journal article·2020-08

Mechanism of blended steel slag mortar with CO2 curing exposed to sulfate attack

Jun Chang, Yangyang Gu, Wajahat Sammer Ansari

Publisher page

Abstract

Abstract Steel slag is a by-product of the steel manufacturing process and can be used as a filler material in cementitious composites. Past researches show CO2 curing solves the problem of poor stability of steel slag and results in good mechanical behavior but their durability characteristics are still unknown. This paper aims to evaluate the performance of CO2 cured blended steel slag exposed to 3 wt% Na2SO4 solutions for up to 120 days. As a comparison, the conventionally cured ordinary Portland cement (OPC) specimens were prepared and taken the same exposure method. The resistance ability of the specimens was evaluated by visual observation, corrosion resistance coefficient K and microstructural analysis. CO2 cured blended steel slag showed better sulfate resistance ability in terms of K values and visual observation compared with OPC for 120 days. The microstructural analysis revealed that much less expansive erosion products ettringite and gypsum were formed in CO2 cured blended steel slag specimens than OPC specimens until 120 days. The small amounts of erosion products in CO2 cured blended steel slag specimens resulted in a decrease of porosity, a denser microstructure than before and increment of strength. However, the accumulation of large amounts of erosion products in internal pores of OPC specimens led to an increase of porosity, a looser microstructure, and degradation. Thus the CO2 cured blended steel slag has good efficiency in sulfate resistance and can be adopted in the construction industry to attain its benefits.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Concrete and Cement Materials Research · Rock Mechanics and Modeling · Concrete Properties and Behavior

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (58)

