Study on the addition effect of metakaolin and mechanically activated kaolin on cement strength and microstructure under different curing conditions
Source abstract
Abstract
The effects of thermally (MK) or mechanically activated kaolin (AK) on the compressive strength of mortars and microstructure of pastes were investigated. Mortar mixtures, in which 10%, 20% and 30% of ordinary Portland cement (OPC) was replaced by either MK or AK, were prepared (w/b of 0.5) and ordinary (age 2, 28 or 90 days) and autoclave cured. Hydration products were determined by X-ray diffraction (XRD) and differential thermal analysis/thermal gravimetry (DTA/TG) analysis, while microstructure was investigated by mercury intrusion porosimetry (MIP). MK substitution increases the compressive strength of ordinary-cured mortars, as a result of the higher content of reactive silica that caused more pronounced pozzolanic reaction, as well as by effective refinement of their pore structure. Positive effects on the compressive strength could be achieved up to 30% substitution of OPC by MK. The OPC substitution by AK resulted in lower strengths of ordinary-cured mortars, compared to both MK mortars and reference. Higher specific surface area and finer particles of AK were insufficient to compensate, through filler effect, lower pozzolanic reaction and additional negative influence of the kaolinite presence. The highest compressive strength was obtained for mortar with 10% of AK (relative strength of 94%). In comparison to the reference, autoclaved MK and AK mortars, exhibited lower compressive strength, as a consequence of increasing the hydrogarnet formation, instead of tobermorite. The highest strength was achieved for mortar with 10% of AK.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete and Cement Materials Research · Building materials and conservation · Innovative concrete reinforcement materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (69)
Show source-provided references
1. Siddique · 2011
2. Sustainable development and climate change initiatives10.1016/j.cemconres.2007.09.008 ↗
3. Sustainable cement production – present and future10.1016/j.cemconres.2011.03.019 ↗
4. 2015
5. Metakaolin and calcined clays as pozzolans for concrete: a review10.1016/S0958-9465(00)00092-5 ↗
6. Metakaolin as cementitious material: history, scours, production and composition – a comprehensive overview10.1016/j.conbuildmat.2012.12.001 ↗
7. Metakaolin: fresh properties and optimum content for mechanical strength in traditional cementitious materials – a comprehensive overview
8. Thermal treatment of kaolin: the effect of mineralogy on the pozzolanic activity10.1016/S0169-1317(01)00040-0 ↗
9. The effect of dehydroxylation/amorphization degree on pozzolanic activity of kaolinite10.1016/S0008-8846(02)00975-4 ↗
10. Metakaolin as supplementary cementitious material: optimization of kaolin to metakaolin conversion10.1007/s10973-005-0806-3 ↗
11. Thermal treatment of kaolin clay to obtain metakaolin10.2298/HEMIND100322014I ↗
12. Pozzolanic reactivity of low grade kaolinitic clays: influence of calcination temperature and impact of calcination products on OPC hydration10.1016/j.clay.2015.01.028 ↗
13. Metakaolin as a main cement constituent. Exploitation of poor Greek kaolins10.1016/j.cemconcomp.2004.02.007 ↗
14. Exploitation of poor Greek kaolins: durability of metakaolin concrete10.1016/j.cemconcomp.2008.11.001 ↗
15. Influence of calcined kaolin on mortar properties10.1016/j.conbuildmat.2010.11.017 ↗
16. Cement substitution by a combination of metakaolin and limestone10.1016/j.cemconres.2012.09.006 ↗
17. Mechanochemical treatment of kaolinite10.1006/jcis.2001.7591 ↗
18. Some physico-chemical alterations caused by mechanochemical treatments in kaolinites of different structural order10.1016/j.tca.2004.11.012 ↗
19. Influence of metakaolin on the properties of mortar and concrete: a review10.1016/j.clay.2008.11.007 ↗
20. Preparation of pozzolanic addition by mechanical treatment of kaolin clay10.1016/j.minpro.2014.09.004 ↗
21. Structural and thermal behavior of proclay kaolinite using high energy ball milling process10.1016/j.powtec.2014.11.018 ↗
22. Pozzolan obtained by mechanochemical and thermal treatments of kaolin10.1016/j.clay.2009.09.008 ↗
23. Pozzolanic activity of mechanochemically and thermally activated kaolins in cement10.1016/j.cemconres.2015.04.017 ↗
24. Pozzolanic activity of thermally and mechanically treated kaolins of hydrothermal origin10.1016/j.clay.2015.08.028 ↗
25. Effects of mechanical and thermal activation on pozzolanic activity of kaolin containing mica10.1016/j.clay.2016.01.029 ↗
26. Study of the reactivity of cement/metakaolin binders at early age for specific use in steam cured precast concrete10.1016/j.conbuildmat.2008.02.022 ↗
