Abstract The partial replacement of Portland cement with supplementary cementing materials (SCMs) is known to improve concrete’s resistance to external sulfate attack. However, an increase in thaumasite formation has been observed in Portland cements with interground limestone. The effects of varying SCM and limestone replacement levels on the severity of external sulfate attack in moderate-C 3 A and high-C 3 A Portland cements in 5 °C and 23 °C Na 2 SO 4 solution are studied. The partial replacement of Portland cement with SCMs greatly enhances the resistance to external sulfate attack, including thaumasite sulfate attack. The rate of deterioration is strongly correlated to SCM content, C 3 A content, and temperature.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete and Cement Materials Research · Building materials and conservation · Magnesium Oxide Properties and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. Effect of ettringite on thaumasite formation10.1016/j.cemconres.2005.11.006 ↗
2. Thaumasite formation in Portland-limestone cement pastes10.1016/S0008-8846(99)00100-3 ↗
3. Physical and microstructural aspects of sulfate attack on ordinary and limestone blended Portland cements10.1016/j.cemconres.2009.08.005 ↗
4. Sulfate attack on cementitious materials containing limestone filler – a review10.1016/j.cemconres.2008.11.007 ↗
5. Thaumasite sulfate attack in Portland and Portland-limestone cement mortars exposed to sulfate solution10.1016/j.conbuildmat.2012.09.104 ↗
6. Use of mineral admixtures to improve the resistance of limestone cement concrete against thaumasite sulfate attack10.1016/j.cemconcomp.2013.01.007 ↗
7. Effect of large amounts of natural pozzolan addition on properties of blended cements10.1016/j.cemconres.2004.07.022 ↗
8. Sulfate attack on concrete with mineral admixtures10.1016/0008-8846(95)00195-6 ↗
9. Sodium sulfate attack on plain and blended cements10.1016/j.buildenv.2005.11.015 ↗
10. Use of mineral admixtures for enhanced resistance against sulfate attack10.1016/j.conbuildmat.2011.03.036 ↗
11. Determination of cement hydration and pozzolanic reaction extents for fly-ash cement pastes10.1016/j.conbuildmat.2011.07.007 ↗
12. The reaction of fly ash in concrete. A critical examination10.1016/0008-8846(89)90088-4 ↗
13. Prevention of thaumasite formation in concrete exposed to sulphate attack10.1016/j.cemconres.2007.04.007 ↗
14. Hydration of tricalcium aluminate (C3A) in the presence and absence of gypsum – studied by Raman spectroscopy and X-Ray diffraction10.1039/b509904h ↗
15. Studies on the carboaluminate formation in limestone filler-blended cements10.1016/S0008-8846(01)00491-4 ↗
16. Mechanism of sulfate attack on Portland cement concrete – another look10.1016/0008-8846(83)90040-6 ↗
17. The effect of cement composition and pH of environment of sulfate resistance of Portland cements and blended cements10.1016/S0958-9465(97)00011-5 ↗
18. The effect of C3A content on sulfate durability of Portland limestone cement mortars10.1016/j.conbuildmat.2012.04.091 ↗
19. CSA A3001-13. Cementitous materials for use in concrete; Portland cement – chemical requirements. Canadian Standards Association (CSA). CSA A3000 Cementitious Materials Compendium; 2013.
20. Does gypsum formation during sulfate attack on concrete lead to expansion?10.1016/S0008-8846(99)00211-2 ↗
21. The pore structure of cement paste blended with fly ash10.1016/j.conbuildmat.2013.04.012 ↗
22. Microstructure and durability of mortars modified with medium active blast furnace slag10.1016/j.conbuildmat.2010.06.077 ↗
23. Supplementary cementitious materials10.1016/j.cemconres.2010.12.001 ↗
24. Synergy between fly ash and limestone powder in ternary cements10.1016/j.cemconcomp.2010.09.006 ↗
25. A thermodynamic and experimental study of the conditions of thaumasite formation10.1016/j.cemconres.2007.11.003 ↗
26. CSA A3004-08. Test methods and standard practices for cementitious materials for use in concrete and masonry; A3004–C8 Test method for determination of expansion of blended hydraulic cement mortar bars due to external sulphate attack. Canadian Standards Association (CSA). CSA A3000 Cementitious Materials Compendium; 2008.
27. CSA A3001-13. Cementitous Materials for use in Concrete; Blended hydraulic cement and blended supplementary cementing materials proportions. Canadian Standards Association (CSA). CSA A3000 Cementitious Materials Compendium; 2013.
28. Compressive strength and sulfate resistance properties of concretes containing Class F and Class C fly ashes10.1016/j.conbuildmat.2012.02.023 ↗
29. Investigation into the synergistic effects in ternary cementitious systems containing Portland cement, fly ash and silica fume10.1016/j.cemconcomp.2011.11.014 ↗
30. Modelling of calcium sulphate solubility in concentrated multi-component sulphate solutions10.1016/j.fluid.2007.07.069 ↗
31. Gypsum: a review of its role in the deterioration of building materials10.1007/s00254-006-0566-9 ↗
32. Solubility of ettringite (Ca6[Al(OH)6]2(SO4)3∗26H2O) at 5–75C10.1016/S0016-7037(99)00078-2 ↗
33. Modeling the effects of solution temperature and concentration during sulfate attack on cement mortars10.1016/S0008-8846(01)00727-X ↗
34. The effect of temperature on thaumasite formation10.1016/j.cemconcomp.2008.09.004 ↗
35. The effect of temperature on the hydration of composite cements containing limestone powder and fly ash10.1617/s11527-011-9819-5 ↗
36. Reactivity of blast-furnace slag in Portland cement blends hydrated under different conditions10.1016/S0008-8846(01)00587-7 ↗
37. Sulfate resistance of Portland-limestone cements in combination with supplementary cementing materials10.1617/s11527-012-9953-8 ↗
38. Durability of concrete – degradation phenomena involving detrimental chemical reactions10.1016/j.cemconres.2007.09.015 ↗
39. Degree of hydration and gel/space ratio of high-volume fly ash/cement systems10.1016/S0008-8846(00)00213-1 ↗
40. Modeling the hydration of concrete incorporating fly ash or slag10.1016/j.cemconres.2010.03.001 ↗
41. The effects of blast-furnace slag and fly ash on the hydration of Portland cement10.1016/0008-8846(91)90090-5 ↗