Incorporation mechanism of titanium in Portland cement clinker and its effects on hydration properties
Source abstract
Abstract
Abstract Titanium is a trace element that might be introduced by industrial wastes to the cement kilns. In this study, the effect of TiO 2 on cement clinker phase formation, ion substitution as well as hydration properties were evaluated by free lime test, X-ray diffraction (XRD), scanning electron microscope-energy dispersive spectrometer (SEM-EDS), isothermal heat-conduction and nuclear magnetic resonance (NMR). Results indicated that titanium was preferentially incorporated in the interstitial phases, especially in C 4 AF, then C 3 A, C 2 S and C 3 S, which could be attributed to the lattice substitution of Ti 4+ to Fe 3+ in C 4 AF and consequently weakened its crystallinity. Meanwhile, the threshold limit for TiO 2 incorporated into clinker was 1.5 wt%, beyond which, the crystal form of C 3 A transformed from cubic to orthorhombic. These changes of C 3 A and C 4 AF promoted the formation of C 3 S by decreasing the liquid phase viscosity during the sintering process. TiO 2 -doped promoted the hydraulic activity of clinker in initial period while postponed the hydration process of C 3 S in later period. However, after 28 days hydration, C–S–H gel polymerization degree did not decrease but improved as the TiO 2 dosage was below 1.5 wt%.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete and Cement Materials Research · Innovative concrete reinforcement materials · Recycled Aggregate Concrete Performance
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. New cement blend to cut CO2 emissions by up to 30%
2. Low carbon measures for cement plant – a review10.1016/j.jclepro.2014.11.003 ↗
3. Waste fibre cement: an interesting alternative raw material for a sustainable Portland clinker production10.1016/j.conbuildmat.2012.04.095 ↗
4. Studies on the solidification mechanisms of Ni and Cd in cement clinker during cement kiln co-processing of hazardous wastes10.1016/j.conbuildmat.2013.12.081 ↗
5. Incorporation of V, Zn and Pb into the crystalline phases of Portland clinker10.1016/S0008-8846(02)00928-6 ↗
6. Incorporation of trace elements in Portland cement clinker: thresholds limits for Cu, Ni, Sn or Zn10.1016/j.cemconres.2011.07.006 ↗
7. Alternative fuels in the cement manufacturing process
8. Utilization of municipal sewage sludge as additives for the production of eco-cement10.1016/j.jhazmat.2012.02.020 ↗
9. Effect of SO3 and MgO on Portland cement clinker: Formation of clinker phases and alite polymorphism10.1016/j.conbuildmat.2014.02.029 ↗
10. Effect of Cr(VI) on the hydration behavior of marble dust blended cement: solidification, leachability and XRD analyses10.1016/j.conbuildmat.2007.04.022 ↗
11. Feature on the role of minor compounds in cement clinker – part l
12. Gartner · 1980
13. The effect of foreign ions on the reactivity of the CaO-SiO2-Al2O3-Fe2O3 system Part II: cations10.1016/S0008-8846(01)00705-0 ↗
14. Influence of titania on the formation of tricalcium silicate10.1016/S0008-8846(98)00231-2 ↗
15. An evaluation of the incorporation of a titanium dioxide producer’s waste material in Portland cement clinker10.1016/S0167-577X(02)00723-1 ↗
16. Miller · 1976 · 16
17. The incorporation of TiO2 into the phases of Portland cement clinker
18. B.V. Volkonskii, S.D. Makashev, N.P. Shteiert. Effect of Phosphorus, Titanium, Manganese and Chromium Compounds on the Clinkering Processes and the Quality of Cement, 1974.
19. Polymorphism and phase changes in the ferrite phase of cements induced by titanium substitution10.1016/0008-8846(84)90054-1 ↗
20. Utilization of municipal sewage sludge as additives for the production of eco-cement10.1016/j.jhazmat.2012.02.020 ↗
21. Hydration of ordinary portland cements made from raw mix containing transition element oxides 110.1016/S0008-8846(97)00250-0 ↗
22. Crystal structure refinement and hydration behaviour of doped tricalcium aluminate10.1016/j.cemconres.2006.06.001 ↗
23. The calcium silicate hydrates10.1016/j.cemconres.2007.11.005 ↗
24. Hydration characteristics and hydration products of tricalcium silicate doped with a combination of MgO, Al2O3 and Fe2O310.1016/j.tca.2008.03.013 ↗
25. High intakes of Cr, Ni, and Zn in clinker: Part I. Influence on burning process and formation of phases10.1016/S0008-8846(99)00195-7 ↗
26. Taylor · 1997
27. Effect of TiO2 on formation of clinker with high C3S
28. Effect of the clinker composition on the threshold limits for Cu, Sn or Zn10.1016/j.cemconres.2012.05.002 ↗
29. A discussion of the paper “a new perspective of the hydration characteristics of cement phases” by J.J. Beaudoin and V.S. Ramachandran10.1016/0008-8846(93)90115-P ↗
30. C 4 AF reactivity—chemistry and hydration of industrial cement
31. Incorporation and substitution mechanism of cadmium in cement clinker10.1016/j.jclepro.2015.09.127 ↗
32. Structural studies of silicates by high-resolution 29Si NMR10.1021/ja00535a008 ↗