Early-age deformation and autogenous cracking risk of slag–limestone filler-cement blended binders
Source abstract
Abstract
This article presents an experimental comparative study of the early-age behavior of binary and ternary cementitious matrices, combining Portland cement (PC), ground granulated blast furnace slag (BFS) and limestone filler (LF). The objective of this work was to quantify the influence of the composition of various blended binders on their physico-chemical evolution and early-age autogenous cracking risk. For this purpose, measurements of the rate of reactions, chemical shrinkage, autogenous shrinkage in free and restrained conditions and mechanical performances were performed on 12 binders prepared with the same water-to-cementitious materials ratio (w/cm = 0.32) and various dosages of PC, BFS and LF. The result analysis showed that the dilution effect reduced the early-age chemical shrinkage while the filler effect and the slag reactions tended to accelerate its development after a few hours of hydration. The substitution of PC with BFS and LF also led to both refining the 28-days pore size distribution measured by mercury intrusion and increasing the magnitude of early-age free autogenous shrinkage. However, in spite of their higher autogenous shrinkage potential, the binary and ternary binders very often exhibited later autogenous cracking ages than the control Portland cement paste.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete and Cement Materials Research · Concrete Properties and Behavior · Innovative concrete reinforcement materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (55)
Show source-provided references
1. Prediction of compressive strengths of mortars made with portland cement-blast furnace slag-fly ash blends10.1016/0008-8846(91)90102-N ↗
2. On predicting compressive strengths of mortars with ternary blends of cement, GGBFS and fly ash10.1016/S0008-8846(97)00039-2 ↗
3. Strength and pore structure of ternary blended cement mortars containing blast furnace slag and silica fume10.1016/S0008-8846(98)00078-7 ↗
4. Preventive measures for alkali-silica reactions (binary and ternary systems)10.1016/S0008-8846(98)00242-7 ↗
5. Use of ternary cementitious systems containing silica fume and fly ash in concrete10.1016/S0008-8846(99)00096-4 ↗
6. Porosity and strength of PFA/SF/OPC ternary blended paste10.1016/S0008-8846(00)00307-0 ↗
7. Ternary and quaternary cements for sustainable development
8. Mechanical behaviour of various mortars made by combined fly ash and limestone in Moroccan Portland cement10.1016/S0008-8846(02)00834-7 ↗
9. Optimization of ternary cementitious mortar blends using factorial experimental plans10.1007/BF02483137 ↗
10. Use of ternary blends containing silica fume and fly ash to suppress expansion due to alkali–silica reaction in concrete10.1016/S0008-8846(01)00680-9 ↗
11. Prediction of compressive strength and optimization of mixture proportioning in ternary cementitious systems10.1007/BF02481065 ↗
12. Strength development of ternary blended cement with limestone filler and blast-furnace slag10.1016/S0958-9465(01)00056-7 ↗
13. Studies on high-performance blended/multiblended cements and their durability characteristics10.1016/S0008-8846(03)00091-7 ↗
14. Strength optimization of “tailor-made cement” with limestone filler and blast furnace slag10.1016/j.cemconres.2004.09.023 ↗
15. Improving the performance of ternary blended cements by mixing different types of fly ashes10.1016/j.cemconres.2007.02.017 ↗
16. Synergistic action of a ternary system of Portland cement – limestone – silica fume in concrete
17. Properties of self-compacting mortars with binary and ternary cementitious blends of fly ash and metakaolin10.1617/s11527-007-9345-7 ↗
18. Use of binary and ternary blends in high strength concrete10.1016/j.conbuildmat.2007.03.026 ↗
19. Properties of self-compacting concretes made with binary, ternary, and quaternary cementitious blends of fly ash, blast furnace slag, and silica fume10.1016/j.conbuildmat.2008.09.015 ↗
20. Assessment of binary and ternary blends of metakaolin and class C fly ash for alkali-silica reaction mitigation in concrete10.1016/j.cemconres.2010.08.006 ↗
21. Improvement of the early-age reactivity of fly ash and blast furnace slag cementitious systems using limestone filler10.1617/s11527-010-9637-1 ↗
22. Synergy between fly ash and limestone powder in ternary cements10.1016/j.cemconcomp.2010.09.006 ↗
23. Hydration mechanisms of ternary Portland cements containing limestone powder and fly ash10.1016/j.cemconres.2010.11.014 ↗
24. Investigation into the synergistic effects in ternary cementitious systems containing portland cement, fly ash and silica fume10.1016/j.cemconcomp.2011.11.014 ↗
25. Fine limestone additions to regulate setting in high volume fly ash mixtures10.1016/j.cemconcomp.2011.09.004 ↗
26. Mechanical and durability properties of ternary concretes containing silica fume and low reactivity blast furnace slag10.1016/j.cemconcomp.2012.01.007 ↗
27. Reducing the environmental impact of concrete
28. Reducing CO2 emissions
29. Sustainable development and climate change initiatives10.1016/j.cemconres.2007.09.008 ↗
30. Strengthening effects of finely ground fly ash, granulated blast furnace slag, and their combination10.1016/S0008-8846(98)00158-6 ↗
31. Gurney L, Bentz DP, Sato T, Weiss WJ. Reducing Set Retardation in High Volume Fly Ash Mixtures with the Use of Limestone: improving constructability for sustainability, Journal of the Transportation Research Board, No. 2290, Concrete Materials, 2012;139–146.
