Durability of carbonated MgO concrete containing fly ash and ground granulated blast-furnace slag
Source abstract
Abstract
This study investigated the durability of carbonated reactive MgO cement (RMC) concrete containing fly ash (FA) and ground granulated blast-furnace slag (GGBS) under conditions involving exposure to sodium chloride, sodium sulfate, freeze-thaw cycling and seawater for up to 6 months. RMC samples were compared in terms of their performance to Portland cement (PC) samples. Changes in sample structure were analyzed by XRD, TGA and SEM. Amongst all the conditions used, sulfate attack led to the most obvious reduction (10.7–17.8%), whereas seawater had the lowest influence (5.8–6.9%) on strength at 6 months. RMC samples revealed a better performance over PC samples in sulfate attack and freeze-thaw cycling, which was associated with the stability of their phases under aggressive environments. Addition of FA and GGBS improved the durability of RMC concrete by enabling denser microstructures and formation of phases that were stable under the tested conditions.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete and Cement Materials Research · Magnesium Oxide Properties and Applications · Innovative concrete reinforcement materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (80)
Show source-provided references
1. Comparative life cycle assessment of reactive MgO and Portland cement production10.1016/j.jclepro.2016.07.071 ↗
2. Liska · 2010
3. Scaled-up commercial production of reactive magnesia cement pressed masonry units Part II: performance10.1680/coma.10.00031 ↗
4. Improving the performance of reactive MgO cement-based concrete mixes10.1016/j.conbuildmat.2016.09.090 ↗
5. Sequestration of CO2 in reactive MgO cement-based mixes with enhanced hydration mechanisms10.1016/j.conbuildmat.2017.03.038 ↗
6. Influence of supplementary cementitious materials on the performance and environmental impacts of reactive magnesia cement concrete10.1016/j.jclepro.2017.05.044 ↗
7. Mixtures of pulverised fuel ash, Portland cement and magnesium oxide: characterisation of pastes and setting behaviour
8. L. Vandeperre, M. Liska, A. Al-Tabbaa, Mixtures of pulverized fuel ash, Portland cement and magnesium oxide: strength evolution and hydration products, in: 6th International Conference on the Science and Engineering of Recycling for Environmental Protection, Yugoslav Engineering Academy, Belgrade, 2006, pp. 539–550.
9. Hydration and mechanical properties of magnesia, pulverized fuel ash, and portland cement blends10.1061/(ASCE)0899-1561(2008)20:5(375) ↗
10. Accelerated carbonation - A potential approach to sequester CO2 in cement paste containing slag and reactive MgO10.1016/j.cemconcomp.2013.07.001 ↗
11. Performance of magnesia cements in porous blocks in acid and magnesium environments10.1680/adcr.11.00011 ↗
12. Resistance of MgO–GGBS and CS–GGBS stabilised marine soft clays to sodium sulfate attack10.1680/geot.14.T.012 ↗
13. Durability of reactive magnesia-activated slag-stabilized low plasticity clay subjected to drying–wetting cycle10.1080/19648189.2015.1030088 ↗
14. Li · 2013
15. Pore structure and chloride permeability of concrete containing nano-particles for pavement10.1016/j.conbuildmat.2010.07.032 ↗
16. Compressive strength, chloride diffusivity and pore structure of high performance metakaolin and silica fume concrete10.1016/j.conbuildmat.2005.07.001 ↗
17. Durability of concrete exposed to leaching and external sulphate attacks10.1016/j.cemconres.2009.07.021 ↗
18. Attack on plain and blended cements exposed to aggressive sulfate environments10.1016/S0958-9465(01)00082-8 ↗
19. Effect of chloride salt, freeze–thaw cycling and externally applied load on the performance of the concrete10.1016/S0008-8846(02)00769-X ↗
20. The effect of silica fume and high-volume Class C fly ash on mechanical properties, chloride penetration and freeze–thaw resistance of self-compacting concrete10.1016/j.conbuildmat.2007.01.002 ↗
21. Effects of mineral and chemical admixtures on high-strength concrete in seawater10.1016/S0008-8846(01)00687-1 ↗
22. Durability of steel reinforced concrete in chloride environments: an overview10.1016/j.conbuildmat.2011.12.038 ↗
23. Factors influencing chloride transport in concrete structures exposed to marine environments10.1016/j.cemconcomp.2007.09.005 ↗
24. Stanish · 2000
25. Water permeability and chloride penetrability of high-strength lightweight aggregate concrete10.1016/S0008-8846(01)00738-4 ↗
