Utilisation of coarse glass powder as pozzolanic cement—A mix design investigation

Z. Kalakada, J.H. Doh, G. Zi

Abstract

Abstract Cement production is a highly energy-intensive and environmentally polluting process, however, despite the detrimental effects, the production rates are increasing annually to meet the ever-rising demand. Hence, it is imperative to look out for materials that can be used in place of cement for promoting green construction and sustainability. On the other hand, glass, post-consumption, is dumped in landfills instead of recycling due to factors such as high recycling cost, cheap imports and lack of awareness to name a few. Since glass is a non-biodegradable material, the practice of dumping waste glass in the landfills is environmentally unsustainable. Recently it has been revealed that glass at particular fineness exhibits pozzolanic characteristics. The focus of this study is to investigate the pozzolanic attribute of a coarse glass powder (≤150 µm) used as a cement replacement; the substitution levels employed were 15% and 30% by weight of cement. In addition to the basic compressive strength testing, durability tests such as drying shrinkage, resistance to chloride ion penetration and heat of hydration were evaluated. The test results indicate that 30% is the ideal replacement level, providing a strength activity index (SAI) of 117%, a 32% higher resistance to chloride ion permeability and a 24% reduction in heat from hydration.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Concrete and Cement Materials Research · Recycled Aggregate Concrete Performance · Recycling and utilization of industrial and municipal waste in materials production

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (62)

