Abstract It would make sense to detect the rules and mechanisms of degradation and mass transport of alkali-activated slag concrete (AASC) in actual service environment. In this paper, hydration products characterization implies higher crystallinity degree of C-S-H activated by NaOH and higher polymerization of the one activated by water glass. During compressive loading, Poisson's ratio of AASC keeps constant at the stress level ranging from 0 to 0.5, with an uprush takes place at stress level of 0.8–0.9. For slag concrete activated by NaOH, volume increases with stress level, while the volume of slag concrete activated by water glass decreases first and then increase with stress level. The apparent chloride diffusion coefficient of specimens activated by NaOH is 4–7 times smaller than the ones activated by water glass, which is verified by the results that volume of pores above 10 μm of water glass activated sample is nearly 20 times more than that of NaOH activated one. Slag concrete activated by water glass is compacted considerably by compressive loading contributing to the decrease in chloride diffusivity, while no significant compacting phenomenon is observed in slag concrete activated by NaOH. However, there is no significant compacting effect on capillary absorption for both specimens activated by two activators.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete and Cement Materials Research · Innovative concrete reinforcement materials · Magnesium Oxide Properties and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. Engineering and durability properties of concretes based on alkali-activated granulated blast furnace slag/metakaolin blends10.1016/j.conbuildmat.2012.01.017 ↗
2. Durability of concrete incorporating GGBS activated by water-glass10.1016/j.conbuildmat.2007.07.023 ↗
3. Effects of sodium hydroxide and sodium silicate solutions on compressive and shear bond strengths of FA–GBFS geopolymer10.1016/j.conbuildmat.2015.05.001 ↗
4. Effect of water–binder ratio on the mechanical properties of calcium hydroxide-based alkali-activated slag concrete10.1016/j.conbuildmat.2011.10.062 ↗
5. Predicting the remaining service life of land concrete by steel corrosion10.1016/S0008-8846(02)01034-7 ↗
6. Microcracking and chloride permeability of concrete under uniaxial compression10.1016/S0958-9465(00)00029-9 ↗
7. Effect of axial compressive damage on gas permeability of ordinary and high-performance concrete10.1016/S0008-8846(01)00546-4 ↗
8. Effect of uniaxial compressive loading on gas permeability and chloride diffusion coefficient of concrete and their relationship10.1016/j.cemconres.2013.05.013 ↗
9. The effect of mechanical stress on permeability of concrete: a review10.1016/j.cemconcomp.2009.02.003 ↗
10. Chloride penetration into concrete after uniaxial compression
11. Effects and interactions of temperature and stress-level related damage on permeability of concrete10.1016/j.cemconres.2006.09.015 ↗
12. Permeability of stressed concrete and role of fiber reinforcement
13. Permeability of stressed concrete10.1080/09613219108727156 ↗
14. Modification of phase evolution in alkali-activated blast furnace slag by the incorporation of fly ash10.1016/j.cemconcomp.2013.09.006 ↗
15. The evolution of strength and crystalline phases for alkali-activated ground blast furnace slag and fly ash-based geopolymers10.1016/j.cemconres.2009.10.010 ↗
16. Mechanical property and structure of alkali-activated fly ash and slag blends10.1080/21650373.2012.752621 ↗
17. X-ray microtomography shows pore structure and tortuosity in alkali-activated binders10.1016/j.cemconres.2012.03.004 ↗
18. Drying and autogenous shrinkage of pastes and mortars with activated slag cement10.1016/j.cemconres.2007.11.002 ↗
19. Effects of dosage and modulus of water glass on early hydration of alkali–slag cements10.1016/S0008-8846(01)00717-7 ↗
20. Effect of activator mix on the hydration and strength behaviour of alkali-activated slag cements10.1680/adcr.2003.15.3.129 ↗
21. Effects of activator characteristics on the reaction product formation in slag binders activated using alkali silicate powder and NaOH10.1016/j.cemconcomp.2012.03.006 ↗
22. Influence of activator on the strength and drying shrinkage of alkali-activated slag mortar10.1016/j.conbuildmat.2007.10.011 ↗
23. Strength, pore structure and permeability of alkali-activated slag mortars10.1016/S0008-8846(96)00174-3 ↗
24. Influence of activator type on hydration kinetics, hydrate assemblage and microstructural development of alkali activated blast-furnace slags10.1016/j.cemconres.2010.11.016 ↗
25. A model for the C-A-S-H gel formed in alkali-activated slag cements10.1016/j.jeurceramsoc.2011.04.036 ↗
26. Effect of interface elastic modulus on damage mechanism of the fiber reinforced concrete10.4028/www.scientific.net/AMR.450-451.1562 ↗
27. Elastic modulus of prestressed concrete beam based on damage mechanics
28. DTA-TGA and FTIR spectroscopies of sol-gel hydrotalcites: aluminum source effect on physicochemical properties10.1016/S0167-577X(96)00296-0 ↗
29. A new method for microcrack evaluation in concrete under compression10.1007/BF02472225 ↗
30. Durability assessment of alkali activated slag (AAS) concrete10.1617/s11527-012-9842-1 ↗
31. Effects of type and dosage of alkaline activator and temperature on the properties of alkali-activated slag mixtures10.1016/j.conbuildmat.2006.07.002 ↗
32. Effects of dosage of alkali-activated solution and curing conditions on the properties and durability of alkali-activated slag concrete10.1016/j.conbuildmat.2012.04.005 ↗
33. Sodium silicate-based, alkali-activated slag mortars: Part I. Strength, hydration and microstructure10.1016/S0008-8846(02)00717-2 ↗
34. Microstructure development of alkali-activated fly ash cement: a descriptive model10.1016/j.cemconres.2004.08.021 ↗
35. The role of hydrotalcite in chloride binding and corrosion protection in concretes with ground granulated blast furnace slag10.1016/j.cemconcomp.2012.04.009 ↗
36. The capillary of concrete
37. Influence of fly ash on the water and chloride permeability of alkali-activated slag mortars and concretes10.1016/j.conbuildmat.2013.07.106 ↗
38. Durability of alkali-activated fly ash concrete: chloride penetration in pastes and mortars10.1016/j.conbuildmat.2014.04.110 ↗
39. Shrinkage characteristics of alkali-activated fly ash/slag paste and mortar at early ages10.1016/j.cemconcomp.2014.07.007 ↗
40. Residual strength and pore structure of high-strength concrete and normal strength concrete after exposure to high temperatures10.1016/S0958-9465(98)00034-1 ↗
41. Pore structure and chloride permeability of concrete containing nano-particles for pavement10.1016/j.conbuildmat.2010.07.032 ↗