26. Sulfate attack on alkali-activated slag concrete10.1016/S0008-8846(01)00659-7 ↗
27. Mechanism of sulfate attack: a fresh look: Part 2. Proposed mechanisms10.1016/S0008-8846(02)00958-4 ↗
28. Marchand · 2003
29. The thaumasite form of sulfate attack in the UK10.1016/S0958-9465(03)00106-9 ↗
30. Evaluation of freeze-thaw damage on concrete material and prestressed concrete specimens10.1016/j.conbuildmat.2016.08.098 ↗
31. The influence of lightweight aggregate on the physico-mechanical properties of concrete exposed to freeze–thaw cycles10.1016/j.coldregions.2009.08.010 ↗
32. Freeze–thaw damage and chemical change of a portland cement concrete in the presence of diluted deicers10.1617/s11527-009-9557-0 ↗
33. Freeze–thaw durability of high strength concrete under deicer salt exposure10.1016/j.conbuildmat.2015.10.194 ↗
34. Mehta · 2002
35. Prediction of time dependent chloride transport in concrete structures exposed to a marine environment10.1016/j.cemconres.2009.09.023 ↗
36. Effect of magnesium and sulfate ions on durability of silica fume blended mixes exposed to the seawater tidal zone10.1016/j.cemconres.2004.09.028 ↗
37. Performance of ground blast furnace slag and ground basaltic pumice concrete against seawater attack10.1016/j.conbuildmat.2007.03.024 ↗
38. Modelling chloride diffusion in concrete: effect of fly ash and slag10.1016/S0008-8846(98)00192-6 ↗
39. Utilization and efficiency of ground granulated blast furnace slag on concrete properties–a review10.1016/j.conbuildmat.2015.12.153 ↗
40. Mechanical activation of granulated blast furnace slag and its effect on the properties and structure of portland slag cement10.1016/j.cemconcomp.2008.05.005 ↗
41. A review on fly ash characteristics–Towards promoting high volume utilization in developing sustainable concrete10.1016/j.jclepro.2017.01.114 ↗
42. The greening of the concrete industry10.1016/j.cemconcomp.2008.12.010 ↗
43. Mechanical and durability properties of high performance concretes containing supplementary cementitious materials10.1016/j.conbuildmat.2009.08.045 ↗
44. Effect of fly ash on the durability properties of high strength concrete10.1016/j.proeng.2011.07.144 ↗
45. Effect of silica fume, metakaolin, and low-calcium fly ash on chemical resistance of concrete10.1016/S0008-8846(01)00548-8 ↗
46. Porosity, gas permeability, carbonation and their interaction in high-volume fly ash concrete10.1680/macr.2008.60.7.535 ↗
47. Long-term mechanical properties and durability characteristics of high-strength/high-performance concrete incorporating supplementary cementing materials under outdoor exposure conditions
48. Strength development and temperature rise in large concrete blocks containing high volumes of low-calcium (ASTM Class F) fly ash
49. Development of low-carbon cementitious materials via carbonating Portland cement–fly ash–magnesia blends under various curing scenarios: a comparative study10.1016/j.jclepro.2016.01.066 ↗
50. Effects of carbonation treatment on the properties of hydrated fly ash-MgO-Portland cement blends10.1016/j.conbuildmat.2015.07.193 ↗
51. Effectiveness of using CO2 pressure to enhance the carbonation of Portland cement-fly ash-MgO mortars10.1016/j.cemconcomp.2016.03.013 ↗
52. Coarse blast furnace slag as a cementitious material, comparative study as a partial replacement of Portland cement and as an alkali activated cement10.1016/j.conbuildmat.2009.02.002 ↗
53. Freeze–thaw cycle test and damage mechanics models of alkali-activated slag concrete10.1016/j.conbuildmat.2010.12.006 ↗
54. Influence of slag chemistry on the hydration of alkali-activated blast-furnace slag—Part I: effect of MgO10.1016/j.cemconres.2011.05.002 ↗
55. Properties of binary and ternary reactive MgO mortar blends subjected to CO2 curing10.1016/j.cemconcomp.2013.03.009 ↗
56. Fiber-reinforced reactive magnesia-based tensile strain-hardening composites10.1016/j.cemconcomp.2018.03.002 ↗
57. Accelerated carbonation–A potential approach to sequester CO2 in cement paste containing slag and reactive MgO10.1016/j.cemconcomp.2013.07.001 ↗
58. Accelerated carbonation of reactive MgO cements10.1680/adcr.2007.19.2.67 ↗
59. Carbonated MgO concrete with improved performance: the influence of temperature and hydration agent on hydration, carbonation and strength gain10.1016/j.cemconcomp.2017.06.006 ↗
60. ASTM -98: Standard Test Method for Normal Consistency of Hydraulic Cement, Annual Book of ASTM Standards, Philadelphia, USA, 1998.
