Investigation on the potential utilization of zeolite as an internal curing agent for autogenous shrinkage mitigation and the effect of modification
Source abstract
Abstract
Abstract This paper presents an experimental investigation on the potential utilization of one natural zeolite as an internal curing agent for mitigation of self-desiccation and the subsequent autogenous shrinkage of cement paste with low w/b ratio (0.25). Incorporation of 20% zeolite by mass leads to higher internal relative humidity (90.4%) during the first 7 d compared to that of control sample (78.1%). It is indicating that the zeolite under investigated shows partially elimination effect on the self-desiccation and the autogenous shrinkage as well based on the time-zero defined by the onset of internal relative humidity drop. To obtain improved internal curing property, attempts have been done to modify the pore structure of zeolite by acid treatment and/or thermal treatment. However, both nitric acid treatment and thermal treatment shows negative effect on the improvement of internal curing property of zeolite. Because nitric acid treatment tends to increase the BET surface area of zeolite by increasing the volume of 2–7 nm pores, and the thermal treatment tends to reduce the porosity rather than to enlarge the pore size of zeolite.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete Properties and Behavior · Concrete and Cement Materials Research · Innovative concrete reinforcement materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. 2007
2. Protected paste volume in concrete: extension to internal curing using saturated lightweight fine aggregate10.1016/S0008-8846(99)00178-7 ↗
3. Prevention of autogenous shrinkage in high-strength concrete by internal curing using wet lightweight aggregates10.1016/S0008-8846(01)00608-1 ↗
4. Water-entrained cement-based materials - I. Principle and theoretical background10.1016/S0008-8846(01)00463-X ↗
5. Water-entrained cement-based materials- II. Implementation and experimental results10.1016/S0008-8846(02)00737-8 ↗
6. Techniques and materials for internal water curing of concrete10.1617/s11527-006-9136-6 ↗
7. A. Bentur, S. Igarashi, K. Kovler, Control of autogenous shrinkage stresses and cracking in high strength concretes, in: Proc. of 5th Int. Symp. of High Strength/High Performance Concrete Sandefjord, Norway, 1999, pp. 1017–1026.
8. P. Lura, K. van Breugel, Moisture exchange as a basic phenomenon to understand volume changes of lightweight aggregate concrete at early age, in: V. Baroghel-Bouny, P.C. Aitcin (Eds.), Proc. Int. Workshop on Shrinkage of Concrete Paris, 2000, pp. 533–546.
9. S. Zhutovsky, K. Kovler, A. Bentur, Influence of wet lightweight aggregate on autogenous shrinkage of concrete at early ages, in: F.-J. Ulm, Z.P. Bazant, F.H. Wittmann (Eds.), Proc. 6th Int. Conf. Creep, Shrinkage and Durability Mechanics of Concrete and Other Quasi-Brittlematerials Cambridge (MA), USA, 2001, pp. 697–702.
10. P. Lura, F. Durand, A. Loukili, K. Kovler, O.M. Jensen, Compressive strength of cement pastes and mortars with suberabsorbent polymers, in: O.M. Jensen, P. Lura, K. Kovler (Eds.), Proc. Int. RILEM Conf. on Volume Changes of Hardening Concrete: Testing and Mitigation, RILEM Publications S.A.R.L., Bagneux, 2006, pp. 117–126.10.1617/2351580052.013 ↗
11. M.T. Hasholt, M.H.S. Jespersen, O.M. Jensen, Mechanical properties of concrete with SAP. Part I: development of compressive strength, in: O.M. Jensen, M.T. Hasholt, S. Laustsen (Eds.), Proc. Int. RILEM Conf. on Use of Superabsorbent Polymers and Other New Additives in Concrete, RILEM Publications S.A.R.L., Lyngby, Denmark, 2010, pp. 117–126.
