Influence of different W/C on the performances and hydration progress of dual liquid high water backfilling material
Source abstract
Abstract
Abstract Sulfoaluminate cement-based high-water materials are widely used in coal and metal mining. There are few reports on the water cement ratio (W/C) affecting the properties and progress of hydration on dual liquid cement-based materials. Here, the effects of different W/C on dual liquid cement-based material on setting time, viscosity, compressive strength, water loss rate, diffusion radius, hydration heat, Fourier transform infrared spectroscopy (FT-IR), X-ray diffraction and SEM tests were studied. The results showed that as the W/C increased, the setting time increased, and the viscosity of single slurry decreased. Furthermore, as the slurry X and Y were mixed, the viscosity had an inflection point, and the compressive strength decreased while the later strength slowly increased; the relative water loss rate within 60 min reached 2.3–2.6, and was essentially stable after 40 h when the water cement ratio increased from 5:1, 6:1, 7:1, 8:1 to 9:1. When W/C = 8:1, it can be considered a turning point; the formula of diffusion radius obtained by experiments showed that the accumulative heat release and heat flow rate obviously decreased when the W/C was greater than 8:1. Also, the analysis results of XRD and SEM indicated that ettringite was the main hydration product, and as the W/C decreased, its density and shape also changed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Tailings Management and Properties · Grouting, Rheology, and Soil Mechanics · Concrete and Cement Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. Similar material simulation of time series system for induced caving of roof in continuous mining under backfill10.1007/s11771-008-0067-y ↗
2. A review of underground mine backfilling methods with emphasis on cemented paste backfill
3. Influence of lithium carbonate on hydration characteristics and strength development of sulphoaluminate cement
4. Hutchinson · 1996
5. An experimental procedure for the in situtesting of cable bolts10.1016/0148-9062(92)92635-P ↗
6. Physical and mechanical properties of normal Portland cement pertaining to fully grouted cable bolts
7. Development and challenges on mining backfill technology
8. Potvin · 2005
9. An investigation of rheological properties of cement-based grout mixed with rice husk ash (RHA)10.1016/j.conbuildmat.2015.05.025 ↗
10. Laboratory characterization of cemented rock fill for underhand cut and fill method of mining
11. A review of early-age properties of cement-based materials10.1016/j.cemconres.2007.09.005 ↗
12. In-line rheological measurements of cement grouts: effects of water/cement ratio and hydration10.1016/j.tust.2014.09.003 ↗
13. Effect of different superplasticisers on the physical and mechanical properties of cement grouts10.1016/j.conbuildmat.2013.09.050 ↗
14. Freeze-thaw durability of cement-based geothermal grouting materials10.1016/j.conbuildmat.2014.01.051 ↗
15. Influence of cement grouts composition on the rheological behaviour10.1016/j.cemconres.2010.11.015 ↗
16. Investigations on the cementitious grouts containing supplementary cementitious materials10.1016/S0008-8846(02)00799-8 ↗
17. F.W. Brackebusch, 1994. Basics of paste backfill systems. Mining Engineering. M. Fal, M. Benzaazoua, S. Ouellet 46 (10) (2005)1175–1178.
18. Design and application of underground mine paste backfill technology10.1007/s10706-007-9154-3 ↗
19. A hydration study of various calcium sulfoaluminate cements10.1016/j.cemconcomp.2014.07.002 ↗
20. Hydration of calcium sulfoaluminate cements-experimental findings and thermodynamic modelling10.1016/j.cemconres.2009.08.014 ↗
21. Chemistry of cement pore fluids(I): suspension reactions of Ca3-xNa2-xAl2O6 solid solutions with and without gypsum addition10.1016/0008-8846(83)90036-4 ↗
22. ASTM, Standard test methods for time of setting of hydraulic cement by Vicatneedle (2008).
23. ASTM, Standard specification for flow table for use in tests of hydrauliccement (2008).
24. Effects of lithium carbonate on performances of sulphoaluminate cement-based dual liquid high water material and its mechanisms10.1016/j.conbuildmat.2017.11.130 ↗
25. Rheological performance and compressive strength of superplasticized cementitious mixtures withmicro/nano-SiO2 additions10.1016/j.conbuildmat.2012.12.025 ↗
26. Hydration studies of calcium CSA cements blended with fly ash10.1016/j.cemconres.2013.07.010 ↗
27. Hydration of calcium sulfoaluminate cements -experimental findings and thermodynamic modelling10.1016/j.cemconres.2009.08.014 ↗
28. Visualization of failure in a pull-out test of cable bolts using X-ray CT10.1016/S0950-0618(00)00075-1 ↗
29. Structure of calcium aluminate sulfate Ca4Al6O16S10.1016/0022-4596(95)80002-7 ↗
30. Analysis of the system 3CaO.Al2O3-CaSO4.2H2O-CaCO3-H2O by FT-IR spectroscopy10.1016/S0008-8846(01)00502-6 ↗
31. C4A3Š hydration in different alkaline media10.1016/j.cemconres.2013.01.008 ↗