Increasing mechanical strength and acid resistance of geopolymers by incorporating different siliceous materials
Source abstract
Abstract
Abstract This study, for the first time, reports using hollow glass microsphere waste (HGMW) and quartz powder (QP) to improve compressive strength and sulphuric acid resistance of fly ash/slag based geopolymers (AAFS), which is aimed for oil-gas well cementing and other uses where acid corrosion medium exists. Due to the lower reactivity of HGMW and QP compared to fly ash and slag, their incorporation needs a high temperature curing process (at 80 °C in this study) to obtain a certain extent of reaction. The resulting product with 5% HGMW and 5% QP exhibits higher compressive strength than the neat AAFS. After sulphuric exposure for 90 days, the high temperature cured samples show less susceptibility to the acid attack in comparison with those samples cured at room temperature and those without HGMW and QP. It is confirmed that better resistance of acid attack of the 80 °C cured mixture with addition of HGMW and QP than the neat AAFS mixture is due to the more crosslinked and compact microstructure. In addition, the volume stability of the geopolymer binders is also assessed and is found to be satisfying under both the ambient and high temperature conditions.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete and Cement Materials Research · Innovative concrete reinforcement materials · Building materials and conservation
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (48)
Show source-provided references
1. Do geopolymers actually contain nanocrystalline zeolites? A reexamination of existing results10.1021/cm050230i ↗
2. Designing precursors for geopolymer cements10.1111/j.1551-2916.2008.02787.x ↗
3. Costs and carbon emissions for geopolymer pastes in comparison to ordinary portland cement10.1016/j.jclepro.2011.02.010 ↗
4. The role of particle technology in developing sustainable construction materials10.1016/j.apt.2009.10.006 ↗
5. Resistance of geopolymer materials to acid attack10.1016/j.cemconres.2004.06.005 ↗
6. Influence of the slag content on the chloride and sulfuric acid resistances of alkali-activated fly ash/slag paste10.1016/j.cemconcomp.2016.06.004 ↗
7. Sulfuric acid resistance of blended ash geopolymer concrete10.1016/j.conbuildmat.2013.01.018 ↗
8. Sulfuric acid attack on hardened paste of geopolymer cements Part 1. Mechanism of corrosion at relatively high concentrations
9. Nitric acid attack on hardened paste of geopolymeric cements – Part 2
10. Nitric acid attack on hardened paste of geopolymeric cements – Part 1
11. The effect of silica availability on the mechanism of geopolymerisation10.1016/j.cemconres.2011.02.001 ↗
12. Acid resistance of inorganic polymer binders. 1. Corrosion rate10.1617/s11527-011-9744-7 ↗
13. Sorptivity and acid resistance of ambient-cured geopolymer mortars containing nano-silica10.1016/j.cemconcomp.2016.06.017 ↗
14. Strength and resistance to sulfate and sulfuric acid of ground fluidized bed combustion fly ash-silica fume alkali-activated composite10.1016/j.apt.2014.02.007 ↗
15. Durability of fly ash based geopolymer concrete in the presence of silica fume10.1016/j.jclepro.2017.02.176 ↗
16. A review on ultra high performance concrete: Part I. Raw materials and mixture design10.1016/j.conbuildmat.2015.10.088 ↗
17. Effect of polycarboxylate and crushed quartz in UHPC: Microstructural investigation10.1016/j.conbuildmat.2013.03.077 ↗
18. Hydration and hardening of class G oil well cement with and without silica sands under high temperature
19. A preliminary study of autoclaved alkali-activated slag blended with quartz powder10.1016/j.conbuildmat.2011.12.104 ↗
20. An investigation on alkali-activated fly ash pastes modified with quartz powder subjected to elevated temperatures10.1016/j.conbuildmat.2016.06.068 ↗
21. An investigation on alkali-activated Egyptian metakaolin pastes blended with quartz powder subjected to elevated temperatures10.1016/j.clay.2016.07.002 ↗
22. The research progress on preparation method and application of hollow glass microsphere
23. Characterization of hollow glass beads
24. Evolution of binder structure in sodium silicate-activated slag-metakaolin blends10.1016/j.cemconcomp.2010.09.004 ↗
25. Reaction kinetics, gel character and strength of ambient temperature cured alkali activated slag-fly ash blends10.1016/j.conbuildmat.2015.01.065 ↗
26. Mechanical property and structure of alkali-activated fly ash and slag blends
27. Alkali-activated fly ash/slag cement – strength behaviour and hydration products10.1016/S0008-8846(00)00298-2 ↗
28. The transition of fly ash-based geopolymer gels into ordered structures and the effect on the compressive strength10.1016/j.conbuildmat.2015.12.049 ↗
29. Compositional, microstructural and mechanical properties of ambient condition cured alkali-activated cement10.1016/j.conbuildmat.2016.03.043 ↗
30. Composition and microstructure of alkali activated fly ash binder: effect of the activator10.1016/j.cemconres.2005.03.003 ↗
31. Can nanosilica sol prevent oil well cement from strength retrogression under high temperature?10.1016/j.conbuildmat.2017.03.221 ↗
32. Class H cement hydration at 180°C and high pressure in the presence of added silica10.1016/j.cemconres.2007.12.004 ↗
33. Quantitative kinetic and structural analysis of geopolymers. Part 1. The activation of metakaolin with sodium hydroxide10.1016/j.tca.2012.03.021 ↗
34. Model quasi-molecule SiO2 as an approach in the IR-spectra description glassy and crystalline framework silicates10.1016/0022-2860(95)08658-I ↗
35. Fractionation and characterization of Texas lignite class-F fly ash by XRD, TGA, FTIR and SFM10.1016/0008-8846(94)90039-6 ↗
36. Modification of phase evolution in alkali-activated blast furnace slag by the incorporation of fly ash10.1016/j.cemconcomp.2013.09.006 ↗
37. Structural reorganisation of class F fly ash in alkaline silicate solutions10.1016/S0927-7757(02)00237-6 ↗
38. Mid-infrared spectroscopic studies of alkali-activated fly ash structure10.1016/j.micromeso.2005.05.057 ↗
39. Shrinkage characteristics of alkali-activated fly ash/slag paste and mortar at early ages10.1016/j.cemconcomp.2014.07.007 ↗
40. Drying and autogenous shrinkage of pastes and mortars with activated slag cement10.1016/j.cemconres.2007.11.002 ↗
41. Quantification of chloride diffusion in fly ash–slag-based geopolymers by X-ray fluorescence (XRF)10.1016/j.conbuildmat.2014.07.031 ↗
42. Compressive strength development and shrinkage of alkali-activated fly ash–slag blends associated with efflorescence10.1617/s11527-015-0694-3 ↗
43. The shrinkage of alkali activated fly ash10.1016/j.cemconres.2014.10.024 ↗
44. Shrinkage mechanisms of alkali-activated slag10.1016/j.cemconres.2016.07.001 ↗
45. Influence of fly ash on the pore structure and shrinkage characteristics of metakaolin-based geopolymer pastes and mortars10.1016/j.conbuildmat.2017.05.067 ↗
46. Engineering properties of alkali-activated fly ash concrete
47. On the development of fly ash-based geopolymer concrete
48. Effect of elevated temperature curing on properties of alkali-activated slag concrete10.1016/S0008-8846(99)00143-X ↗