Show source-provided references
1. US Geological Survey. Mineral commodity summaries 2019. US Geological Survey, Reston, VA. http://prd-wret.s3-us-west-2.amazonaws.com/assets/palladium/production/atoms/files/mcs2019_all.pdf, 2019.
2. Life cycle assessment of the production of Portland cement: a Southern Europe case study10.1016/j.jclepro.2016.02.110 ↗
3. CO2 emission trading within the European Union and Annex B countries: the cement industry case10.1016/j.enpol.2004.06.003 ↗
4. N. Oreskes, E.M. Conway. Merchants of doubt: How a handful of scientists obscured the truth on issues from tobacco smoke to global warming. Bloomsbury, New York, 2011.
5. Compressive strength and electron paramagnetic resonance studies on waste glass admixtured cement10.4236/njgc.2011.13017 ↗
6. Modulus of rupture evaluation of cement stabilized recycled glass/recycled concrete aggregate blends10.1016/j.conbuildmat.2015.03.048 ↗
7. Fatigue performance of rubber-modified recycled aggregate concrete (RRAC) for pavement10.1016/j.conbuildmat.2015.07.042 ↗
8. Performance of recycled aggregate concrete based on a new concrete recycling technology10.1016/j.conbuildmat.2015.07.021 ↗
9. Bond behavior between steel bar and recycled aggregate concrete after freeze–thaw cycles10.1016/j.coldregions.2015.06.008 ↗
10. Carbonation behaviour of recycled aggregate concrete10.1016/j.cemconcomp.2015.04.017 ↗
11. A novel mix design methodology for recycled aggregate concrete10.1016/j.conbuildmat.2016.06.061 ↗
12. Studies on concrete containing ground waste glass10.1016/S0008-8846(99)00213-6 ↗
13. Value-added utilisation of waste glass in concrete
14. Effect of glass powder on chloride ion transport and alkali–aggregate reaction expansion of lightweight aggregate concrete10.1007/s11595-009-2312-0 ↗
15. Chloride transport in fly ash and glass powder modified concretes—influence of test methods on microstructure10.1016/j.cemconcomp.2009.11.010 ↗
16. Green and durable mortar produced with milled waste glass10.1680/macr.11.00082 ↗
17. The potential pozzolanic activity of glass and red-clay ceramic waste as cement mortars components10.1016/j.conbuildmat.2011.12.110 ↗
18. Durability properties of a concrete with waste glass sludge exposed to freeze-and-thaw condition and de-icing salt10.1016/j.conbuildmat.2014.05.081 ↗
19. Waste glass sludge as a partial cement replacement in mortar10.1016/j.conbuildmat.2014.11.007 ↗
20. Pozzolanic reaction of the waste glass sludge incorporating precipitation additives10.12989/cac.2016.17.2.255 ↗
21. J. Pickin, P. Randell. Australian national waste report 2016. Department of the Environment and Energy. Blue Environment, Docklands, VIC, Australia. https://www.environment.gov.au/system/files/resources/d075c9bc-45b3-4ac0-a8f2-6494c7d1fa0d/files/national-waste-report-2016.pdf, 2017.
22. Effectiveness of novel and traditional methods to incorporate industrial wastes in cementitious materials—an overview10.1016/j.resconrec.2013.03.003 ↗
23. Waste glass as coarse aggregate for concrete10.1520/JTE10117J ↗
24. Properties of concrete containing waste glass10.1016/j.cemconres.2003.07.003 ↗
25. ASR expansion behavior of recycled glass fine aggregates in concrete10.1016/j.cemconres.2009.09.003 ↗
26. Using lithium nitrate and pozzolanic glass powder in concrete as ASR suppressors10.1016/j.cemconcomp.2007.08.010 ↗
27. Fracture mechanics of ASR in concretes with waste glass particles of different sizes
28. The effectiveness of supplementary cementing materials in suppressing expansion due to ASR: another look at the reaction mechanisms part 2: Pore solution chemistry10.1016/0008-8846(94)90047-7 ↗
29. The effect of metakaolin on alkali–silica reaction in concrete10.1016/S0008-8846(99)00261-6 ↗
30. Investigating the alkali-silica reaction of recycled glass aggregates in concrete materials10.1061/(ASCE)MT.1943-5533.0000126 ↗
31. Use of waste glass as sand in mortar: part I—fresh, mechanical and durability properties10.1016/j.cemconcomp.2012.08.028 ↗
32. Effect of particle size on alkali—silica reaction in recycled glass mortars10.1016/j.conbuildmat.2014.05.092 ↗
33. Effect of glass powders on the mechanical and durability properties of cementitious materials10.1016/j.conbuildmat.2015.06.010 ↗
34. Fresh properties of self-compacting concrete containing ground waste glass microparticles as cementing material10.3151/jact.13.50 ↗
35. Electrical conductivity based characterization of plain and coarse glass powder modified cement pastes10.1016/j.cemconcomp.2007.05.005 ↗
36. I. You, G. Zi, D. Yoo, David A. Lange. Durability of concrete containing LCD glass powder for pavement. ACI Materials Journal - In press, 2019.10.14359/51716814 ↗
37. Effect of new mixing method of glass powder as cement replacement on mechanical behavior of concrete10.1016/j.conbuildmat.2019.01.077 ↗
38. Properties of high volume glass powder concrete10.1016/j.cemconcomp.2016.10.010 ↗
39. Pozzolanic reaction of glass powder and its role in controlling alkali–silica reaction10.1016/j.cemconcomp.2015.12.008 ↗
40. An investigation into the hydration and microstructure of cement pastes modified with glass powders10.1016/j.conbuildmat.2016.02.085 ↗
41. Utilization of waste glass powder in the production of cement and concrete10.1016/j.conbuildmat.2016.08.016 ↗
42. Performance of glass-powder concrete in field applications10.1016/j.conbuildmat.2016.02.006 ↗
43. Effect of glass powder on sulfuric acid resistance of cementitious materials10.1016/j.conbuildmat.2016.03.049 ↗
44. Transport properties of concrete with glass powder as supplementary cementitious material
45. Effect of curing temperature and glass type on the pozzolanic reactivity of glass powder10.1016/j.cemconres.2014.01.015 ↗
46. Durability of mortar using waste glass powder as cement replacement10.1016/j.conbuildmat.2012.04.027 ↗
47. Performance of glass powder as a pozzolanic material in concrete: a field trial on concrete slabs10.1016/j.cemconres.2005.12.012 ↗
48. Characteristics and pozzolanic reactivity of glass powders10.1016/j.cemconres.2004.05.015 ↗
49. Effect of glass powder on the compression strength and the workability of concrete10.1080/23311916.2017.1373415 ↗
50. The effect of pulverized-fuel ash upon the workability of cement paste and concrete10.1680/macr.1980.32.113.219 ↗
51. Cement Industry Federation (CIF). Cement Industry Federation Industry Report 2017. CIF, Forrest, ACT, Australia, 2017.
52. Standards Australia. AS 3972. General purpose and blended cements. Standards Australia, Sydney, NSW, Australia, 2010.
53. Standards Australia. AS 1141.5–2000. Methods for sampling and testing aggregates Particle density and water absorption of fine aggregate. Standards Australia, Sydney, NSW, Australia, 2000.
54. Standards Australia. 1012.8. 1: Methods of testing concrete—Method for making and curing concrete—Compression and indirect tensile test specimens. Standards Australia, Sydney, NSW, Australia, 2014.
55. ASTM International. ASTM-C511. Standard specification for mixing rooms, moist cabinets, moist rooms, and water storage tanks used in the testing of hydraulic cements and concretes. ASTM International, West Conshohocken, PA, 2013.
56. Standards Australia. AS 1012.3. 1–1998. Methods of testing concrete—Determination of properties related to the consistency of concrete. Standards Australia, Sydney, NSW, Australia, 1998.
57. Standards Australia. AS 1012.9 Methods of testing concrete—Compressive strength tests—Concrete, mortar and grout specimens. Standards Australia, Sydney, NSW, Australia, 2014.
58. ASTM International. ASTM-C618. Standard specification for coal fly ash and raw or calcined natural pozzolan for use as a mineral Admixture in Portland Cement Concrete. ASTM International, West Conshohocken, PA, 2003.
59. American Association of State Highway and Transportation Officials (AASHTO). AASHTO designation: T 358-15: Standard method of test for surface resistivity indication of concrete’s ability to resist chloride ion penetration, AASHTO, Washington, DC, 2015.
60. H.R. Hamilton, A.J. Boyd, E.A. Vivas. Permeability of concrete—Comparison of conductive and diffusion methods. Final report submitted to Florida Department of Transportation (Contract No. BD536). http://ftp.fdot.gov/file/d/FTP/FDOT%20LTS/CO/research/Completed_Proj/Summary_SMO/FDOT_BD536_rpt.pdf, 2007.
61. Standards Australia. 1012.13. Methods of testing concrete: Method 13: Determination of the drying shrinkage of the concrete samples prepared in the field or in the laboratory. Standards Australia, Sydney, NSW, Australia, 1992.
62. Utilization of waste glass in ECO-cement: strength properties and microstructural observations10.1016/j.wasman.2006.07.014 ↗