journal article·2020-01

Autogenous and drying shrinkages of mortars and pore structure of pastes made with activated binder of calcium carbide residue and fly ash

Saofee Dueramae, Weerachart Tangchirapat, Prinya Chindaprasirt, Chai Jaturapitakkul, Piti Sukontasukkul

Publisher page

Abstract

Abstract Present study evaluates the strength development and shrinkage characteristics of mortars made with a non-cement binder composed of calcium carbide residue and fly ash under several activation techniques. The activation techniques used for improving the strength development were adding NaOH to the binder (0.5, 1.0, and 1.5% by weight of binder), curing at a temperature of 60 °C, and combining both adding NaOH and curing at a temperature of 60 °C. The compressive strengths of mortars were examined at 3, 7, 28 and 90 days. The shrinkage characteristics of the mortars were evaluated in terms of the autogenous and drying shrinkages. The pore structure of the paste was also analyzed using mercury intrusion porosimetry. The results showed that all of the activation techniques could enhance the compressive strength of mortar and improve the pore structure of the paste made from the mixture of calcium carbide residue and fly ash. The technique to improve strength by combining addition of NaOH and curing at 60 °C was found to be the most effective method, and produced the mortar with a compressive strength as high as 51.1 MPa at 90 days. The shrinkage behaviors of the mortar made from the mixture of calcium carbide residue and fly ash were similar to the ordinary Portland cement mortar. The autogenous shrinkage was associated with the internal reaction process, while the drying shrinkage was depended on evaporation of water in pore structures during the drying process. Additionally, the use of NaOH as an activator significantly increased the magnitude of the autogenous and drying shrinkages of mortar. However, the drying shrinkage was greatly reduced with the activation by curing at 60 °C.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Concrete and Cement Materials Research · Innovative concrete reinforcement materials · Concrete Properties and Behavior

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (40)

Show source-provided references
1. Trends and developments in green cement and concrete technology10.1016/j.ijsbe.2013.05.001 ↗
2. Global concrete industry sustainability
3. Alkali-activated fly ashes: a cement for the future10.1016/S0008-8846(98)00243-9 ↗
4. Shi · 2003
5. Davidovits · 2008
6. Effects of calcium carbide residue–fly ash binder on mechanical properties of concrete10.1061/(ASCE)MT.1943-5533.0000127 ↗
7. Microstructure of calcium carbide residue–ground fly ash paste10.1061/(ASCE)MT.1943-5533.0000167 ↗
8. The effect of type and concentration of activators on flowability and compressive strength of natural pozzolan and slag-based geopolymers10.1016/j.conbuildmat.2016.02.086 ↗
9. Production and performance of alkali-activated cold-bonded lightweight aggregate in concrete10.1016/j.jobe.2018.09.012 ↗
10. Alkali activated clay mortars with different activators10.1016/j.conbuildmat.2019.03.244 ↗
11. Engineering properties of natural pozzolan/slag based alkali-activated concrete10.1016/j.conbuildmat.2019.02.107 ↗
12. Alkali-activated fly ash/slag cements: Strength behaviour and hydration products10.1016/S0008-8846(00)00298-2 ↗
13. The geopolymerisation of alumino-silicate minerals10.1016/S0301-7516(99)00074-5 ↗
14. Alkali-activated fly ash: Effect of thermal curing conditions on mechanical and microstructural development – part II10.1016/j.fuel.2006.07.010 ↗
15. Effect of curing temperature on the development of hard structure of metakaolin-based geopolymer10.1016/j.conbuildmat.2009.12.023 ↗
16. The mechanical properties of fly ash-based geopolymer concrete with alkaline activators10.1016/j.conbuildmat.2013.05.069 ↗
17. Shrinkage characteristics of alkali-activated slag cements10.1061/(ASCE)MT.1943-5533.0001058 ↗
18. Drying and autogenous shrinkage of pastes and mortars with activated slag cement10.1016/j.cemconres.2007.11.002 ↗
19. Understanding the drying shrinkage performance of alkali-activated slag mortars10.1016/j.cemconcomp.2016.11.010 ↗
20. On drying shrinkage in alkali-activated concrete: Improving dimensional stability by aging or heat-curing10.1016/j.cemconres.2016.10.003 ↗
21. ASTM C 618-17 (2017). Standard specification for coal fly ash and raw or calcined natural pozzolan for use in concrete. ASTM International.
22. ASTM C109 (2016). Standard test method for compressive strength of hydraulic cement mortars (using 2-in. or [50-mm] cube specimens). ASTM International.
23. Effect of different curing temperatures on alkali activated palm oil fuel ash paste10.1016/j.conbuildmat.2015.06.052 ↗
24. ASTM C157-17 (2017). Standard test method for length change of hardened hydraulic-cement mortar and concrete. ASTM International.
25. Influence of NaOH solution on the synthesis of fly ash geopolymer10.1016/j.mineng.2009.03.022 ↗
26. Influence of atmospheric steam curing by solar energy on the compressive and flexural strength of concretes10.1016/j.conbuildmat.2013.08.085 ↗
27. Physico-chemical, mechanical, microstructure and durability characteristics of alkali activated Egyptian slag10.1016/j.conbuildmat.2014.07.026 ↗
28. Compressive strength and microstructure of fly ash based geopolymer blended with silica fume under thermal cycle10.1016/j.cemconcomp.2017.01.009 ↗
29. Effect of curing temperatures on the alkali activation of crystalline continuous casting stainless steel slag10.1016/j.conbuildmat.2014.08.067 ↗
30. Mercury porosimetry of hardened cement pastes10.1016/S0008-8846(99)00083-6 ↗
31. The pore structure and permeability of alkali activated fly ash10.1016/j.fuel.2012.05.034 ↗
32. Early-age autogenous cracking of cementitious matrices: physico-chemical analysis and micro/macro investigations10.1617/s11527-010-9663-z ↗
33. Shrinkage characteristics of alkali-activated fly ash/slag paste and mortar at early ages10.1016/j.cemconcomp.2014.07.007 ↗
34. Drying shrinkage mechanisms in Portland cement paste10.1111/j.1151-2916.1987.tb05002.x ↗
35. Influence of activator on the strength and drying shrinkage of alkali-activated slag mortar10.1016/j.conbuildmat.2007.10.011 ↗
36. Spatial distribution of pores in fly ash-based inorganic polymer gels visualised by Wood’s metal intrusion10.1016/j.micromeso.2009.05.016 ↗
37. High-volume fly ash concrete with high strength and low drying shrinkage10.1061/(ASCE)0899-1561(2003)15:2(153) ↗
38. Effect of elevated temperature curing on properties of alkali-activated slag concrete10.1016/S0008-8846(99)00143-X ↗
39. Alkali activation of a slag at ambient and elevated temperatures10.1016/j.cemconcomp.2011.08.003 ↗
40. Shrinkage mitigation strategies in alkali-activated slag10.1016/j.cemconres.2017.08.025 ↗