The effects of air entrainment and pozzolans on frost resistance of 50–60 MPa grade concrete
Source abstract
Abstract
Abstract An experimental investigation was conducted using an air-entraining agent and pozzolans such as silica fume and fly ash, to meet the design strengths 50 and 60 MPa, as well as frost resistance to 300 cycles of freezing and thawing. Among a series of concretes of grade 50 or 60 MPa, only a small part could resist 300 cycles of freezing and thawing. It was demonstrated that frost resistance might be independent on strength of concrete. By means of mercury intrusion porosimeter, the pore structure characteristics of six concretes were identified. Air entrainment, no matter whether the pozzolans were used, caused an increase in cumulative pore volume, and also an increase in the mean pore size. It is revealed that, as to concrete at a 0.32 water/binder ratio, air entrainment should be a main approach to enhance frost resistance, although the pozzolans could be used to increase long-term strength of concrete.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete and Cement Materials Research · Concrete Properties and Behavior · Innovative concrete reinforcement materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (22)
Show source-provided references
1. Aitcin · 1998
2. Mehta · 1993
3. Feng · 1992
4. Frost resistance concrete10.1016/0950-0618(95)00067-4 ↗
5. Feng · 1996
6. Li JY. Durability design and construction of concrete structures in freezing and thawing environment [in Chinese]. In: Chen ZY, editor. Proceedings of the symposium on durability and design of concrete structures, Beijing (China); 2002, p. 108–18.
7. The durability characteristics of high performance concrete: a review10.1016/S0958-9465(02)00081-1 ↗
8. High strength concrete without air entrainment: Effect of rapid temperature cycling above and below 0°C
9. Pigeon · 1995 · vol. 4
10. Theoretical investigation on frost resistance of high performance concrete [in Chinese]
11. Internal frost resistance and salt frost scaling of self-compacting concrete10.1016/S0008-8846(02)00968-7 ↗
12. Impact of BS EN 450 PFA on concrete construction in the UK10.1016/S0950-0618(97)00029-9 ↗
13. Frost resistance of high-performance concrete
14. Modification of the properties of concrete by a new pozzolan – a waste catalyst from the catalytic process in a fluidized bed10.1016/S0008-8846(01)00646-9 ↗
15. An explanation for the unsaturated state of water stored concrete10.1016/S0958-9465(02)00124-5 ↗
16. Experimental identification of ice formation in small concrete pores10.1016/j.cemconres.2004.01.022 ↗
17. Durability of Portland blast-furnace slag cement concrete10.1016/S0958-9465(98)00032-8 ↗
18. Investigation of micro-cracks and microstructure of high performance lightweight aggregate concrete10.1016/S0360-1323(01)00051-8 ↗
19. Mechanical properties and frost resistance of silica fume concrete10.1016/S0958-9465(97)00020-6 ↗
20. Aggregate–cement paste transition zone properties affecting the salt–frost damage of high-performance concretes10.1016/j.cemconres.2004.06.009 ↗
21. Chinese Standard GBJ 82–85. Test methods for determination of long-term properties and durability of normal concrete [in Chinese], Beijing (China), 1986.
22. Bruno V, Chabannet M, Ambroise J, Pera J. Betons tres hautes performances (B.T.H.P.): microfissuration et durabilite. In: Malhotra VM, editor. Proceedings of the second CANMET/ACI international conference of concrete durability, Montreal, Canada; 1991, p. 175–94.