Effects of high temperature and post-fire-curing on compressive strength and microstructure of calcium carbonate whisker-fly ash-cement system
Source abstract
Abstract
Abstract Building fire disasters may cause large economic loss and casualties. To improve the fire resistance ability of concrete and repair the fire-damaged concrete structures using an in-situ repairing technique (such as post-fire-curing) can greatly offset these adverse effects. Thus, the present study employed fly ash (FA) to form a CW-FA-cement system which was proved to enhance the high-temperature resistance of cement and CW blended cement and was also favorable for recovery of compressive strength and microstructure induced by water re-curing. In details, incorporation of FA was effective to reduce the deterioration of cement and CW blended cement and was favorable for recovery of compressive strength and microstructure after water re-curing. Incorporation of CW was favorable to increase the restorability of compressive strength re-cured after 400 °C and performed a combined effect with FA to improve the recovery of compressive strength re-cured after 800 °C. Through the microstructural tests, the deterioration of compressive strength was due to the decomposition of hydration products. The recovery of compressive strength was due to the rehydration of dehydrated cement, further hydration of unhydrated cement particles, pozzolanic effect of FA and combined effect of CW and FA. Furthermore, the cement blends containing CW and FA had a good high temperature resistance and restorability.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Fire effects on concrete materials · Concrete and Cement Materials Research · Concrete Properties and Behavior
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. Deterioration and recovery of FRC after high temperature exposure10.1016/j.cemconcomp.2018.07.020 ↗
2. The influence of water absorption and porosity on the deterioration of cement paste and concrete exposed to elevated temperatures, as in a fire event10.1016/j.cemconcomp.2012.06.007 ↗
3. Deterioration and recovery of metakaolin blended concrete subjected to high temperature10.1023/A:1021775110075 ↗
4. Comparison of the strength and durability performance of normal- and high-strength pozzolanic concretes at elevated temperatures10.1016/S0008-8846(01)00580-4 ↗
5. High-temperature behaviour of HPC with polypropylene fibres: from spalling to microstructure10.1016/S0008-8846(01)00596-8 ↗
6. Influence of different fibers on the change of pore pressure of self-consolidating concrete exposed to fire10.1016/j.conbuildmat.2016.03.070 ↗
7. Change in microstructure of hardened cement paste subjected to elevated temperatures10.1016/j.conbuildmat.2006.11.002 ↗
8. Effect of high temperature and cooling regimes on the compressive strength and pore properties of high performance concrete10.1016/S0950-0618(00)00031-3 ↗
9. Effect of high temperature on strength and microstructural properties of cemented paste backfill10.1016/j.firesaf.2008.12.004 ↗
10. Influence of PFA on cracking of concrete and cement paste after exposure to high temperatures10.1016/S0008-8846(03)00216-3 ↗
11. Mechanical properties of concrete at high temperature—a review10.1016/j.conbuildmat.2015.05.131 ↗
12. Experimental study of micro/macro crack development and stress–strain relations of cement-based composite materials at elevated temperatures10.1016/j.cemconres.2003.08.029 ↗
13. Influence of high temperature on strength, ultrasonic velocity and mass loss of calcium carbonate whisker reinforced cement paste10.1016/j.compositesb.2019.01.030 ↗
14. Microstructure and Strength of Calcium Carbonate (CaCO3) whisker reinforced cement paste after exposed to high temperatures10.1007/s10694-019-00839-3 ↗
15. High temperature and residual properties of reactive powder concrete – a review10.1016/j.conbuildmat.2017.04.083 ↗
16. Strength and durability recovery of fire-damaged concrete after post-fire-curing10.1016/S0008-8846(01)00582-8 ↗
17. Effect of fly ash and PVA fiber on microstructural damage and residual properties of engineered cementitious composites exposed to high temperatures10.1061/(ASCE)MT.1943-5533.0000335 ↗
18. Experimental research for the effect of high temperature on the mechanical properties of steel fiber-reinforced concrete10.1016/j.conbuildmat.2014.11.005 ↗
19. Fire resistance of ultra-high performance strain hardening cementitious composite: residual mechanical properties and spalling resistance10.1016/j.cemconcomp.2018.02.014 ↗
20. Characterization of high strength mortars with nano alumina at elevated temperatures10.1016/j.cemconres.2013.08.003 ↗
21. The influence of nanomaterials on the thermal resistance of cement-based composites—a review10.3390/nano8070465 ↗
22. Multiscale carbon nanosphere–carbon fiber reinforcement for cement-based composites with enhanced high-temperature resistance10.1007/s10853-014-8655-8 ↗
23. Effects of slag and cooling method on the progressive deterioration of concrete after exposure to elevated temperatures as in a fire event10.1617/s11527-010-9660-2 ↗
24. Study on high-performance concrete at high temperatures in China (2004–2016) - an updated overview10.1016/j.firesaf.2017.10.007 ↗
25. Effects of re-curing on residual mechanical properties of concrete after high temperature exposure10.1016/j.conbuildmat.2017.11.005 ↗
26. Flexural behavior of fiber and nanoparticle reinforced concrete at high temperatures10.1002/fam.2526 ↗
27. Effect of macro-, micro- and nano-calcium carbonate on properties of cementitious composites—a review10.3390/ma12050781 ↗
28. Recent advances in understanding the role of supplementary cementitious materials in concrete10.1016/j.cemconres.2015.03.018 ↗
29. Impact of high temperature on PFA concrete10.1016/S0008-8846(01)00513-0 ↗
30. Self-healing ability of fly ash–cement systems10.1016/j.cemconcomp.2008.12.009 ↗
31. Self-healing capability of cementitious composites incorporating different supplementary cementitious materials10.1016/j.cemconcomp.2012.08.013 ↗
32. Effects of different nanomaterials on hardening and performance of ultra-high strength concrete (UHSC)10.1016/j.cemconcomp.2016.03.003 ↗
33. Dehydration and rehydration processes of cement paste exposed to high temperature environments10.1023/B:JMSC.0000025827.65956.18 ↗
34. Effects of re-curing on microstructure of concrete after high temperature exposure10.1016/j.conbuildmat.2018.02.122 ↗
35. Thermal analysis and microstructure of Portland cement-fly ash-silica fume pastes10.1007/s10973-009-0403-y ↗
36. Thermal analysis of the 3CaO·Al2O3-CaSO4·2H2O-CaCO3-H2O system10.1016/0040-6031(86)85139-5 ↗
37. Natural 1.1 and 1.4 nm tobermorites from Fuka, Okayama, Japan10.1016/S0008-8846(03)00099-1 ↗
38. Thermogravimetry of ternary cement blends10.1007/s10973-013-3017-3 ↗
39. Studies on the carboaluminate formation in limestone filler-blended cements10.1016/S0008-8846(01)00491-4 ↗
40. Multi-scale investigation of the performance of limestone in concrete10.1016/j.conbuildmat.2014.10.042 ↗
41. Durdziński · 2016