12. Effect of internal curing by using superabsorbent polymers (SAP) on autogenous shrinkage and other properties of a high-performance fine-grained concrete: results of a RILEM round-robin test, TC 225-SAP10.1617/s11527-013-0078-5 ↗
13. Internal curing by superabsorbent polymers in ultra-high performance concrete10.1016/j.cemconres.2015.05.005 ↗
14. Properties of alkali-activated clinoptilolite10.1016/S0008-8846(00)00331-8 ↗
15. Characterization and pozzolanic activity of thermally treated zeolite10.1007/s10973-005-0849-5 ↗
16. Some advances in understanding the pozzolanic activity of zeolites: the effect of zeolite structure10.1016/j.cemconcomp.2007.08.004 ↗
17. Supplementary Cementitious Materials10.2138/rmg.2012.74.6 ↗
18. Use of natural zeolite as a supplementary cementitious material10.1016/j.cemconcomp.2009.10.006 ↗
19. The effect of zeolite on the properties and hydration of blended cements10.1016/j.cemconcomp.2009.10.004 ↗
20. Properties of cement mortars containing clinoptilolite as a supplementary cementitious material10.1016/j.conbuildmat.2011.02.006 ↗
21. The possibility of self-curing concrete
22. Internal curing and autogenous shrinkage of high-strength concrete
23. T.A. Bier, B. Stolte, H. Tokushige, M. Kawakami, Early shrinkage as influenced by water movement in mortars containing zeolites, in: Proc 9th Int. Symp. on high performance concrete-design, verification & utilization, energy events Centre, Rotorua, New Zealand, 2011.
24. An investigation on the use of zeolite aggregates for internal curing of concrete10.1016/j.conbuildmat.2012.10.009 ↗
25. Calcining natural zeolites to improve their effect on cementitious mixture workability10.1016/j.cemconres.2016.04.002 ↗
26. Monitoring the effect of hydrothermal treatments on the structure of a natural zeolite through a combined XRD, FTIR, XRF, SEM and N2-porosimetry analysis10.1016/j.micromeso.2010.05.004 ↗
27. Natural zeolites as effective adsorbents in water and wastewater treatment10.1016/j.cej.2009.10.029 ↗
28. Atrazine adsorption by acid-activated zeolite-rich tuffs10.1016/j.clay.2010.04.008 ↗
29. The effect of HCl treatment on water vapor adsorption characteristics of clinoptilolite rich natural zeolite10.1016/j.micromeso.2004.08.013 ↗
30. The effect of acid treatment on the reactivity of natural zeolites used as supplementary cementitious materials10.1016/j.cemconres.2015.08.007 ↗
31. Effects of the secondary minerals of the natural pozzolans on their pozzolanic activity10.1016/j.cemconres.2008.02.005 ↗
32. The effect of various treatment conditions on natural zeolites: ion exchange, acidic, thermal and steam treatments10.1016/j.jcis.2012.01.017 ↗
33. Factors Affecting Threshold Chloride for Reinforcement Corrosion in Concrete10.1016/0008-8846(95)00148-6 ↗
34. ASTM C1698 · 2009
35. ASTM C191 · 2013
36. Examining the “time-zero” of autogenous shrinkage in high/ultra-high performance cement pastes10.1016/j.cemconres.2017.03.010 ↗
37. Composition, optical properties, cell dimensions and thermal stability of some heulandite group zeolites
38. Brunauer · 1943 · Volume I
39. Jensen · 1993
40. P. Lura, B. Lothenbach, Influence of pore solution chemistry on shrinkage of cement paste, in: RILEM Proceedings 071: The 50-year Teaching and Research Anniversary of Prof. Sun Wei on Advances in Civil Engineering Materials, 2010, pp. 191–200.
41. Prediction of self-desiccation in low water-to-cement ratio pastes based on pore structure evolution10.1016/j.cemconres.2013.03.013 ↗
42. L.E. Burris, Increasing the reactivity of natural zeolites used as supplementary cementitious materials, The University of Texas at Austin, PhD thesis, 2014.