Effect of LiAl-layered double hydroxides on hydration of calcium sulfoaluminate cement at low temperature
Source abstract
Abstract
Abstract To reveal the effect of LiAl-layered double hydroxides (LiAl-LDHs) on hydration of calcium sulfoaluminate cement at low temperature, pastes with and without it were prepared and cured at temperature −10 °C. Setting times and compressive strength of pastes were measured. Mercury intrusion porosimetry (MIP) was used to reveal the evolution of pastes microstructure. X-ray diffraction (XRD), Thermogravimetric analysis (TG) and 27Al nuclear magnetic resonance (NMR) were adopted to qualify and quantify the hydration productions. The results show that, LiAl-LDHs is an effective hydration accelerator of CSA cement at low temperature. Initial and final setting times are reduced linearly with the increase of LiAl-LDHs content. However, peak of compressive strength emerges at the content of 1.0%. At this content, modified paste achieves 5.5 times compressive strength of plain one at 1 day and 1.4 times at 28 days. In presence of LiAl-LDHs, more ettringite crystallizes in modified pastes up to 28 days. Denser pastes obtained thereby.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete and Cement Materials Research · Magnesium Oxide Properties and Applications · Layered Double Hydroxides Synthesis and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. Cement production globally and in the U.S. from 2010 to 2018. https://www.statista.com/statistics/219343/cement-production-worldwide/ (03.28.2019 last accessed)
2. Factors affecting early-age hydration of ordinary portland cement studied by NMR10.1007/s00723-007-0019-y ↗
3. Kinetic and thermodynamic modeling of Portland cement hydration at low temperatures10.1007/s11696-016-0007-5 ↗
4. Effect of the hydration temperature on the microstructure of Class G cement: C-S-H composition and density10.1016/j.cemconres.2017.02.008 ↗
5. Effect of the hydration temperature on the pore structure of cement paste: experimental investigation and micromechanical modelling10.1016/j.cemconres.2018.06.014 ↗
6. Behavior of fresh and hardened concretes with antifreeze admixtures in deep-freeze low temperatures and exterior winter conditions10.1016/j.conbuildmat.2014.12.011 ↗
7. The effects of low temperature curing on the compressive strength of ordinary and high performance concrete10.1016/j.conbuildmat.2004.04.033 ↗
8. Effect of temperature on the hydration of Portland cement blended with siliceous fly ash10.1016/j.cemconres.2013.07.006 ↗
9. Effect of temperature on the microstructure of calcium silicate hydrate (C-S-H)10.1016/j.cemconres.2013.06.008 ↗
10. Effect of temperature and age on the relationship between dynamic and static elastic modulus of concrete10.1016/j.cemconres.2003.12.011 ↗
11. Effect of curing temperature and glass type on the pozzolanic reactivity of glass powder10.1016/j.cemconres.2014.01.015 ↗
12. Effect of pozzolans on the hydration process of Portland cement cured at low temperatures10.1016/j.cemconcomp.2013.05.007 ↗
13. Long term effect of silica fume on the principle properties of low temperature cured ceramics10.1016/S0008-8846(97)00147-6 ↗
14. Effect of low temperature on hydration performance of the complex binder of silica fume-portland cement10.1007/s11595-014-0870-2 ↗
15. Influence of curing temperatures on the hydration of calcium aluminate cement/Portland cement/calcium sulfate blends10.1016/j.cemconcomp.2017.03.016 ↗
16. Low-temperature curing strength enhancement in cement-based materials containing limestone powder10.1617/s11527-017-1042-6 ↗
17. Preparation, properties and hydration process of low temperature nano-composite cement slurry10.1016/j.conbuildmat.2019.02.049 ↗
18. Effect of colloidal nanosilica on early-age compressive strength of oil well cement stone at low temperature10.1016/j.conbuildmat.2018.03.220 ↗
19. Influence of curing temperature on the process of hydration of supersulfated cements at early age10.1016/j.cemconres.2015.07.002 ↗
20. Hydration evolution and compressive strength of calcium sulphoaluminate cement constantly cured over the temperature range of 0 to 80 °C10.1016/j.cemconres.2017.05.025 ↗
21. Experimental study of calcium sulfoaluminate cement-based self-leveling compound exposed to various temperatures and moisture conditions: hydration mechanism and mortar properties10.1016/j.cemconres.2018.03.012 ↗
22. Influence of LiAl-layered double hydroxides with 3D micro-nano structures on the properties of calcium sulphoaluminate cement clinker10.1016/j.cemconcomp.2016.03.009 ↗
23. Calcium sulfoaluminate (Ye'elimite) hydration in the presence of gypsum, calcite, and vaterite10.1016/j.cemconres.2014.07.004 ↗
24. Early hydration of calcium sulfoaluminate cement through electrical resistivity measurement and microstructure investigations10.1016/j.conbuildmat.2010.09.042 ↗
25. Effects of lithium carbonate on performances of sulphoaluminate cement-based dual liquid high water material and its mechanisms10.1016/j.conbuildmat.2017.11.130 ↗
26. Hydration stage identification and phase transformation of calcium sulfoaluminate cement at early age10.1016/j.conbuildmat.2014.11.006 ↗
27. Retardation effect of elevated temperature on the setting of calcium sulfoaluminate cement clinker10.1016/j.conbuildmat.2018.05.061 ↗
28. Using gypsum to control hydration kinetics of CSA cements10.1016/j.conbuildmat.2017.07.217 ↗
29. Influence of superfine ettringite on the properties of sulphoaluminate cement-based grouting materials10.1016/j.conbuildmat.2018.02.013 ↗
30. Effects of limestone powder on the hydration and microstructure development of calcium sulphoaluminate cement under long-term curing10.1016/j.conbuildmat.2018.12.054 ↗
31. Hydration products in sulfoaluminate cements: evaluation of amorphous phases by XRD/solid-state NMR10.1016/j.cemconres.2016.05.014 ↗
32. Microstructural evolution of aluminum hydroxide gel during the hydration of calcium sulfoaluminate under different alkali concentrations10.1016/j.conbuildmat.2018.06.010 ↗
33. AH3 phase in the hydration product system of AFt-AFm-AH 3 in calcium sulfoaluminate cements: a microstructural study10.1016/j.conbuildmat.2018.02.052 ↗
34. Improvement of workability and early strength of calcium sulphoaluminate cement at various temperature by chemical admixtures10.1016/j.conbuildmat.2017.11.076 ↗