journal article·2015-01

An investigation on very high volume slag pastes subjected to elevated temperatures

Alaa M. Rashad

Publisher page

Abstract

Abstract In this investigation, high volume slag (HVS) pastes were studied under heat treatment. Portland cement (PC) was replaced with ground granulated blast-furnace slag (shortened as slag) at levels of 0%, 85%, 90%, 95% and 100%, by weight. The pastes were exposed to elevated temperatures ranging from 200 °C to 800 °C with an increment of 200 °C for 2 h. Compressive strengths and pH values before and after firing were measured. The various decomposition phases formed were identified using X-ray diffraction (XRD) and thermogravimetric (TGA) analyses. The morphology of the formed hydrates was studied using scanning electron microscopy (SEM). Visual inspections were also conducted. The results showed an increase in the reference compressive strength of HVS pastes with heat treatment up to 600 °C, then a reduction at 800 °C was observed. The relative compressive strength of HVS pastes was higher than that of 100% PC paste. The optimum slag content was 85% which exhibited residual compressive strength comparable to that of 100% PC at 600 °C and 800 °C. The pH values of the pastes decreased with increasing heat treatment and slag content.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Fire effects on concrete materials · Concrete and Cement Materials Research · Innovative concrete reinforcement materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Global warming impact on the cement and aggregates industries
2. Hendriks CA, Worrell E, de Jager D, Blok K, Riemer P. Emission reduction of greenhouse gases from the cement industry. In: IEA greenhouse gas control technologies conference; 2004.
3. The effect of activator concentration on the residual strength of alkali-activated fly ash pastes subjected to thermal load10.1016/j.conbuildmat.2010.12.044 ↗
4. Hydration and properties of sodium sulfate activated slag10.1016/j.cemconcomp.2012.12.010 ↗
5. Alkali-activated composites based on slag from iron and steel metallurgy
6. Alkali activated cements opportunities and challenges10.1016/S0008-8846(98)00093-3 ↗
7. High performance cementing materials from industrial slags – a review10.1016/S0921-3449(99)00060-9 ↗
8. Studies on Portland cement with large amount of slag10.1016/S0008-8846(00)00208-8 ↗
9. Supplementary cementing materials10.1007/978-3-642-17866-5 ↗
10. Compressive strength of concrete mixtures with binary and ternary cement blends
11. Monitoring electrical resistance of concretes containing alternative cementitious materials to assess their resistance to chloride penetration10.1016/S0958-9465(01)00075-0 ↗
12. Laboratory investigation of low-permeability concretes containing slag and silica fume
13. Investigation of the influence of blast-furnace slag on the resistance of concrete against organic acid or sulphate attack by means of accelerated degradation tests10.1016/j.cemconres.2011.09.009 ↗
14. Durability and strength evaluation of high-performance concrete in marine structure10.1016/j.conbuildmat.2010.01.013 ↗
15. An experimental study on corrosion resistance of concrete with ground granulated blast furnace slag10.1016/j.cemconres.2004.11.010 ↗
16. Shah · 1994
17. Phase transformations and mechanical strength of OPC/slag pastes submitted to high temperatures10.1617/s11527-007-9247-8 ↗
18. Long-term progressive deterioration following fire exposure of OPC versus slag blended cement pastes10.1617/s11527-008-9369-7 ↗
19. Development of a high-temperature-resistant mortar by slag and pumice10.1016/j.firesaf.2008.02.001 ↗
20. Effect of elevated temperature on physic-mechanical properties of blended cement concrete10.1016/j.conbuildmat.2010.06.078 ↗
21. Effects of elevated temperatures on properties of concrete containing ground granulated blast furnace slag as cementitious material10.1016/j.conbuildmat.2012.04.103 ↗
22. Residual compressive behavior of pre-heated high-performance concrete with blast-furnace-slag10.1016/j.firesaf.2005.11.001 ↗
23. Chemical and mechanical stability of sodium sulfate activated slag after exposure to elevated temperature10.1016/j.cemconres.2011.10.007 ↗
24. Phan · 1996
25. A study on durability properties of high-performance concretes incorporating high replacement levels of slag10.1617/s11527-007-9260-y ↗
26. Wet and dry cured compressive strength of concrete containing ground granulated blast-furnace slag10.1016/j.buildenv.2006.07.027 ↗
27. Mineral admixtures contribution to the development of heat of hydration and strength10.1520/CCA10293J ↗
28. Mechanical properties of hardened cement paste exposed to temperature up to 700°C, 1292F
29. Use of coconut husk ash, corn cob ash and peanut shell ash as cement replacement
30. Change in microstructure of hardened cement paste subjected to elevated temperatures10.1016/j.conbuildmat.2006.11.002 ↗
31. Microstructure of fire-damaged concrete
32. Böhni · 2005