journal article·2008-10

Cement-lateritic gravels mixtures: Microstructure and strength characteristics

Younoussa Millogo, Mohamed Hajjaji, Raguilnaba Ouedraogo, Moussa Gomina

Publisher page

Abstract

Abstract Microstructure of cement-lateritic gravels mixes, containing up to 8 wt% cement, was investigated by means of X-ray diffraction, infrared spectrometry, differential thermal analysis, scanning electron microscopy and energy dispersive spectrometry. Also, strength characteristics of the mixtures were measured. The results show that cement admixtures resulted in the formation of 1.4 nm-tobermorite, ettringite, iron oxyhydroxide, portlandite and calcite. The increasing amount of tobermorite, due to the increase of the cement content, was attended with a noticeable reduction of particles segregation. In addition, its marked crystallization, observed for the high curing time (28 days), contributed to the improvement of the mechanical strength. As regards the application aspect, the results show that cement amended lateritic gravels are convenient for base course construction.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Concrete and Cement Materials Research · Geotechnical and construction materials studies · Grouting, Rheology, and Soil Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Gidigasu · 1976
2. Messou M. Comportement mécanique d’une couche de base en graveleux latéritiques améliorés au ciment : cas des routes en Côte d’Ivoire. Thèse de Doct-Ing en Génie Civil à l’ Ecole Nationale des Ponts et Chaussées, Paris; 1980.
3. Utilisation des graveleux latéritiques en technique routière
4. Tockol I, Massiéra M, Chiasson PA, Maiga MS. Les graveleux latéritiques dans les pays du sahel: Cas des routes non revêtues. 7éme Congrès International de AIGI, Rotterdam, Holland; 1994.
5. Lime treatment of laterite soils and gravels-revisited10.1016/0950-0618(95)00030-J ↗
6. Autret P. Latérites et graveleux latéritiques. Laboratoire Central des Ponts et Chaussées, France; 1983.
7. The effect of repeated loading on the ultimate unconfined compressive strength of a lime stabilized laterite10.1016/0013-7952(86)90034-7 ↗
8. Stabilization effect of locally produced lime on selected lateritic soils10.1016/0950-0618(90)90006-M ↗
9. Lime modification of problem laterite10.1016/0013-7952(91)90040-R ↗
10. A comparative evaluation of cement and lime modification of laterite10.1016/0013-7952(95)00067-4 ↗
11. Use of lateritic soils for road construction in north Dahomey10.1016/0013-7952(73)90031-8 ↗
12. Millogo Y, Traoré K, Ouedraogo R, Kaboré K, Blanchart P, Thomassin JH. Geotechnical, mechanical, chemical and mineralogical characterization of lateritic gravels of Sapouy (Burkina Faso) used in road construction. Construct Build Mater, in press, doi:10.1016/j.conbuildmat.2006.07.014.10.1016/j.conbuildmat.2006.07.014 ↗
13. NF P94-051, Détermination des limites d’Atterberg; Mars 1993.
14. NF EN P933-9, Essais pour déterminer les caractéristiques géométriques des granulats. Essai au bleu de méthylène; Août 1999.
15. NF P94-093, Détermination des références de compactage d’un matériau; Octobre 1999.
16. NF P94-078, Indice CBR après immersion- Indice CBR immédiat- Indice Portant Immédiat; Décembre 1992.
17. NF P18-560, Analyse granulométrique par tamisage; Octobre 1978.
18. NF P94-057, Analyse granulométrique des sols, Méthode par sédimentation; Mai 1992.
19. NF P18-406, Bétons – Essai de compression; Décembre1981.
20. NF P18-408, Bétons – Essai de fendage; Décembre 1981.
21. The effect of high curing temperature on the kinetics in MK/lime and MK-bended cement matrices at 60°C10.1016/S0008-8846(02)01040-2 ↗
22. Influence of silica fume on the properties of fired then water cured lime-rich clay bricks
23. Stabilisation of clayey soils with high calcium fly as hand cement10.1016/j.cemconcomp.2004.02.019 ↗
24. Compositional changes in lime-based mortars exposed to different environments10.1016/j.tca.2005.03.015 ↗
25. Hydratation of portland cement clinker in the presence of carbonaceous material10.1016/0008-8846(95)00104-K ↗
26. Structure of calcium silicate hydrate (C–S–H): near-, mid-, and far-infrared spectroscopy10.1111/j.1151-2916.1999.tb01826.x ↗
27. Journées Ouvrages d’Art du Réseau des L.P.C., Lyon; 13 Avril 2005.
28. Hydrogarnet formation during autoclaving at 180°C in unstirred metakaolin-lime-quartz slurries10.1016/S0008-8846(98)00088-X ↗
29. Microstructural investigation of a silica fume-cement-lime mortar10.1016/S0958-9465(02)00006-9 ↗
30. Interaction of silica fume with calcium hydroxide solutions and hydrated cement pastes10.1016/S0008-8846(98)00133-1 ↗
31. Viallis-Terrisse H. Interaction des silicates de calcium hydratés, principaux constituants du ciment, avec les chlorures d’alcalins. Analogie avec les argiles. Thèse de Doctorat de l’Université de Bourgogne (France), UF des Sciences et Techniques; 2000.