Effects of calcined dolomite addition on reaction kinetics of one-part sodium carbonate-activated slag cements
Source abstract
Abstract
Abstract In the present study, an environment-friendly one-part alkali-activated cement dry mixture was prepared by using blast furnace slag as the aluminosilicate precursor, solid sodium carbonate as the alkali activator and calcined dolomite (CD) as the reaction kinetics controlling additive. The effects of CD addition on the reaction kinetics and phase evolution of the hydrated cement paste were investigated by using the isothermal conduction calorimetry (ICC), X-ray diffractometry (XRD), thermogravimetric analysis (TGA) and nitrogen adsorption technique. The CD addition promoted the formation of hydrotalcite-like phase in the paste to consume the excess CO32− ions. This is helpful in raising the alkalinity of the pore solution, and consequently enhancing the rate and degree of the alkali-activation. The growth of space-filling C-A-S-H gel phase leads to a more compact pore structure in the paste with higher CD content. The CD addition enables the Na2CO3-activated slag paste to set within 24 h, and improves the compressive strength to an acceptable value of 32.9–41.6 MPa after 28 days of curing at ambient temperature.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete and Cement Materials Research · Magnesium Oxide Properties and Applications · Innovative concrete reinforcement materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (58)
Show source-provided references
1. Geopolymer technology: the current state of the art10.1007/s10853-006-0637-z ↗
2. Durability of alkali-activated materials: progress and perspectives10.1111/jace.12831 ↗
3. An overview of geopolymers derived from industrial by-products10.1016/j.conbuildmat.2016.09.136 ↗
4. Designing precursors for geopolymer cements10.1111/j.1551-2916.2008.02787.x ↗
5. Influence of activator type on hydration kinetics, hydrate assemblage and microstructural development of alkali activated blast-furnace slags10.1016/j.cemconres.2010.11.016 ↗
6. One-part alkali-activated materials: a review10.1016/j.cemconres.2017.10.001 ↗
7. Costs and carbon emissions for geopolymer pastes in comparison to ordinary portland cement10.1016/j.jclepro.2011.02.010 ↗
8. Effect of fly ash microsphere on the rheology and microstructure of alkali-activated fly ash/slag pastes10.1016/j.cemconres.2018.04.008 ↗
9. Cost-efficient one-part alkali-activated mortars with low global warming potential for floor heating systems applications10.1080/19648189.2015.1125392 ↗
10. Synthesizing one-part geopolymers from rice husk ash10.1016/j.conbuildmat.2016.08.017 ↗
11. Pore characteristics in one-part mix geopolymers foamed by H2O2: the impact of mix design10.1016/j.matdes.2017.05.084 ↗
12. One-part geopolymer mixes from geothermal silica and sodium aluminate10.1021/ie8006825 ↗
13. Degree of reaction and phase content of silica-based one-part geopolymers investigated using chemical and NMR spectroscopic methods10.1007/s10853-015-9232-5 ↗
14. Micromechanics-based investigation of a sustainable ambient temperature cured one-part strain hardening geopolymer composite10.1016/j.conbuildmat.2016.11.117 ↗
15. Effects of alkali on one-part alkali-activated cement synthesized by calcining bentonite with dolomite and Na2CO310.1016/j.clay.2017.01.020 ↗
16. One-part geopolymers based on thermally treated red mud/NaOH blends10.1111/jace.13231 ↗
17. Synthesis, characterization and mechanisms of one-part geopolymeric cement by calcining low-quality kaolin with alkali10.1617/s11527-014-0350-3 ↗
18. Thermal activation of albite for the synthesis of one-part mix geopolymers10.1111/j.1551-2916.2011.04925.x ↗
19. Synthesis of heat and ambient cured one-part geopolymer mixes with different grades of sodium silicate10.1016/j.ceramint.2014.12.154 ↗
20. Fly ash-based geopolymers: the relationship between composition, pore structure and efflorescence10.1016/j.cemconres.2014.06.004 ↗
21. Compressive strength development and shrinkage of alkali-activated fly ash-slag blends associated with efflorescence10.1617/s11527-015-0694-3 ↗
22. Nomenclature of the hydrotalcite supergroup: natural layered double hydroxides10.1180/minmag.2012.076.5.10 ↗
23. Role of carbonates in the chemical evolution of sodium carbonate-activated slag binders10.1617/s11527-014-0412-6 ↗
24. Development of greener alkali-activated cement: utilisation of sodium carbonate for activating slag and fly ash mixtures10.1016/j.jclepro.2015.12.010 ↗
