Gainful utilization of waste glass for production of sulphuric acid resistance concrete
Source abstract
Abstract
Abstract Waste glass aggregates produced from mixed coloured beverage bottles was utilized in concrete. The present work inspects the performance of concrete with waste glass at different replacement stages (18%, 19%, 20%, 21%, 22%, 23% and 24%) when subjected to acidic (sulphuric acid) atmosphere. Performance of concrete was evaluated by determining transformation in mass, compressive strength and micro-structure. Beverage bottles being made of soda lime was found to be sacrificial in nature when the concrete samples were exposed to acidic environment and thus protected the strength giving products of cement hydration from damage. This was proved by the findings shown in the results of compressive strength examination when the samples were subjected to the exposure conditions. Micro-structural study which was executed to confirm the outcomes of hardened properties by conducting X-ray diffraction, Fourier transform infrared spectroscopy, thermo-gravimetric analysis and field emission scanning electron microscopy tests showed the hydration products were relatively less damaged in the presence of waste glass. The positive result of using waste glass was effective only up to a substitution level of 21%. Increased porosity due to higher incorporation of waste glass, greater than 21% led to the fall in performance of initial mechanical properties. However, the acid resistance of the concrete mixes with a maximum amount of waste glass (24%) is higher by 54% in terms of compressive strength at the end of 90 days exposure period. It is concluded that the best optimized performance in terms of compressive strength and acid resistance can be obtained at 21% substitution level.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete and Cement Materials Research · Recycling and utilization of industrial and municipal waste in materials production · Recycled Aggregate Concrete Performance
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. Evaluation of mechanical and durability properties of crumb rubber concrete10.1016/j.conbuildmat.2017.08.131 ↗
2. Sustainable production of concrete containing discarded beverage glass as fine aggregate10.1016/j.conbuildmat.2018.05.119 ↗
3. Magnetic properties of magnetite-based nano-glass-ceramics obtained from a Fe-rich scale and borosilicate glass wastes
4. Porous glass-ceramics from alkali activation and sinter-crystallization of mixtures of waste glass and residues from plasma processing of municipal solid waste10.1016/j.jclepro.2018.03.167 ↗
5. Assessment of solar panel waste glass in the manufacture of sepiolite based clay bricks10.1016/j.matlet.2018.02.049 ↗
6. Addition of waste glass for improving the immobilization of heavy metals during the use of electroplating sludge in the production of clay bricks10.1016/j.conbuildmat.2017.12.177 ↗
7. Extensive reuse of soda-lime waste glass in fly ash-based geopolymers10.1016/j.conbuildmat.2018.08.096 ↗
8. Use of selected waste materials in concrete mixes10.1016/j.wasman.2006.07.026 ↗
9. Concrete with recycled glass as fine aggregates
10. Properties of glass concrete reinforced with short basalt fibre10.1016/j.matdes.2012.05.062 ↗
11. Properties of concrete contains mixed colour waste recycled glass as sand and cement replacement10.1016/j.conbuildmat.2007.01.019 ↗
12. Recycling of WG as a partial replacement for fine aggregate in concrete10.1016/j.wasman.2008.08.012 ↗
13. Evaluation of the durability of concrete made with crushed glass aggregates10.1016/j.jclepro.2012.09.021 ↗
14. Decreasing concrete sewer pipe degradation using admixtures
15. Acid attack of cement-based materials—a review. Part 1 principle of acid attack10.1016/S0950-0618(01)00012-5 ↗
16. Chemical, microbiological, and in situ test methods for biogenic sulfuric acid corrosion of concrete10.1016/S0008-8846(00)00219-2 ↗
17. Chemical and microbiological tests to simulate sulfuric acid corrosion of polymer-modified concrete10.1016/S0008-8846(01)00565-8 ↗
18. Effect of limestone filler on the deterioration of mortars and pastes exposed to sulfate solutions at ambient temperature10.1016/j.cemconres.2007.08.003 ↗
19. D. Planel, Les effets couplés de la précipitation d’espèces secondaires sur le comportement mécanique et la dégradation chimique des bétons. PhD thesis, Univ. Marne-la-Vallée, France; (2002) [in French].