32. Effect of supplementary cementitious materials on shrinkage and crack development in concrete10.1016/j.cemconcomp.2006.10.003 ↗
33. NF EN 197-1. Cement – Part 1: composition, specifications and conformity criteria for common cements; 2001.
34. Chemical shrinkage of cement pastes and mortars at very early age: effect of limestone filler and granular inclusions10.1016/j.cemconcomp.2007.06.004 ↗
35. NF P 15-433. Methods of testing cement – determination of shrinkage and swelling; 1994.
36. Early-age autogenous cracking of cementitious matrices: physico-chemical analysis and micro/macro investigations10.1617/s11527-010-9663-z ↗
37. Taylor · 1990
38. Hydration, setting and hardening of Portland cement
39. Heat of hydration models for cementitious materials
40. The effects of supplementary cementing materials in modifying the heat of hydration of concrete10.1617/s11527-008-9425-3 ↗
41. Mercury porosimetry – an inappropriate method for the measurement of pore size distributions in cement-based materials10.1016/S0008-8846(00)00370-7 ↗
42. Autogenous deformations of cement pastes – Part II: W/C effects, micro-macro correlations, and threshold values10.1016/j.cemconres.2004.10.020 ↗
43. Modeling of early age behavior of blast furnace slag concrete based on micro-physical properties10.1016/j.cemconres.2011.06.005 ↗
44. The hydration of slag, Part 2: reaction models for blended cement10.1007/s10853-006-0874-1 ↗
45. Influence of limestone on the hydration of Portland cements10.1016/j.cemconres.2008.01.002 ↗
46. Predicting Ca(OH)2 content and chemical shrinkage of hydrating cement pastes using analytical approach10.1016/j.cemconres.2003.07.006 ↗
47. Siddique · 2008
48. Influence of cement and admixture on autogenous shrinkage of cement paste10.1016/0008-8846(95)00010-0 ↗
49. Autogenous shrinkage of ground-granulated blast-furnace slag concrete
50. Effect of curing temperature and type of cement on early-age shrinkage of high-performance concrete10.1016/S0008-8846(01)00601-9 ↗
51. Autogenous relative humidity change and autogenous shrinkage of high performance cement pastes10.1016/j.cemconres.2004.06.028 ↗
52. Autogenous shrinkage of concrete containing granulated blast-furnace slag10.1016/j.cemconres.2006.01.005 ↗
53. Zhou J, Ye G, Schlangen E, van Breugel K. Autogenous deformation of Portland cement paste blended with blast furnace slag measured by mini-TSTM. In: Jensen OM, Lura P, Kovler K, editors. Proceedings of the International RILEM Conference on Volume Changes of Hardening Concrete: Testing and Mitigation; 2006. p. 367-374.10.1617/2351580052.039 ↗
54. Effect of autogenous deformation on the cracking risk of slag cement concretes10.1016/j.cemconcomp.2010.12.003 ↗
55. Assessing residual stress development and stress relaxation in restrained concrete ring specimens10.1016/S0958-9465(03)00069-6 ↗