Portland cement-blast furnace slag mortars activated using waterglass: – Part 1: Effect of slag replacement and alkali concentration

E. Acevedo-Martinez, L.Y. Gomez-Zamorano, J.I. Escalante-Garcia

Publisher page

Abstract

Abstract Mortars of PC replaced with 0% to100% blast furnace slag were activated by waterglass at 0–10 wt.% of Na 2 O, aiming to investigate the effect of the alkaline activation in reducing the low early strength observed in Portland cement–slag blends. For the activated blended mortars, increased %Na 2 O and slag contents favored strength; 80% slag showed favorable results with 6 and 10%Na 2 O, while 30–50% slag, the presence of the alkaline activator was unfavorable relative to the non-activated Portland cement and slag mortars. The microstructures showed denser matrices of hydration products as the amount of slag and alkali concentration were increased, corresponding to the strength observations.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Concrete and Cement Materials Research · Magnesium Oxide Properties and Applications · Innovative concrete reinforcement materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (44)

Show source-provided references
1. Field III FR, Clark JP, Ashby MF. Market Drivers for Materials and Process Development in the 21st Century. MRS Bulletin, September 2000, p. 716–25.10.1557/mrs2001.198 ↗
2. Environmental reforms of materials science education in the 21st century10.1016/S0254-0584(99)00106-6 ↗
3. Hydrothermal reactions of fly ash with Ca(OH)2 and CaSO4⋅H2O10.1016/S0008-8846(97)00116-6 ↗
4. Alkali-activation of fly/ash7slag cement, strength behaviour and hydration products10.1016/S0008-8846(00)00298-2 ↗
5. Lang E. Blast furnace Cements. In: Bensted J, Barnes P, editors. Structure and Performance of Cements, 2001, p. 310–26 [chapter 12].
6. High performance cementing materials from industrial slags – a review10.1016/S0921-3449(99)00060-9 ↗
7. Chandra · 1997
8. Siddique · 2008
9. Studies on the corrosion resistance of reinforced steel inconcrete with ground granulated blast-furnace slag—an overview10.1016/j.jhazmat.2006.07.022 ↗
10. Dubovoy VS, Gebler SH, Klieger P, Whiting DA. Effects of ground granulated blast furnace slag on some properties of pastes, mortars and concretes. Frohnsdorff, editor. Blended Cements, ASTM STP 897 American Society for Testing and Materials, Philadelphia, 1986. p. 29–48.10.1520/STP36390S ↗
11. Early strength development and hydration of alkali activated blast furnace slag 7fly ash blends10.1680/adcr.1999.11.4.189 ↗
12. Shi · 2007
13. Alkali-silicate admixture for cement composites incorporating pozzolan or blast furnace slag10.1016/0008-8846(93)90182-9 ↗
14. Regourd M, Slags and slags cements, concrete technology and design, vol. 3. Cement Replacement Materials. London: Surrey University Press; 1986.
15. Reactivityofblast-furnaceslagin Portland cement blends hydrated under different condition10.1016/S0008-8846(01)00587-7 ↗
16. Properties of concrete incorporating fly ash and ground granulatedblast-furnace slag10.1016/S0958-9465(02)00058-6 ↗
17. Comparison of different methods for activation of ordinary Portland cement–slag mortars10.1016/j.conbuildmat.2010.06.060 ↗
18. Reactivity of blast furnace slag in Portland cement blends hydrated under different conditions10.1016/S0008-8846(01)00587-7 ↗
19. Investigation of the hydration of Portland blast furnace slag cement: hydration kinetics10.1680/adcr.1989.2.5.9 ↗
20. Manufacture and characteristics of Portland blast furnace-slag cements
21. Hydration of mechanically activated granulated blast furnace slag10.1007/s11663-005-0089-x ↗
22. High performance cementing materials from industrial slags10.1016/S0921-3449(99)00060-9 ↗
23. Reactivity and mechanical properties of alkali activated blast furnace slag
24. Jiang W, Alkali activated cementitious materials: mechanisms, microstructure and properties. Ph.D. Thesis. The Pennsylvania State University, Pennsylvania, US; 1997.
25. Effect of sodium sulphate on the hydration of granulated blast furnace slag blended Portland cement
26. Early activation and properties of slag cement10.1016/0008-8846(90)90060-B ↗
27. Investigation of Portland slag cement activated by waterglass10.1016/S0008-8846(98)00069-6 ↗
28. Ghosh SN, Joshi DM, Chanda S, Vaishnav H. Studies on activation of slag cement. In: Proceedings of 10th ICCC Gotemborg Sweden, 1997, 3ii92. p. 4.
29. Marciano Jr. E, Battagin AF. The influence of alkali activator in the early hydration and performance of Portland blast furnace slag cement. In: Proceedings of 10th ICCC Gotemborg Sweden, 1997, 3ii103. p. 4.
30. Alkali activation of Australian slag cements10.1016/S0008-8846(98)00170-7 ↗
31. The effect of chemical activators on early strength of ordinary Portland cement–slag mortars10.1016/j.conbuildmat.2010.04.006 ↗
32. Larosa-thompson J, Gill P, Scheetz BE, Silsbee MR. Sodium silicate applications for cement and concrete. In: Tenth ICCC Gotemborg Sweden, 1997, 3ii024. p. 8.
33. Statistical analysis of strength development as a function of various parameters on activated metakaolin/slag cements10.1111/j.1551-2916.2009.03414.x ↗
34. Strength, pore structure and permeability of alkali-activated slag mortars10.1016/S0008-8846(96)00174-3 ↗
35. Technology of Monolithic Refractories. Plibrico Japan; 1984. p. 115–23.
36. Characteristics of a NaOH activated blast furnace slag blended with a fine particle silica waste
37. The microstructure and mechanical properties of blended cements hydrated at various temperatures10.1016/S0008-8846(01)00471-9 ↗
38. Effect of temperature on the hydration of the main clínker phases in Portland cement: Part II, blended cements10.1016/S0008-8846(98)00107-0 ↗
39. Coarse blast furnace slag as a cementitious material, comparative study as a partial replacement of Portland cement and as an alkali activated cement10.1016/j.conbuildmat.2009.02.002 ↗
40. Soroka I, Portland Cement Paste and Concrete. Macmillan; 1979.10.1007/978-1-349-03994-4 ↗
41. Nonevaporable water from neat OPC and replacement materials in composite cements hydrated at different temperatures10.1016/S0008-8846(03)00208-4 ↗
42. Pore solution of alkali activated grond granulated blast furnace slag10.1016/S0008-8846(98)00212-9 ↗
43. Investigation on some factors affecting the characteristics of alkali–phosphorous slag cement10.1016/0008-8846(89)90004-5 ↗
44. Sodium silicate-based alkali activated slag mortars. Part1: strength, hydration and microstructure10.1016/S0008-8846(02)00717-2 ↗