Effect of glycerol introduced into PLA based composites on the UV weathering behavior
Source abstract
Abstract
Abstract Effect of accelerated weathering time and glycerol on the photodegradation behavior of starch/wood flour/PLA composites was studied. The decreased intensity of diffraction peaks characterized by XRD indicated that the crystal structure was damaged. The chemical structure changes characterized by FTIR showed the formation of carboxylic acid. The decreased extent of the C O absorbance intensity of the composite with 15% glycerol proved that glycerol had a stabilize effect on the UV durability of the composites. After weathering, the maximum decomposition temperature decreased prominently due to the chain cleavage. With the prolonged weathering time, the tensile and flexural strengths decreased gradually.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: biodegradable polymer synthesis and properties · Natural Fiber Reinforced Composites · Advanced Cellulose Research Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. Biodegradability studies of poly (butylenesuccinate)/organo-montmorillonite nanocomposites under controlled compost soil conditions: effects of clay loading and compatibiliser10.1016/j.polymdegradstab.2012.05.024 ↗
2. Bionanocomposite based on cellulose nanowhisker from oil palm biomass-filled poly (lactic acid)10.1016/j.polymertesting.2015.10.003 ↗
3. Quantitative evaluation of photodegradation and racemization of poly(l-lactic acid) under UV-C irradiation10.1016/j.polymdegradstab.2010.03.034 ↗
4. Polylactic acid (PLA) biocomposites reinforced with coir fibres: evaluation of mechanical performance and multifunctional properties10.1016/j.compositesa.2014.04.003 ↗
5. Evaluation of PLA-lignin bioplastics properties before and after accelerated weathering10.1016/j.compositesb.2014.10.006 ↗
6. Degradation of polylactide composites under UV irradiation at 254nm10.1016/j.jphotochem.2015.06.029 ↗
7. The influence of UV-C irradiation on the properties of thermoplastic starch and polycaprolactone biocomposite with sisal bleached fibers10.1016/j.polymdegradstab.2011.11.010 ↗
8. About the end life of novel aliphatic and aliphatic-aromatic (co)polyesters after UV-weathering: structure/degradability relationships10.1016/j.polymdegradstab.2013.03.030 ↗
9. Modelling of photodegradation effect on elastic-viscoplastic behaviour of amorphous polylactic acid films10.1016/j.jmps.2009.10.003 ↗
10. Accelerated weathering performance of polylactide and its montmorillonite nanocomposite10.1016/j.clay.2015.12.025 ↗
11. Photochemical reactivity of PLA at the vicinity of glass transition temperature. The photo-rheology method10.1016/j.eurpolymj.2016.06.016 ↗
12. Biodegradation of poly(l-lactide) (PLA) exposed to UV irradiation by a mesophilic bacterium10.1016/j.ibiod.2013.08.013 ↗
13. Consequences of accelerated weathering in polylactide nanocomposites reinforced with halloysite nanotubes10.1177/0021998315575038 ↗
14. Effect of TiO2-crystal forms on the photo-degradation of EVA/PLA blend under accelerated weather testing10.1007/s11664-016-4409-5 ↗
15. Influence of fiber modifications on PLA/fiber composites. Behavior to accelerated weathering10.1016/j.compositesb.2016.02.032 ↗
16. Stability of poly(l-lactide)/TiO2 nanocomposite thin films under UV irradiation at 254 nm10.1016/j.polymdegradstab.2013.01.003 ↗
17. Photodegradation of biodegradable polyesters: a comprehensive study on poly(l-lactide) and poly(ɛ-caprolactone)10.1016/j.polymdegradstab.2005.07.007 ↗
18. Photooxidation of polylactide/calcium sulphate composites10.1016/j.polymdegradstab.2010.12.023 ↗
19. Characterization of EVA/PLA blends when exposed to different environments10.1007/s10924-013-0614-y ↗
20. Poly (lactic acid)/titanium dioxide composites: preparation and performance under ultraviolet irradiation10.1016/j.polymdegradstab.2012.03.039 ↗
21. Influences of halloysite nanotubes on crystallisation behaviour of polylactide10.1179/1743289814Y.0000000116 ↗
22. Influence of keratin on polylactic acid/chitosan composite properties. Behavior upon accelerated weathering10.1021/ie400848t ↗
23. Influence of accelerated ageing on the physico-mechanical properties of alkali-treated industrial hemp fibre reinforced poly(lactic acid) (PLA) composites10.1016/j.polymdegradstab.2009.10.010 ↗
24. Degradation of poly(L-lactide) films under ultraviolet irradiation and water bath10.1080/03602559.2011.551970 ↗
25. Electrical, mechanical and thermal properties of aligned silver nanowire/polylactide nanocomposite films10.1016/j.compositesb.2016.06.044 ↗
26. Accelerated ageing of polylactide in aqueous environments: comparative study between distilled water and seawater10.1016/j.polymdegradstab.2014.01.020 ↗
27. Effect of lignin nanoparticles and masterbatch procedures on the final properties of glycidyl methacrylate-g-poly (lactic acid) films before and after accelerated UV weathering10.1016/j.indcrop.2015.09.057 ↗
28. Photodegradation of poly(L-lactic acid): effects of photosensitizer10.1002/mame.200500278 ↗
29. Hybrid clay mineral-carbon nanotube-PLA nanocomposite films. Preparation and photodegradation effect on their mechanical, thermal and electrical properties10.1016/j.clay.2012.11.004 ↗
30. Preparation, characterization and properties of PLA/TiO2 nanocomposites based on a novel vane extruder10.1039/C4RA14538K ↗
31. Biodegradable poly(L-lactic acid)/TiO2 nanocomposites: thermal properties and degradation10.1002/app.34729 ↗