Bonding performance of adhesive systems for cross-laminated timber treated with micronized copper azole type C (MCA-C)
Source abstract
Abstract
Abstract The feasibility of manufacturing cross-laminated timber (CLT) from southern yellow pine (United States grown) treated with micronized copper azole type C (MCA-C) preservative was evaluated. Lumber (2x6 visually graded no. 2 boards) was treated to two retention levels (1.0 and 2.4 kg/m3), planed to a thickness of 35 mm, and assembled along with an untreated control group using three adhesive systems following product specifications: melamine formaldehyde (MF), resorcinol formaldehyde (RF), and one-component polyurethane (PUR). Block shear and delamination tests were conducted to examine the bonding performance in accordance with ASTM D905 and ASTM D2559 Standards, respectively. One-way analysis of variance and Kruskal-Wallis H test were conducted to evaluate the effects of preservative retention and adhesive type on block shear strength (BSS) and wood failure percentage (WFP). Regardless of adhesive type, the 1.0 kg/m3 retention treatment significantly lowered BSS compared to the untreated control. CLT composed of the laminations treated at 2.4 kg/m3 maintained BSS when PUR and RF were used but not MF. The average WFP of each CLT configuration ranged from 89% to 99%. The untreated CLT specimens did not experience any delamination under accelerated weathering cycles. The delamination rates of the treated specimens assembled using MF and RF increased with the preservative retention level, while PUR provided delamination rates less than 1% to the laminations treated at both levels. These combined data suggest that, under the conditions tested, PUR provided overall better bonding performance than MF and RF for MCA-C treated wood.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Wood Treatment and Properties · Lignin and Wood Chemistry · Natural Fiber Reinforced Composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (56)
Show source-provided references
1. Cross laminated timber (CLT): overview and development10.1007/s00107-015-0999-5 ↗
2. Introduction to cross laminated timber
3. Durability of mass timber structures: a review of the biological risks10.22382/wfs-2018-045 ↗
4. Wood preservation for preventing biodeterioration of Cross Laminated Timber (CLT) panels assembled in tropical locations
5. A comprehensive review of copper-based wood preservatives
6. Using copper-tolerant fungi to biodegrade wood treated with copper-based preservatives10.1016/S0964-8305(99)00047-5 ↗
7. Copper-based wood preservative systems used for residential applications in north America and Europe10.1021/bk-2014-1158.ch012 ↗
8. American Wood Protection Association (AWPA) · 2018
9. Synchrotron based X-ray fluorescence microscopy confirms copper in the corrosion products of metals in contact with treated wood
10. Exposure testing of fasteners in preservative treated wood: gravimetric corrosion rates and corrosion product analyses10.1016/j.corsci.2010.08.014 ↗
11. Corrosion of metals in wood: Comparing the results of a rapid test method with long-term exposure tests across six wood treatments10.1016/j.corsci.2011.01.039 ↗
12. Trials on the efficacy of micronized copper in Australia
13. Mechanical interlocking of adhesive bonds to CCA-treated southern pine a scanning electron-microscopic study
14. Surface characterization of chromated copper arsenate (CCA)-treated red maple10.1163/156856198X00281 ↗
15. Wood adhesives and bonding theory
16. Adhesive bonding of wood treated with ACQ and copper azole preservatives
17. Strength and durability of phenol-resorcinol-formaldehyde bonds to CCA-treated radiata pine wood
18. Adhesive performance of woods treated with alternative preservatives10.1007/s00226-005-0036-7 ↗
19. Compatibility of nonacidic waterborne preservatives with phenol-formaldehyde adhesives
20. ASTM D905-08, Standard test method for strength properties of adhesive bonds in shear by compression loading., ASTM International, West Conshohocken, PA, 2013. doi:10.1520/D0905-08R13.10.1520/D0905-08R13 ↗
21. ASTM D2559-12ae1, Standard specification for adhesives for structural laminated wood products for use under exterior (wet use) exposure conditions, ASTM International, West Conshohocken, PA, 2016. doi:10.1520/D2559-12A.1.4.
22. NDS, NDS Supplement: Design Values for Wood Construction, American National Standards Institute/American Wood Council (ANSI/AWC), 2018.
23. AWPA P62-16, Standard for micronized copper azole type C (MCA-C), American Wood Protection Association, Birmingham, AL, 2018.
24. AWPA U1-18, Use Category System: User Specification for Treated Wood, American Wood Protection Association, Birmingham, AL, 2018.
25. AWPA A9-18, Standard Method for Analysis of Treated Wood and Treating Solutions by X-ray Spectroscopy, American Wood Protection Association, Birmingham, AL, 2018.
26. ASTM -16, Standard Test Methods for Direct Moisture Content Measurement of Wood and Wood-Based Materials, ASTM International, West Conshohocken, PA, 2016.
