Corrosion performance of blended concretes exposed to different aggressive environments

Ana María Aguirre-Guerrero, Ruby Mejía-de-Gutiérrez, Maria João Ribeiro Montês-Correia

Publisher page

Abstract

Abstract The research study presented herein evaluates the corrosion behaviour of the reinforcing steel in blended concretes using two pozzolanic additives—metakaolin (MK) and silica fume (SF)—at 10% replacement of cement weight. They are exposed to CO2 and chlorides. The corrosion process was followed by monitoring of open-circuit potential (OCP), polarisation resistance (Rp) and electrochemical impedance spectroscopy (EIS). Electrochemical measurements show that the addition of MK and SF enhances corrosion resistance exposed to chlorides, however under accelerated carbonation these concretes show higher corrosion rates. In the simultaneous exposition to carbon dioxide and chlorides, SF-concrete shows a decrease of corrosion rate.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Concrete Corrosion and Durability · Concrete and Cement Materials Research · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (58)

Show source-provided references
1. Durability of steel reinforced concrete in chloride environments: an overview10.1016/j.conbuildmat.2011.12.038 ↗
2. Sustainability of cement, concrete and cement replacement materials in construction
3. Bertolini · 2004
4. Durability of reinforced concrete exposed to aggressive conditions10.3989/mc.2013.00313 ↗
5. Influence of cement type and temperature on the rate of corrosion of steel in concrete exposed to carbonation10.5006/1.3278306 ↗
6. Evaluation of concrete durability due to carbonation in harbor concrete structures10.1016/j.conbuildmat.2013.07.057 ↗
7. Carbonation of concrete bridge structures in three South African localities10.1016/j.cemconcomp.2007.06.005 ↗
8. El-Reedy · 2008
9. Carmona · 2005
10. Influence of steel–concrete interface condition on galvanic corrosion currents in carbonated concrete10.1016/j.corsci.2010.04.037 ↗
11. Supplementary cementitious materials10.1016/j.cemconres.2010.12.001 ↗
12. Pozzolanic cements10.1016/0958-9465(93)90023-3 ↗
13. 8 – Influence of supplementary cementitious materials (SCMs) on concrete durability
14. Recent advances in understanding the role of supplementary cementitious materials in concrete10.1016/j.cemconres.2015.03.018 ↗
15. Chloride-induced corrosion behaviour of reinforcing steel in spent fluid cracking catalyst modified mortars10.1016/j.cemconres.2013.01.011 ↗
16. Blended cement containing fluid catalytic cracking catalyst residue (FCC): hydration and paste microstructure10.4067/S0718-50732013000200003 ↗
17. Resistance of blended concrete containing an industrial petrochemical residue to chloride ion penetration and carbonation10.15446/ing.investig.v34n1.38730 ↗
18. Effect of metakaolin on the corrosion resistance of structural lightweight concrete10.1016/j.conbuildmat.2015.02.049 ↗
19. Compressive strength, chloride diffusivity and pore structure of high performance metakaolin and silica fume concrete10.1016/j.conbuildmat.2005.07.001 ↗
20. Influence of metakaolin as supplementary cementing material on strength and durability of concretes10.1016/j.conbuildmat.2011.12.050 ↗
21. Corrosion behaviour of reinforcing steel embedded in chloride contaminated concretes with and without metakaolin10.1016/j.compositesb.2012.09.085 ↗
22. Concreto adicionado con metacaolín: Comportamiento a carbonatación y cloruros
23. Strength properties and durability aspects of high strength concrete using Korean metakaolin10.1016/j.conbuildmat.2006.05.007 ↗
24. Utilization of silica fume in concrete: review of hardened properties10.1016/j.resconrec.2011.06.012 ↗
25. Utilization of silica fume in concrete: review of durability properties10.1016/j.resconrec.2011.09.016 ↗
26. Effect of fly ash and repeated loading on diffusion coefficient in chloride migration test10.1016/j.conbuildmat.2010.11.016 ↗
