journal article·2011-03

Influence of fly ash and silica fume on the consistency retention and compressive strength of concrete subjected to prolonged agitating

Şakir Erdoğdu, Caner Arslantürk, Şirin Kurbetci

Publisher page

Abstract

Abstract Good workability at construction site is essential for high quality concrete since concretes of bad workability are prone to yield low strength and poor durability properties since placement and consolidation procedures cannot be performed properly. Nevertheless, this is what usually encountered in practice because slump loss is indispensable particularly when long delivery times are the case. This would be more pronounced when mineral additives are incorporated into the concretes. In this study, concretes of C25/30 class with fly ash and silica fume were produced and slumps were measured with time elapsed. At the end of each agitating period, the slumps of the mixtures were restored to the initial slumps using a superplasticizer and specimens were thereafter prepared for strength measurement. The effectiveness of using fly ash and silica fume in concrete in relation with slump loss was sought by determining the amount of superplasticizer used. Regardless of the mixture recipe, it can be concluded that as the total amount of cementitious materials increases in the concrete mix of the same initial slump, the slump loss with the elapsed time decreases.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Concrete and Cement Materials Research · Innovative concrete reinforcement materials · Construction Engineering and Safety

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. Slump loss, compressive strength of concrete made with WRR and HRWR admixtures and subjected to prolonged agitating10.1016/0008-8846(94)90159-7 ↗
2. Concrete slump loss
3. Hot weather concreting with admixtures10.1016/S0958-9465(98)80005-X ↗
4. Influence of superplasticizer type and dosage on the slump of Portland cement mortars-Part II10.1016/S0008-8846(02)00838-4 ↗
5. Concrete mixture design for hot weather: experimental and statistical analyses10.1680/macr.1998.50.2.95 ↗
6. Retempering of prolonged-mixed concrete with admixtures in hot weather
7. Theory of concrete slump loss as related to the use of chemical admixtures
8. Slump retention of fly ash concrete with and without chemical admixtures
9. Effect of chemical admixtures on workability and strength properties of prolonged agitated concrete10.1016/S0008-8846(98)00029-5 ↗
10. Effect of retempering on the compressive strength of ready-mixed concrete in hot-dry environments10.1016/j.cemconcomp.2006.08.007 ↗
11. Effect of retempering on consistency and compressive strength of concrete subjected to prolonged agitating10.1016/S0008-8846(01)00699-8 ↗
12. Effect of retempering with superplasticizer admixtures on slump loss and compressive strength of concrete subjected to prolonged agitating10.1016/j.cemconres.2004.08.020 ↗
13. The superplasticizer adsorption capacity of cement pastes, pore solution, and parameters affecting flow loss10.1016/0008-8846(95)00137-2 ↗
14. Interaction between cement and chemical admixture from the point of cement hydration, absorption behaviour of admixture, and paste rheology10.1016/S0008-8846(99)00004-6 ↗
15. Influence of prolonged agitation on water movement related properties of water reducer and retarder admixture concretes10.1016/S0008-8846(97)00054-9 ↗
16. Effect of prolonged agitating on compressive strength of concrete with and without fly ash and/or chemical admixtures
17. Influence of silica fume on the workability and the compressive strength of high-performance concretes10.1016/S0008-8846(98)00010-6 ↗
18. ACI Committee 226.3R-87, Use of fly ash in concrete. ACI, Detroit; 1990.
19. Efficiency of silica fume in concrete10.1016/0008-8846(95)00120-2 ↗
20. ACI Committee 226, Silica fume in concrete. ACI Mater J 1987;158–66.
21. Dissolution rate of silica fume in very high strength concrete10.1016/0008-8846(87)90132-3 ↗
22. High strength concrete containing natural pozzolan and silica fume10.1016/S0958-9465(00)00037-8 ↗
23. Neville · 1986