20. Mechanism of sulfate attack: a fresh look. Part 1: summary of experimental results10.1016/S0008-8846(02)00724-X ↗
21. Physical and microstructural aspects of sulfate attack on ordinary and limestone blended Portland cements10.1016/j.cemconres.2009.08.005 ↗
22. Skalny · 2002
23. Waste E-glass particles used in cementitious mixtures10.1016/j.cemconres.2005.12.010 ↗
24. Feasibility of using recycled glass in architectural cement mortars10.1016/j.cemconcomp.2011.05.006 ↗
25. Properties of architectural mortar prepared with recycled glass with different particle sizes10.1016/j.matdes.2011.01.011 ↗
26. IS 1489, Portland Pozzolana Cement-Specification Part 1 Fly Ash Based, Bureau of Indian Standards (New Delhi, India), 1991.
27. ASTM C340-67, 1967. Specification for Portland-Pozzolan Cement. Astm.
28. IS 383, Coarse and Fine Aggregate for Concrete - Specification, Bureau of Indian Standards (New Delhi, India), 2016.
29. IS-4031 (Part V):1988, Methods of physical tests for hydraulic cement-determination of initial and final setting times, Bur. Indian Stand. New Delhi. (1988).
30. IS 516, Method of Tests for Strength of Concrete, Bureau of Indian Standards (New Delhi, India), 1959.
31. ASTM C 642, Standard Test Method for Density, Absorption, and Voids in Hardened Concrete, Annual Book of ASTM Standards (Pennsylvania, USA), 2006. doi:10.1520/C0642-13.5.
32. IS:2386 (Part lll), Method of Test for aggregate for concrete., Bur. Indian Stand. New Delhi. (1963) (Reaffirmed 2002).
33. IS 2386 (Part I), Methods of Test for Aggregates for Concrete Part I Particle Size and Shape, Bureau of Indian Standards (New Delhi, India), 1963.
34. IS 2386 (Part IV), Methods of Test for Aggregates for Concrete Part 4 Mechanical Properties, Bureau of Indian Standards (New Delhi, India), 1963.
35. ASTM C311, 2003. Standard Test Methods for Sampling and Testing Fly Ash or Natural Pozzolans for Use. Glass 04, 1–9. https://doi.org/10.1520/C031110.1520/C0311 ↗
36. IS:2386-7, Methods of Test for Aggregates for Concrete , Part VII : Alkali Aggregate Reactivity, (1963) 8–11.
37. ASTM C138 / C138M – 08. Standard Test Method for Density (Unit Weight), Yield, and Air Content (Gravimetric) of Concrete. 10.1520/C0138_C0138M-08
38. IS:1199, 1959. Methods of Sampling and Analysis of Concrete. Bureau of Indian Standards, New Delhi.
39. ASTM C39 / C39M – 18. Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens. 10.1520/C0039_C0039M-18
40. Standard Test Methods for Chemical Resistance of Mortars
41. Studies on mechanical properties of concrete containing waste glass aggregate10.1016/j.cemconres.2004.02.006 ↗
42. Bulk engineering and durability properties of washed glass sand concrete10.1016/j.conbuildmat.2008.05.022 ↗
43. A study of the effects of LCD glass sand on the properties of concrete10.1016/j.wasman.2008.03.005 ↗
44. Olmstead · Converting portions of the Los Angeles outfall sewer into a septic tank · 1990
45. Evaluation of sulfate resistance of concrete with recycled and natural aggregates10.1016/j.conbuildmat.2017.06.161 ↗
46. Observation of phase transformations in cement during hydration10.1016/j.conbuildmat.2015.10.027 ↗