27. Long-term chloride diffusion in silica fume concrete in harsh marine climates10.1016/j.cemconcomp.2009.08.005 ↗
28. Effects of silica fume and steel fiber on chloride ion penetration and corrosion behaviour of cement-based composites10.1007/s11595-013-0679-4 ↗
29. Carbonation-induced reinforcement corrosion in silica fume concrete10.1016/j.conbuildmat.2008.08.005 ↗
30. Comparing a natural pozzolan, zeolite, to metakaolin and silica fume in terms of their effect on the durability characteristics of concrete: a laboratory study10.1016/j.conbuildmat.2012.11.054 ↗
31. Influence of metakaolin on the properties of mortar and concrete: a review10.1016/j.clay.2008.11.007 ↗
32. Corrosion monitoring of reinforced concrete structures – a review10.1016/S1452-3981(23)17049-0 ↗
33. Analysis of the electrochemical phenomenon at the rebar–concrete interface using the electrochemical impedance spectroscopic technique10.1680/macr.2010.62.3.177 ↗
34. Corrosion evolution of reinforcing steel in concrete under dry/wet cyclic conditions contaminated with chloride10.1016/S1005-0302(12)60149-2 ↗
35. Tutti · 1982 · 4
36. Chloride-induced corrosion on reinforcing steel: from the fundamentals to the monitoring techniques10.1016/S0958-9465(02)00089-6 ↗
37. Quantitative measurements of corrosion measurements10.1002/maco.19780290804 ↗
38. Corrosion rate monitoring in the laboratory and on-site10.1016/0950-0618(95)00044-5 ↗
39. Técnicas electroquímicas de corriente directa para la medición de la velocidad de corrosión. Resistencia a la polarización
40. Assignment of features in impedance spectra of the cement-paste/steel system10.1016/S0008-8846(98)00156-2 ↗
41. An a.c. impedance study of steel in concrete10.1007/BF00620572 ↗
42. Corrosion rate of ordinary and high-performance concrete subjected to chloride attack by AC impedance spectroscopy10.1016/j.conbuildmat.2005.01.062 ↗
43. Correlation of microstructure, electrical properties and electrochemical phenomena in reinforced mortar. Breakdown to multi-phase interface structures. Part II: pore network, electrical properties and electrochemical response10.1016/j.matchar.2007.06.016 ↗
44. Performance-based approach to durability of concrete containing flash-calcined metakaolin as cement replacement10.1016/j.conbuildmat.2014.01.063 ↗
45. The effect of metakaolin on the corrosion behaviour of cement mortars10.1016/j.cemconcomp.2004.02.041 ↗
46. Synergic effect of Friedel’s salt from pozzolan and from OPC co-precipitating in a chloride solution10.1016/j.conbuildmat.2011.12.040 ↗
47. Corrosion behaviour of rebars in fly ash mortar exposed to carbon dioxide and chlorides10.1016/S0958-9465(01)00025-7 ↗
48. Stability of Friedel’s salt in carbonated concrete structural elements10.1016/S0008-8846(96)85010-1 ↗
49. Accelerated carbonation effect on behaviour of ternary Portland cements10.1016/j.compositesb.2012.12.008 ↗
50. Chloride binding in sound and carbonated cementitious materials with various types of binder10.1016/j.conbuildmat.2014.05.049 ↗
51. Effect of coupled deterioration by freeze–thaw, carbonation and chlorides on concrete service life10.1016/j.cemconcomp.2013.10.008 ↗
52. Steel corrosion assessment by electrochemical impedance on metakaolin blended mortars10.1590/S1516-14392013005000178 ↗
53. Effect of fly ash on concrete reinforcement corrosion studied by EIS10.1016/S0958-9465(00)00003-2 ↗
54. Corrosion measurements of steel reinforcement in concrete exposed to a tropical marine atmosphere10.1016/S0008-8846(01)00713-X ↗
55. Equivalent circuit for modelling the steel-concrete interface. I. Experimental evidence and theoretical predictions10.1016/S0010-938X(98)00036-5 ↗
56. Electrochemical impedance behaviour and transport properties of silica fume contained concrete10.1016/j.conbuildmat.2013.05.010 ↗
57. Relation between resistivity and corrosion rate of reinforcements in carbonated mortar made with several cement types10.1016/0008-8846(88)90091-9 ↗
58. Effect of kaolin treatment temperature on mortar chloride permeability10.3989/mc.2007.v57.i285.39 ↗