25. Setting of alkali-activated slag cement. Influence of activator nature10.1680/adcr.2001.13.3.115 ↗
26. Effect of activator mix on the hydration and strength behaviour of alkali-activated slag cements10.1680/adcr.2003.15.3.129 ↗
27. Evolution of binder structure in sodium silicate-activated slag-metakaolin blends10.1016/j.cemconcomp.2010.09.004 ↗
28. Characterization of aged slag concretes
29. Isothermal calorimetry and in-situ XRD study of the NaOH activated fly ash, metakaolin and slag10.1016/j.cemconres.2017.10.004 ↗
30. Structure and strength of NaOH activated concretes containing fly ash or GGBFS as the sole binder10.1016/j.cemconcomp.2010.03.007 ↗
31. Controlling the reaction kinetics of sodium carbonate-activated slag cements using calcined layered double hydroxides10.1016/j.cemconres.2015.11.012 ↗
32. MgO content of slag controls phase evolution and structural changes induced by accelerated carbonation in alkali-activated binders10.1016/j.cemconres.2013.12.003 ↗
33. Characterisation of reactive magnesia and sodium carbonate-activated fly ash/slag paste blends10.1016/j.conbuildmat.2015.06.015 ↗
34. Limitations of the hydrotalcite formation in Portland composite cement pastes containing dolomite and metakaolin10.1016/j.cemconres.2017.11.007 ↗
35. Understanding the hydration of dolomite in cementitious systems with reactive aluminosilicates such as calcined clay10.1016/j.cemconres.2018.03.010 ↗
36. Kinetics of thermal decomposition of dolomite10.1023/A:1010174726982 ↗
37. Mechanical properties and microstructural analysis of slag based cementitious binder with calcined dolomite as an activator10.1016/j.conbuildmat.2017.05.221 ↗
38. Activation of ground granulated blast furnace slag by using calcined dolomite10.1016/j.conbuildmat.2014.06.044 ↗
39. Compressive strength of one-part alkali activated fly ash using red mud as alkali supplier10.1016/j.conbuildmat.2016.08.015 ↗
40. ASTM C191-08, Standard Test Methods for Time of Setting of Hydraulic Cement by Vicat Needle, (2008).
41. Effect of silicate modulus and metakaolin incorporation on the carbonation of alkali silicate-activated slags10.1016/j.cemconres.2010.02.003 ↗
42. Effects of slag on reaction and composition of alkali-activated fly ash-slag blends
43. Influence of activator on the strength and drying shrinkage of alkali-activated slag mortar10.1016/j.conbuildmat.2007.10.011 ↗
44. Quantitative kinetic and structural analysis of geopolymers. Part 1. The activation of metakaolin with sodium hydroxide10.1016/j.tca.2013.01.040 ↗
45. Accelerated carbonation testing of alkali-activated binders significantly underestimates service life: the role of pore solution chemistry10.1016/j.cemconres.2012.07.002 ↗
46. Structure of calcium silicate hydrates formed in alkaline-activated slag: influence of the type of alkaline activator10.1111/j.1151-2916.2003.tb03481.x ↗
47. Gel nanostructure in alkali-activated binders based on slag and fly ash, and effects of accelerated carbonation10.1016/j.cemconres.2013.06.007 ↗
48. Compositional, microstructural and mechanical properties of ambient condition cured alkali-activated cement10.1016/j.conbuildmat.2016.03.043 ↗
49. Physical evolution of Na-geopolymer derived from metakaolin up to 1000 °C10.1007/s10853-006-0535-4 ↗
50. Effect of elevated temperature on alkali-activated geopolymeric binders compared to Portland cement-based binders10.1016/j.cemconres.2016.09.013 ↗
51. The thermal decomposition ofhuntite andhydromagnesite —a review10.1016/j.tca.2010.06.012 ↗
52. The pore structure and permeability of alkali activated fly ash10.1016/j.fuel.2012.05.034 ↗
53. Structural reorganization of class F fly ash in alkaline silicate solutions10.1016/S0927-7757(02)00237-6 ↗
54. The role played by the reactive alumina content in the alkaline activation of fly ashes10.1016/j.micromeso.2005.11.015 ↗
55. Quantitative kinetic and structural analysis of geopolymers. Part 2. The activation of sodium silicate activation of metakaolin10.1016/j.tca.2012.03.021 ↗
56. Modification of phase evolution in alkali-activated blast furnace slag by the incorporation of fly ash10.1016/j.cemconcomp.2013.09.006 ↗
57. Chloride-binding capacity of hydrotalcite in cement pastes containing dolomite and metakaolin10.1016/j.cemconres.2018.02.002 ↗
58. Stability of the hydrate phase assemblage in Portland composite cements containing dolomite and metakaolin after leaching, carbonation, and chloride exposure10.1016/j.cemconcomp.2018.02.013 ↗