/j.conbuildmat.2013.09.054 ↗
9. Effects of H2O/Na2O molar ratio on the strength of alkaline activated ground blast furnace slag-ultrafine palm oil fuel ash based concrete10.1016/j.matdes.2013.09.078 ↗
10. Strength and microstructural performance of nano-SiO2 gel (NSG) infused alkaline activated ground blast furnace slag-ultrafine palm oil fuel ash (AAGU) based mortar10.4028/www.scientific.net/AMR.856.280 ↗
11. Inorganic polymers from alkali activation of metakaolin: effect of setting and curing on structure10.1016/j.jssc.2013.02.003 ↗
12. Influence of admixtures on the properties of alkali-activated slag mortars subjected to different curing conditions10.1016/j.matdes.2012.08.049 ↗
13. Role of microwave radiation in curing the fly ash geopolymer10.1016/j.apt.2012.12.005 ↗
14. The influence of the NaOH solution on the properties of the fly ash-based geopolymer mortar cured at different temperatures10.1016/j.compositesb.2013.10.082 ↗
15. Xie J, Kayali O. Effect of initial water content and curing moisture conditions on the development of fly ash-based geopolymers in heat and ambient temperature. Constr Build Mater 2013 [in press], http://dx.doi.org/10.1016/j.conbuildmat.2013.10.047.10.1016/j.conbuildmat.2013.10.047 ↗
16. Effects of dosage of alkali-activated solution and curing conditions on the properties and durability of alkali-activated slag concrete10.1016/j.conbuildmat.2012.04.005 ↗
17. Effects of NaOH concentrations on physical and electrical properties of high calcium fly ash geopolymer paste10.1016/j.cemconcomp.2013.09.012 ↗
18. Davidovits · 2011
19. The effects of Na2O/SiO2 molar ratio, curing temperature and age on compressive strength, morphology and microstructure of alkali-activated fly ash-based geopolymers10.1016/j.cemconcomp.2011.03.006 ↗
20. Geopolymeric materials prepared using class F fly ash elevated temperature curing10.1016/j.cemconres.2004.06.031 ↗
21. Properties of polypropylene composites filled with a mixture of household waste of mate-tea and wood particles10.1016/j.conbuildmat.2014.02.022 ↗
22. Physical properties and mechanical behaviour of concrete made with recycled aggregates and fly ash10.1016/j.conbuildmat.2013.04.051 ↗
23. ASTM: C-33. Standard specification for concrete aggregate. West Conshohocken, PA: ASTM International, American Society for Testing and Materials; 2001.
24. Low-calcium, fly-ash-based geopolymer concrete
25. Bakharev · 2000
26. Effect of binder content on the performance of alkali-activated slag concretes10.1016/j.cemconres.2010.08.017 ↗
27. Hydration of alkali activated ground granulated blast furnace slag10.1023/A:1004742027117 ↗
28. Provis · 2009
29. Role of water in the synthesis of calcined kaolin-based geopolymer10.1016/j.clay.2008.09.003 ↗
30. Roode M, Hemmings RT. Development of a unified theory for predicting the behaviour of glass waste products. Contract report no. ISQ83-00162. Canada: CANMET; 1985.