Abstract The safety verification of glass structures is usually made on the basis of a deterministic approach, without assessing the underlying probability of collapse. In this article, we propose to use the semi- probabilistic method in the limit-state design of glass structures by presenting properly-calibrated values of the partial safety factors of material strength, so as to obtain a probability of failure compatible with the target values indicated for each class of consequence by Eurocode 1 (EN 1990). Starting from a micromechanically-motivated model of fracture propagation, typically used for brittle materials, experimental results conducted in a previous campaign have been interpreted using the Weibull statistical distribution, taking into account that size-effect, type of stress (e.g., uniaxial vs. bi-axial) and the insidious phenomenon of subcritical crack growth (static fatigue due to fracture growth in time without increase of load) can affect the probability of failure. Actions like wind, snow and live (anthropic) loads have been modeled using the statistical distributions recommended in international structural codes. Then, the probabilistic method of level III has been applied for the verification of paradigmatic case studies, which have served to calibrate the partial safety factors to be used in the semi-probabilistic approach. A novelty, to our knowledge, is the proposal of a multiplication coefficient for the partial safety factor of material strength, instead that for the factors of loads, to distinguish in the verification the different classes of consequences, each one characterized by the probability threshold of collapse. The results of this study will furnish the basis for the design of glass structures according to the general performance requirements established by EN 1990.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Structural Analysis of Composite Materials · Wind and Air Flow Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. ASTM. ASTM C 1368: Standard test method for determination of slow crack growth parameters of advanced ceramics by constant stress-rate flexural testing at ambient temperature. American Society Testing of Materials; 2001.
2. Weakest link theory reformulated for arbitrary fracture criterion10.1111/j.1151-2916.1978.tb09327.x ↗
3. Glass as a material
4. Progressive damage and fracture of laminated glass beams10.1016/j.conbuildmat.2009.09.007 ↗
5. Discrimination of multiaxiality criteria using brittle fracture loci10.1016/0955-2219(96)00055-6 ↗
6. CEN-TC129. EN 1288-2-2000: Glass in building – determination of the bending strength of glass – Part 2: Coaxial double ring test on flat specimens with large test surface areas. European Standard; 2000.
7. CEN-TC129. EN 1288-3-2000: Glass in building – determination of the bending strength of glass – Part 3: Test with specimen supported at two points (four point bending). European Standard; 2000.
8. CEN-TC129-WG8. PrEN-13474: Glass in building – determination of the strength of glass panes by calculation and testing. Project of European Standard (withdrawn); 2012.
9. CEN-TC129-WG8. EN-16612: Glass in building – determination of the load resistance of glass panes by calculation and testing. European Standard; 2013.
10. CEN-TC250. EN 1991-1-1: Eurocode 1 – actions on structures – Part 1-1: General actions – densities, self weight, imposed loads on buildings. European Harmonized Standard; 2002.
11. CEN-TC250. EN 1991-1-3: Eurocode 1 – actions on structures – Part 1-3: General actions – snow loads. European Harmonized Standard; 2003.
12. CEN-TC250. EN 1990: Eurocode 0 – basis of structural design. European Harmonized Standard; 2005.
13. CEN-TC250. EN 1991-1-4: Eurocode 1 – actions on structures – Part 1-4: General actions – wind actions. European Harmonized Standard; 2005.
14. Equivalence of physically based statistical fracture theories for reliable analysis of ceramics in multi-axial loading10.1111/j.1151-2916.1990.tb05245.x ↗
15. Slow crack growth of brittle materials with exponential crack velocity under cyclic fatigue loading10.1016/j.ijfatigue.2005.03.007 ↗
16. CNR, National Research Council. CNR-DT207: Istruzioni per la valutazione delle azioni e degli effetti del vento sulle costruzioni. Technical document; 2008.
17. CNR, National Research Council. CNR-DT210: Istruzioni per la progettazione, l’esecuzione ed il controllo di costruzioni con elementi strutturali di vetro. Technical document; 2013.
18. Collini L, Royer-Carfagni G. Flexural strength of glass-ceramic for structural applications. Eur J Ceram Soc; 2014 [in press].http://www.sciencedirect.com/science/article/pii/S095522191300495010.1016/j.jeurceramsoc.2013.10.032 ↗
19. Dall’Igna R, D’Este A, Silvestri M. Comments on test methods for determination of structural glass strength. In: Proceedings XXV ATIV Conference, Parma, Italy; 2010. p. 5–13.
20. Method of reproducibility predamaging float glass as a basis to determinate the bending strength
21. A method for evaluating the time-dependent failure characteristics of brittle materials and its application to polycrystalline alumina10.1007/BF00550196 ↗
22. A general approach for the statistical analysis of multiaxial fracture10.1111/j.1151-2916.1978.tb09314.x ↗
23. On the inconsistency of a formulation for the effective thickness of laminated glass, recently implemented by standards10.1016/j.compositesb.2013.05.025 ↗
24. Haldimann M. Fracture strength of structural glass elements – analytical and numerical modelling, testing and design. Thesis No. 3671, EPFL Lausanne, CH; 2006.
25. JCSS. Probabilistic model code Part 2: Load models. Joint Committee on Structural Safety (JCSS); 2001.
26. Madsen · 1985
27. M.I.T., Ministero Infrastrutture e Trasporti. Nuova Circolare delle norme tecniche per le costruzioni, Circolare 02/02/2009 No. 617; 2009.
28. Munz · 1999
29. Murakami · 1987
30. Porter MI, Houlsby GT. Development crack size and limit state design methods for edge abraded glass members. Report No. OUEL 2111/99, University of Oxford; 1999.
31. Fail-safe point fixing of structural glass. New advances10.1016/j.engstruct.2009.02.050 ↗
32. Sedlacek · 1999
33. Fracture velocity and fracture energy of glass in the fatigue range10.1111/j.1151-2916.1961.tb15341.x ↗
34. Crack velocity functions and thresholds in brittle solids
35. Fracture surface energy of glass10.1111/j.1151-2916.1969.tb13350.x ↗
36. Stress corrosion and static fatigue of glass10.1111/j.1151-2916.1970.tb15962.x ↗