27. FPInnovations, CLT Handbook U.S. Edition, FPInnovations, pointe-Claire, 2013.
28. Hexion Inc., CascomelTM 4720 withWonderbondTM Hardener 5025A (Cold Set) – Product Bulletin, Columbus, OH, 2016.
29. Hexion Inc., CASCOPHEN® ADHESIVE SYSTEM G-1131 – Product Bulletin, Columbus, OH, 2015.
30. Purbond, PURBOND HB E452 Single-component polyurethane adhesive for the manufacture of engineered wood products, 2009.
31. Purbond, Application instructions: Bonding of SOUTHERN PINE wood with primer LOCTITE PR 3105 and PURBOND HB X adhesives, Sempach Station, Switzerland, 2017.
32. Block shear strength and delamination of cross-laminated timber fabricated with Japanese Larch10.15376/biores.11.4.10240-10250 ↗
33. Estimating shear properties of walnut wood: a combined experimental and theoretical approach10.1617/s11527-017-1119-2 ↗
34. Image J2: ImageJ for the next generation of scientific image data10.1186/s12859-017-1934-z ↗
35. ASTM D2395-17, Standard Test Methods for Density and Specific Gravity (Relative Density) of Wood and Wood-Based Materials, ASTM International, West Conshohocken, PA, 2017.
36. IBM Corp., IBM SPSS Statistics for Windows, Version 25.0, 2017.
37. Two samples
38. The evaluation of panel bond quality and durability of hem-fir cross-laminated timber (CLT)10.1007/s00107-017-1283-7 ↗
39. Shear strength and durability testing of adhesive bonds in cross-laminated timber10.1080/00218464.2015.1094391 ↗
40. J.E. Winandy, Effects of waterborne preservative treatment on mechanical properties: a review, in: Proc. 91st Annu. Meet. Am. Wood-Preservers’ Assoc., 1995: pp. 17–34.
41. H.M. Barnes, G.B. Lindsey, J. Hill, M. Pompeo, R. Hodge, Bending Properties of Southern Pine Treated with Micronized Preservative Systems, in: Proc. 39th Annu. Meet. Int. Res. Gr. Wood Prot., Istanbul, 2008: pp. 1–7.
42. Effects of the wood preservatives on mechanical properties of yellow pine (Pinus sylvestris L.) wood10.1016/j.buildenv.2004.01.032 ↗
43. C.R. Frihart, C.G. Hunt, Chapter 10: Adhesives with Wood Materials Bond Formation and Performance, in: Wood Handb. Wood as an Eng. Mater., FPL-GTR-19, U.S. Department of Agriculture, Forest Service, Forest Products Laboratory, Madison, WI, 2010: p. 508. doi:10.2737/FPL-GTR-190.10.2737/FPL-GTR-190 ↗
44. Enhanced adhesion of melamine-urea and melamine adhesvies to CCA-treated southern pine lumber
45. L. Jin, P. Walcheski, A. Preston, Laboratory studies on copper availability in wood treated with soluble amine copper and micronized copper systems, in: Proc. 39th Annu. Meet. Int. Res. Gr. Wood Prot., 2008: pp. 1–10.
46. Synthesis of epoxy-loaded poly(melamine-formaldehyde) microcapsules: effect of pH regulation method and emulsifier selection10.1016/j.colsurfa.2017.02.053 ↗
47. Evaluation of the effect of knots on rolling shear strength of cross laminated timber (CLT)10.1016/j.conbuildmat.2019.06.165 ↗
48. D.E. Kretschmann, Chapter 05: Mechanical Properties of Wood, in: Wood Handb. Wood as an Eng. Mater., FPL-GTR-19, U.S. Department of Agriculture, Forest Service, Forest Products Laboratory, Madison, WI, 2010: p. 508. doi:10.2737/FPL-GTR-190.10.2737/FPL-GTR-190 ↗
49. Effect of grain angle on shear strength of Douglas-fir wood10.1515/hf-2011-0031 ↗
50. S. V. Glass, S.L. Zelinka, Chapter 04: Moisture Relations and Physical Properties of Wood, in: Wood Handb. Wood as an Eng. Mater., FPL-GTR-19, U.S. Department of Agriculture, Forest Service, Forest Products Laboratory, Madison, WI, 2010: p. 508. doi:10.2737/FPL-GTR-190.10.2737/FPL-GTR-190 ↗
51. Adhesive penetration in wood – a review
52. Production of glued laminated timber with copper azole treated maritime pine10.1007/s00107-009-0373-6 ↗
53. Mechanical properties of adhesives for bonding wood-a review10.1016/j.ijadhadh.2013.03.013 ↗
54. Adhesive groups and how they relate to the durability of bonded wood10.1163/156856108X379137 ↗
55. Bonding quality of industrially produced cross-laminated timber (CLT) as determined in delamination tests10.1016/j.conbuildmat.2016.12.057 ↗
56. CEN, EN 16351 Timber Structures – Cross Laminted Timber – Requirements, European Committee for Standardization, Belgium, 2015.