Show source-provided references
1. Changes in mineralogical and leaching properties of converter steel slag resulting from accelerated carbonation at low CO2 pressure10.1016/j.wasman.2011.05.022 ↗
2. Cementitious and pozzolanic behavior of electric arc furnace steel slags10.1016/j.cemconres.2008.11.002 ↗
3. High-strength KOBM steel slag binder activated by carbonation10.1016/j.conbuildmat.2015.09.028 ↗
4. Effect of accelerated carbonation on AOD stainless steel slag for its valorisation as a CO2-sequestering construction material10.1016/j.cej.2014.02.051 ↗
5. Development of large steelmaking slag blocks using a new carbonation process10.1680/adcr.2000.12.3.97 ↗
6. Mechanical performance and microstructure of the calcium carbonate binders produced by carbonating steel slag paste under CO2 curing10.1016/j.cemconres.2016.05.013 ↗
7. Monitoring of stainless-steel slag carbonation using X-ray computed microtomography10.1021/es402767q ↗
8. Durability of concrete structures in tropical atoll environment10.1016/j.oceaneng.2017.02.020 ↗
9. Durability of concrete-degradation phenomena involving detrimental chemical reactions10.1016/j.cemconres.2007.09.015 ↗
10. The effect of temperature on the rate of sulfate attack of Portland cement blended mortars in Na2SO4 solution10.1016/j.cemconres.2015.02.024 ↗
11. Advanced testing and performance specifications for the cementitious materials under external sulfate attacks10.1016/j.conbuildmat.2016.09.133 ↗
12. Behavior of mortar exposed to different exposure conditions of sulfate attack10.1016/j.oceaneng.2018.03.017 ↗
13. Current knowledge of external sulfate attack10.1680/adcr.14.00089 ↗
14. Salt weathering distress on concrete exposed to sodium sulfate environment
15. Experimental asymptotic analysis of expansion of concrete exposed to sulfate attack
16. Effect of calcium chloride and initial curing temperature on expansion caused by sulfate exposure
17. Carbon sequestration through accelerated carbonation of BOF slag: influence of particle size characteristics10.1016/j.cej.2016.04.015 ↗
18. GB/T 17671-1999, Method of testing cements-Determination of strength, 1999.
19. GB/T 749-2008, Test method for determining the capability of resisting sulfate corrode of cement, 2008.
20. Rapid hardening β-C2S mineral and microstructure changes activated by accelerated carbonation curing10.1007/s10973-017-6165-z ↗
21. Effects of mineralogical changes in BOFS during carbonation on pH and Ca and Si leaching10.1016/j.conbuildmat.2018.10.057 ↗
22. Durability of concrete exposed to leaching and external sulphate attacks10.1016/j.cemconres.2009.07.021 ↗
23. The confused world of sulfate attack on concrete10.1016/j.cemconres.2004.04.004 ↗
24. Degradation mechanisms of Portland cement mortar under seawater attack and drying-wetting cycles10.1016/j.conbuildmat.2019.116934 ↗
25. Sulfate resistance of carbonated ternary mortar blends: Portland cement, reactive MgO and supplementary cementitious materials10.1016/j.jclepro.2019.117933 ↗
26. Effects of biaxial confinement in mortars exposed to external sulfate attack10.1016/j.cemconcomp.2018.10.017 ↗
27. New procedure to investigate external sulphate attack on cementitious materials10.1016/j.cemconcomp.2011.11.010 ↗
28. Radojevic · 1999
29. Effect of limestone filler on the deterioration of mortars and pastes exposed to sulfate solutions at ambient temperature10.1016/j.cemconres.2007.08.003 ↗
30. Effects of gypsum formation on the performance of cement mortars during external sulfate attack10.1016/S0008-8846(02)00955-9 ↗
31. Multi-criteria analysis of the mechanism of degradation of Portland cement based mortars exposed to external sulphate attack10.1016/j.cemconres.2012.06.005 ↗
32. Ye’elimite synthesis by chemical routes10.1016/j.jeurceramsoc.2018.10.025 ↗
33. Rietveld quantitative phase analysis of Yeelimite-containing cements10.1016/j.cemconres.2012.03.018 ↗
34. R values in analysis of powder diffraction data using Rietveld refinement10.1107/S0021889893012348 ↗
35. Effects of amorphous AH3 phase on mechanical properties and hydration process of C4A3S̅-CS̅H2-CH-H2O system10.1016/j.conbuildmat.2016.11.111 ↗
36. Effect of sulfate attack on the stress-strain relationship of FRP-confined concrete10.1016/j.conbuildmat.2015.12.038 ↗
37. The sulfate corrosion resistance behavior of slag cement mortar10.1016/j.conbuildmat.2014.08.019 ↗
38. Deterioration mechanism of plain and blended cement mortars partially exposed to sulfate attack10.1016/j.conbuildmat.2017.08.017 ↗
39. Microstructure changes of waste hydrated cement paste induced by accelerated carbonation10.1016/j.conbuildmat.2014.12.017 ↗
40. Kinetic study of ettringite carbonation reaction10.1016/0008-8846(94)90123-6 ↗
41. Changes in microstructure characteristics of cement paste on carbonation10.1016/j.cemconres.2018.04.016 ↗
42. Microstructural origins of cement paste degradation by external sulfate attack10.1016/j.conbuildmat.2015.07.186 ↗
43. Influence of silica fume replacement of cement on physical properties and resistance to sulfate attack, freezing and thawing, and alkali-silica reactivity
44. Modeling of damage in cement-based materials subjected to external sulfate attack - part 1: formulation
45. Sulfate attack on concrete: separating myths from reality
46. FTIR study of the sol-gel synthesis of cementitious gels: C-S-H and N-A-S-H10.1007/s10971-007-1643-6 ↗
47. The role of β-C2S and γ-C2S in carbon capture and strength development10.1617/s11527-016-0797-5 ↗
48. Quantitative analysis of synthetic calcium carbonate polymorphs using FT-IR spectroscopy10.1016/S0039-9140(02)00638-0 ↗
49. Comparison of FT-IR, Thermal Analysis and XRD for Determination of Products of Cement Hydration10.4028/www.scientific.net/AMR.168-170.518 ↗
50. A Fourier transform infrared spectroscopic investigation of the early hydration of Portland cement and the influence of sodium lignosulfonate10.1016/S0008-8846(99)00243-4 ↗
51. Attack of limestone cement-based material exposed to magnesium sulfate solution at low temperature10.1007/s11595-014-0949-9 ↗
52. The effects of carbonation and hydration on the mineralogy and microstructure of basic oxygen furnace slag products10.1016/j.jcou.2019.06.001 ↗
53. Deterioration mechanisms of sulfate attack on concrete under alternate action10.1007/s11595-010-2355-2 ↗
54. Study of deterioration of concrete exposed to different types of sulfate solutions under drying-wetting cycles10.1016/j.conbuildmat.2016.04.094 ↗
55. Effects of accelerated carbonation on the microstructure of Portland cement pastes containing reactive MgO10.1016/j.cemconres.2012.02.017 ↗
56. Scrivener · 2018
57. Investigation of concrete exposed to dual sulfate attack10.1016/j.cemconres.2014.06.002 ↗
58. Durability of geopolymer materials in sodium and magnesium sulfate solutions10.1016/j.cemconres.2004.09.002 ↗