61. Enhancing the carbonation of MgO cement porous blocks through improved curing conditions10.1016/j.cemconres.2014.02.005 ↗
62. Investigation of carbonation depth and its influence on the performance and microstructure of MgO cement and PC mixes10.1016/j.conbuildmat.2016.05.067 ↗
63. Influence of mix design on the carbonation, mechanical properties and microstructure of reactive MgO cement-based concrete10.1016/j.cemconcomp.2017.03.004 ↗
64. Study on the expansion of concrete under attack of sulfate and sulfate–chloride ions10.1016/j.conbuildmat.2012.05.003 ↗
65. Durable fiber reinforced self-compacting concrete10.1016/j.cemconres.2003.07.005 ↗
66. Strength deterioration of high strength concrete in sulfate environment10.1016/S0008-8846(99)00106-4 ↗
67. Durability of concrete made with granite and marble as recycle aggregates10.1016/j.jmatprotec.2007.12.120 ↗
68. The test method of long-term and durability on ordinary concrete. National Standard of the People's Republic of China, 1997.
69. ASTM, Standard test method for compressive strength of cylindrical concrete specimens, C39-16, 2016.
70. ASTM C642-06: Standard test method for density, absorption and voids in hardened concrete, ASTM International, Philadelphia, USA, 2006.
71. ASTM C25-17: Standard Test Methods for Chemical Analysis of Limestone, Quicklime, and Hydrated Lime, ASTM International, West Conshohocken, PA, USA, 2017.
72. AgNO3-based colorimetric methods for measurement of chloride penetration in concrete10.1016/j.conbuildmat.2011.06.003 ↗
73. AgNO3 spray tests: advantages, weaknesses, and various applications to quantify chloride ingress into concrete. Part 1: Non-steady-state diffusion tests and exposure to natural conditions10.1617/s11527-007-9233-1 ↗
74. Influence of fly ash fineness on the chloride penetration of concrete10.1016/j.conbuildmat.2005.08.010 ↗
75. Effect of supplementary cementing materials on concrete resistance against carbonation and chloride ingress10.1016/S0008-8846(99)00249-5 ↗
76. T. Sato, N. Akita, A. Hamadate, K. Fukushi, Formation and stability of magnesium hydrocarbonate minerals during serpentinization and weathering of serpentinites, in: Eleventh Annual VM Goldschmidt Conference, 2001.
77. In situ investigation of the thermal decomposition of Co–Al hydrotalcite in different atmospheres10.1039/b009320n ↗
78. Formation of magnesium silicate hydrate (MSH) cement pastes using sodium hexametaphosphate10.1016/j.cemconres.2014.07.001 ↗
79. Effect of temperature on the microstructure of calcium silicate hydrate CSH10.1016/j.cemconres.2013.06.008 ↗
80. Hydrotalcite decomposition mechanism: a clue to the structure and reactivity of spinel-like mixed oxides10.1021/jp960040i ↗