27. Metakaolin, a solution for the precast industry to limit the clinker content in concrete: mechanical aspects10.1016/j.conbuildmat.2009.12.032 ↗
28. Use of the second-derivative differential thermal curve in the evaluation of cement-quartz pastes with metakaolin addition autoclaved at 180°C10.1016/S0040-6031(97)00409-7 ↗
29. DTA–TGA of unstirred autoclaved metakaolin–lime–quartz slurries. The formation of hydrogarnet10.1016/S0040-6031(98)00307-4 ↗
30. Autoclaved cement-quartz pastes with metakaolin additions10.1016/S1065-7355(97)00073-4 ↗
31. Research of possibilities for use domestic kaolin clays for production of metakaolin10.2298/HEMIND0902107M ↗
32. Ilić · 2010
33. Properties of composite cement with commercial and manufactured metakaolin
34. Mechanochemical treatment of Serbian kaolin clay to obtain high reactive pozzolana10.2298/JSC120829107M ↗
35. Neville · 2011
36. Amorphous kaolin as cement replacement material
37. Strengths of the mortars containing amorphous kaolin as cement replacement material
38. Recent advances in understanding the role of supplementary cementitious materials in concrete10.1016/j.cemconres.2015.03.018 ↗
39. The filler effect: the influence of filler content and surface area on10.1111/jace.12264 ↗
40. Supplementary cementitious materials10.1016/j.cemconres.2010.12.001 ↗
41. Mineral admixtures in mortars: quantification of the physical effects of inert materials on short-term hydration
42. Kaolinitic calcined clays – Portland cement system: hydration and properties10.1016/j.conbuildmat.2014.04.065 ↗
43. Performance evaluation of cement mortars modified with metakaolin or ground brick10.1016/j.conbuildmat.2008.08.027 ↗
44. Metakaolin as an extender in South African cement10.1061/(ASCE)0899-1561(2006)18:4(619) ↗
45. Kaolinite obtained by ball milling as a potential substituent for cement: mechanical performance effect on mortar based cement and milled kaolinite
46. Properties of metakaolin blended cements10.1016/1065-7355(94)90007-8 ↗
47. Hydration reaction and hardening of calcined clays and related minerals. I. Preliminary investigation on metakaolinite10.1016/0008-8846(83)90109-6 ↗
48. Effect of cement type on metakaolin efficiency10.1016/j.cemconres.2014.06.007 ↗
49. Thermal analysis to assess pozzolanic activity of calcined kaolinitic clays10.1007/s10973-014-3816-1 ↗
50. Mindess · 2002
51. Formulation of blended cement: effect of process variables on clay pozzolanic activity10.1016/j.conbuildmat.2008.07.015 ↗
52. The effect of high curing temperature on the reaction kinetics in MK/lime and MK-blended cement matrices at 60°C10.1016/S0008-8846(02)01040-2 ↗
53. Potential use of argentine kaolinitic clays as pozzolanic material10.1016/j.clay.2014.09.009 ↗
54. Class H cement hydration at 180°C and high pressure in the presence of added silica10.1016/j.cemconres.2007.12.004 ↗
55. Cementitious properties of ladle slag fines under autoclave curing conditions10.1016/S0008-8846(03)00211-4 ↗
56. Taylor · 1990
57. Durability studies on concrete containing wollastonite10.1016/j.jclepro.2014.10.038 ↗
58. Effects of quartz particle size on hydrogarnet formation during autoclaving at 180°C in the CaO-Al2O3-SiO2-H2O system10.1016/S0008-8846(98)00112-4 ↗
59. Differential scanning calorimetry study of ordinary Portland cement10.1016/S0008-8846(99)00128-3 ↗
60. Early hydration of clinker-slag-metakaolin combination in steam curing conditions, relation with mechanical properties10.1016/j.cemconres.2009.07.023 ↗
61. Influence of MK on the reaction kinetics in MK/lime and MK-blended cement systems at 20°C10.1016/S0008-8846(00)00465-8 ↗
62. Evaluation of pozzolanic activity and physicomechanical characteristics in metakaolin-lime pastes10.1007/s10973-005-7262-y ↗
63. Hydratation reaction and hardening of calcined clays and related minerals. Influence of mineralogical properties of the raw-kaolinite on the reactivity of metakaolinite10.1016/0008-8846(83)90010-8 ↗
64. Hydration products of lime–metakaolin pastes at ambient temperature with ageing10.1016/j.tca.2012.02.013 ↗
65. Differential scanning calorimetry study of ordinary Portland cement paste containing metakaolin and theoretical approach of metakaolin activity10.1016/S0958-9465(00)00090-1 ↗
66. Effect of autoclave curing on the microstructure of blended cement mixture incorporating ground dune sand and ground granulated blast furnace slag10.1007/s40069-015-0104-9 ↗
67. Pore size distribution of high performance metakaolin concrete10.1007/BF02852633 ↗
68. Pore size distribution of metakaolin paste10.1016/0008-8846(96)00147-0 ↗
69. Influence of metakaolin surface area on properties of cement-based materials10.1061/(ASCE)0899-1561(2007)19:9(762) ↗