The effect of curing temperature on white cement hydration
Source abstract
Abstract
Cement manufacture has undergone extensive change in its attempts to rise to the successive challenges posed by society. The hydration of Portland cement is a complex phenomenon that depends on both reagent characteristics and reaction conditions. It is a well-known fact that the curing temperature plays an important role on the hydration kinetics. The present study is the first to be undertaken on the effect of curing temperature on white Portland cement paste hydration over long hydration times (365 days at 20ºC and 124 days at 60 ºC). The technique used, 29Si and 27Al NMR spectroscopy, is particularly well adapted to the study of cement hydration. White cement hydration generates a C-S-H gel in which the aluminium taken up forms bridge bonds. After nine days at 60 ºC, the degree of reaction expressed in terms of the Al(IV)/Al(VI) ratio nearly doubles the value found after 90 days at 20 ºC.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete and Cement Materials Research · Concrete Properties and Behavior · Magnesium Oxide Properties and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (27)
Show source-provided references
1. Massazza F, Daimond M. Chemistry of hydration of cements and cementitious systems. In: National council for cement and building materials. Proceedings of ninth international congress on the chemistry of cement. The offsetters, vol. 1. New Delhi, India; 1992. p. 383–448.
2. Phase-resolved strain measurements in hydrated ordinary Portland cement using synchrotron X-rays10.1111/j.1551-2916.2006.01118.x ↗
3. Effect of curing conditions on the mortars with and without GGBFS10.1016/j.conbuildmat.2006.08.013 ↗
4. The effect of metakaolin on the reaction products and microporosity in blended pastes submitted to long hydration time and high curing temperature
5. Influence of metastable hydrated phases on the pore size distribution and degree of hydration of MK blended cements cured at 60°C10.1016/j.cemconres.2004.10.038 ↗
6. Study of hydrated phases present in a MK-lime system cured at 60°C and 60 months of reaction10.1016/j.cemconres.2006.01.001 ↗
7. Effect of hydration temperature on cement paste structure
8. Reaction kinetics of Portland cement mortars hydrated at different temperatures10.1016/0008-8846(92)90141-H ↗
9. Asaga K, Ishizaki M, Takahashi S, Konoshi K, Tsurumi T, Diamond M. Effect of curing temperature on the hydration of cement Portland compounds. In: National council for cement and building materials. Proceedings of the ninth international congress on the chemistry of cement. The offsetters, vol. 4. New Delhi, India; 1992. p. 181–7.
10. Hydration setting and hardening of Portland cement
11. Effects of the temperature and relative humidity on the structure of CSH gel10.1016/0008-8846(95)00116-T ↗
12. Scrivener KL, Wieker W. Advances in hydration at low, ambient and elevated temperatures. In: National council for cement and building materials. Proceedings of the ninth international congress on the chemistry of cement, vol. 1. New Delhi, India; 1992. p. 449–57.
13. Impact of prolonged warm (85°C) moist cure on Portland cement paste10.1016/S0008-8846(00)00286-6 ↗
14. Silicate polymerization during the hydration of alite10.1016/0008-8846(83)90089-3 ↗
15. Micro-Raman spectroscopy in white Portland cement hydration: long-term study at room temperature10.1002/jrs.1428 ↗
16. Incorporation of aluminium in the calcium silicate hydrate (C–S–H) of hydrated Portland cements: a high-field 27Al and 29Si MAS NMR investigation10.1021/ic020607b ↗
17. The role of Al in C–S–H: NMR, XRD, and compositional results for precipitated sample10.1016/j.cemconres.2005.03.002 ↗
18. 29Si and 27Al MASNMR study of Strätlingite10.1111/j.1151-2916.1995.tb08910.x ↗
19. Influence of MK on the reaction kinetics in MK/lime and MK-blended cement systems at 20°C10.1016/S0008-8846(00)00465-8 ↗
20. 29Si and 27Al high-resolution NMR characterization of calcium silicate hydrate phases in activated blast-furnace slag pastes10.1016/S0008-8846(01)00530-0 ↗
21. Effect of quartz content on the nature of Al-substituted 11 ang tobermorite in hydrothermally treated CaO-Al2O3–SiO2–H2O systems10.1680/adcr.1999.11.4.179 ↗
22. Characterization of calcium aluminate phases in cements by 27Al MAS NMR spectroscopy10.1021/ic00058a043 ↗
23. Hydration of C3A in the presence of Ca(OH)2, CaSO4·H2O and CaCO310.1016/0008-8846(91)90183-I ↗
24. The nature of C–S–H in hardened cements10.1016/S0008-8846(99)00168-4 ↗
25. Location of aluminium in substituted calcium silicate hydrate (C–S–H) gels as determined by 29Si and 27Al NMR and EELS10.1111/j.1151-2916.1993.tb07765.x ↗
26. 29Si solid state NMR study of tricalcium silicate and cement hydration at high temperature10.1016/0008-8846(93)90177-B ↗
27. Direct synthesis and hydration of calcium aluminosulfate (Ca4Al6O16S)10.1111/j.1151-2916.2002.tb00129.x ↗