Effect of dry/wet ratio and pH on the stress corrosion cracking behavior of rusted X100 steel in an alternating dry/wet environment
Source abstract
Abstract
Abstract The stress corrosion cracking (SCC) behavior of X100 steel under alternating dry/wet conditions was investigated through electrochemical experiments and slow strain-rate testing. The results show that the corrosion morphology transforms from general corrosion to pitting with increasing dry/wet ratio (D/W). The corrosion product layer becomes less protective with decreasing pH, which leads to pitting and shows that anodic dissolution is promoted. In addition, local acidification under the corrosion product layer promotes the hydrogen evolution reaction. We conclude that the SCC mechanism of X100 steel under alternating dry/wet conditions at low pH and a high D/W ratio involves anodic dissolution and hydrogen evolution.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (66)
Show source-provided references
1. Corrosion behavior of X65 pipeline steel: Comparison of wet–Dry cycle and full immersion10.1016/j.corsci.2018.01.007 ↗
2. Corrosion fatigue crack growth modelling for subsea pipeline steels10.1016/j.oceaneng.2017.06.057 ↗
3. Hydrostatic pressure effects on stress corrosion cracking of X70 pipeline steel in a simulated deep-sea environment10.1016/j.ijhydene.2017.09.061 ↗
4. Hydrostatic pressure effects on corrosion behavior of X70 pipeline steel in a simulated deep-sea environment10.1016/j.jelechem.2018.05.010 ↗
5. Three-dimensional Finite Element Analysis for Flying Shearing of X100 Hot-rolled Steel Plate10.1016/j.proeng.2014.10.355 ↗
6. Effect of sulfate-reducing bacteria and cathodic potential on stress corrosion cracking of X70 steel in sea-mud simulated solution10.1016/j.msea.2018.02.007 ↗
7. Hydrogen induced cracking susceptibility of API 5L X70 pipeline steel in relation to microstructure and crystallographic texture developed after different thermomechanical treatments10.1016/j.matchar.2018.08.034 ↗
8. Effect of SO2 content on SCC behavior of E690 high-strength steel in SO2-polluted marine atmosphere10.1016/j.oceaneng.2018.06.051 ↗
9. Electrochemical mechanism of stress corrosion cracking of API X70 pipeline steel under different AC frequencies10.1016/j.conbuildmat.2018.03.209 ↗
10. Characterization of fiber laser welds in X100 pipeline steel10.1016/j.matdes.2008.09.042 ↗
11. Corrosion inhibition of API X120 steel in a highly aggressive medium using stearamidopropyl dimethylamine10.1016/j.molliq.2017.03.116 ↗
12. Effect of temperature and erosion on pitting corrosion of X100 steel in aqueous silica slurries containing bicarbonate and chloride content10.1016/j.corsci.2014.01.021 ↗
13. Failure assessment and safe life prediction of corroded oil and gas pipelines10.1016/j.petrol.2016.12.029 ↗
14. Local chemistry–electrochemistry and stress corrosion susceptibility of X80 steel below disbonded coating in acidic soil environment under cathodic protection10.1016/j.conbuildmat.2020.118203 ↗
15. Comparative study of the stress corrosion behavior of a multiuse bainite steel in the simulated tropical marine atmosphere and seawater environments10.1016/j.conbuildmat.2019.117903 ↗
16. Crack growth behaviour of E690 steel in artificial seawater with various pH values10.1016/j.corsci.2019.108336 ↗
17. Fundamental investigation of stress corrosion cracking of E690 steel in simulated marine thin electrolyte layer10.1016/j.corsci.2018.12.029 ↗
18. Guo · 2014
19. Modelling of pitting corrosion in marine and offshore steel structures – A technical review10.1016/j.jlp.2015.06.008 ↗
20. Corrosion mechanisms of mild steel in chloride-rich atmospheres10.1002/maco.201508488 ↗
21. A SEM/XPS/SKP study on the distribution of chlorides in contaminated rusty steel10.1016/j.corsci.2005.07.009 ↗
22. Long-term atmospheric corrosion of mild steel10.1016/j.corsci.2010.10.007 ↗
23. Methods for salt contamination of steel corrosion products: A characterization study10.1002/maco.200704061 ↗
24. Schumacher · 1979
25. A.A. Younis, M.M.B. El-Sabbah, R. Holze, The effect of chloride concentration and pH on pitting corrosion of AA7075 aluminum alloy coated with phenyltrimethoxysilane, J Solid State Electr 16(3) (2012) 1033-1040.10.1007/s10008-011-1476-7 ↗
26. Electrochemical corrosion, hydrogen permeation and stress corrosion cracking behavior of E690 steel in thiosulfate-containing artificial seawater10.1016/j.corsci.2018.08.048 ↗
27. Passivation behavior and surface chemistry of 2507 super duplex stainless steel in artificial seawater: Influence of dissolved oxygen and pH10.1016/j.corsci.2019.02.002 ↗
28. Corrosion behavior of E690 high-strength steel in alternating wet-dry marine environment with different pH values10.1007/s11665-015-1781-x ↗
29. Effect of pH and hydrogen on the stress corrosion cracking behavior of duplex stainless steel in marine atmosphere environment10.1016/j.oceaneng.2017.10.002 ↗
30. Electrochemical Behavior of Rust Formed on Carbon Steel in a Wet/Dry Environment Containing Chloride Ions10.5006/1.3280597 ↗
31. S. Feliu, M. Morcillo, Corrosión y protección de los metales en la atmósfera, 1982.
32. An study on accelerated corrosion testing of weathering steel10.1016/j.matchemphys.2013.07.009 ↗
33. Role of climatic conditions on corrosion characteristics of structural steels10.1016/j.corsci.2007.06.026 ↗
34. The effects of temperature and pH on the characteristics of corrosion product in CO2 corrosion of grade X70 steel10.1016/j.matdes.2010.01.038 ↗
35. The effect of hydrogen on stress corrosion behavior of X65 steel welded joint in simulated deep sea environment10.1016/j.oceaneng.2016.01.020 ↗
36. Comparative study on the stress corrosion cracking of X70 pipeline steel in simulated shallow and deep sea environments10.1016/j.msea.2016.12.118 ↗
37. Comparative study on corrosion behaviour of rusted X100 steel in dry/wet cycle and immersion environments10.1016/j.conbuildmat.2019.117440 ↗
38. Atmospheric corrosion of field-exposed AZ31 magnesium in a tropical marine environment10.1016/j.corsci.2013.06.047 ↗
39. The inhibition effect of tannic acid on mild steel corrosion in seawater wet/dry cyclic conditions10.1016/j.corsci.2013.01.040 ↗
40. Effects of solution pH and Cl− on electrochemical behaviour of an Aermet100 ultra-high strength steel in acidic environments10.1016/j.corsci.2011.08.024 ↗
41. Corrosion inhibition of mild steel by aerobic biofilm10.1016/j.electacta.2005.02.017 ↗
42. Corrosion characterization of new tin–silver binary alloys in nitric acid solutions10.1016/j.corsci.2008.02.003 ↗
43. The role of Zn precipitates and Cl− anions in pitting corrosion of Sn–Zn solder alloys10.1016/j.corsci.2014.12.014 ↗
44. In situ observation of initial rust formation process on carbon steel under Na2SO4 and NaCl solution films with wet/dry cycles using synchrotron radiation X-rays10.1016/j.corsci.2004.10.021 ↗
45. The long term growth of the protective rust layer formed on weathering steel by atmospheric corrosion during a quarter of a century10.1016/0010-938X(94)90158-9 ↗
46. On the atmospheric corrosion of metals which are covered with thin electrolyte layers—II. Experimental results10.1016/0010-938X(90)90033-2 ↗
47. Electrochemical measurements of time-of-wetness and atmospheric corrosion rates10.5006/0010-9312-33.1.13 ↗
48. Laboratory studies of atmospheric corrosion—I. Weight loss and electrochemical measurements10.1016/0010-938X(80)90119-5 ↗
49. Electrochemical monitoring of atmospheric corrosion phenomena10.1016/0010-938X(76)90052-4 ↗
50. Corrosion resistance and mechanical properties of low-alloy steels under atmospheric conditions10.1016/j.corsci.2004.04.009 ↗
51. Corrosion of low carbon steel in atmospheric environments of different chloride content10.1016/j.corsci.2009.02.009 ↗
52. Electrochemical mechanism of atmospheric rusting10.1038/206980a0 ↗
53. Composition and protective ability of rust layer formed on weathering steel exposed to various environments10.1016/j.corsci.2005.10.004 ↗
54. J. Dong, J. Dong, E. Han, C. Liu, W.J.C.S. Ke, P. Technology, Corrosion Behavior of Rusted Mild Steel under Wet/Dry Alternate Conditions, 18(6) (2006) 414.
55. K.W.D. Junhua, Study on the rusting evolution and the performance of resisting to atmospheric corrosion for Mn-Cu Steel, 46(11) (2010) 1365-1378.10.3724/SP.J.1037.2010.01365 ↗
56. On the akaganéite crystal structure, phase transformations and possible role in post-excavational corrosion of iron artifacts10.1016/S0010-938X(03)00078-7 ↗
57. Akaganéite-type β-FeO(OH) nanocrystals: preparation and characterization10.1016/S1387-1811(00)00259-6 ↗
58. Lattice vibration spectra. Part XCV. Infrared spectroscopic studies on the iron oxide hydroxides goethite (α), akaganéite (β), lepidocrocite (γ), and feroxyhite (δ)10.1016/S0992-4361(99)80017-4 ↗
59. Effect of NaCl on rusting of steel in wet and dry corrosion cycle10.2355/tetsutohagane1955.81.11_1079 ↗
60. Electrochemical study of indoor atmospheric corrosion layers formed on ancient iron artefacts10.1016/j.electacta.2007.04.029 ↗
61. Corrosion evolution and stress corrosion cracking of E690 steel for marine construction in artificial seawater under potentiostatic anodic polarization10.1016/j.conbuildmat.2019.117763 ↗
62. On the formation of β-FeOOH (akaganéite) in chloride-containing environments10.1016/j.corsci.2006.06.003 ↗
63. Influence of cations and anions on the formation of β-FeOOH10.1016/j.corsci.2004.10.014 ↗
64. Influences of metal ions on the formation of β-FeOOH particles10.1016/S0010-938X(00)00153-0 ↗
65. Characterization of the rust formed on weathering steel exposed to Qinghai salt lake atmosphere10.1016/j.corsci.2007.06.020 ↗
66. Combined effect of cathodic potential and sulfur species on calcareous deposition, hydrogen permeation, and hydrogen embrittlement of a low carbon bainite steel in artificial seawater10.1016/j.corsci.2019.07.013 ↗