Abstract

Although the use of slag has many advantages, the low hydration of slag at early age causes the strength to be low. Hence, its uses are restricted, and should be activated. In this investigation, a mechanical method was used to activate ordinary Portland cement (OPC)-slag mortars (OSM). Fourteen OSMs were made, two of them as control. Three groups of mortars were used. The first group includes both the ground slag and OPC. In the second group ground slag and ungrounded OPC were used, and in the third group ground OPC and ungrounded slag used. For the first group, 7- and 28-day strengths were attained as 65 and 80 MPa, respectively. Finally, the results showed that the optimum strengths attributed to the first group, especially at early ages. All the mix proportions were made for water-binder and sand-binder ratios as 0.33 and 2.25, with 50% level of slag, respectively.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Concrete and Cement Materials Research · Innovative concrete reinforcement materials · Innovations in Concrete and Construction Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. Interrelation between fine grinding and mechanical activation10.1016/0301-7516(95)00028-3 ↗
2. Juhasz · 1994
3. Mittal · 1996
4. Blended cements-manufacturing process technologies
5. Influence of curing temperature on cement hydration and mechanical strength development of fly ash mortars10.1016/S0008-8846(97)00098-7 ↗
6. Davidovits · 1994
7. Mechanical activation of solid and its application in technology
8. Improved processing of blended slag cement through mechanical activation10.1023/B:JMSC.0000026948.85440.cc ↗
9. Finish grinding of slag
10. The action of alkalis on blast-furnace slag
11. Investigation of mechanical properties and structure of alkali activated blast-furnace slag mortars
12. Some properties of alkali-activated slag cements
13. Investigation of hydraulic activity of ground granulated blast furnace slag in concrete10.1016/S0008-8846(03)00062-0 ↗
14. Effect of temperature and aging on the mechanical properties of concrete, part II Prediction model10.1016/S0008-8846(02)00745-7 ↗
15. The effect of particle size distribution on the properties of blended cements incorporating GGBFS and natural pozzolan (NP)10.1016/j.powtec.2007.03.033 ↗
16. Mechanochemical activation of calcium oxide powder10.1016/0032-5910(96)03094-X ↗
17. Neville · 2008
18. Neville · 2008
19. Optimum level of replacement slag in OPC–slag mortars
20. Tungsten mine waste geopolymeric binder: preliminary hydration products investigations10.1016/j.conbuildmat.2008.01.003 ↗
21. The coexistence of geopolymeric gel and calcium silicate hydrates at the early stage of alkaline activation10.1016/j.cemconres.2004.10.042 ↗
22. Microanalysis of calcium silicate hydrate gel formed within a geopolymeric binder10.1023/A:1025904905176 ↗
23. Investigations on mix design of tungsten mine waste geopolymeric binder10.1016/j.conbuildmat.2007.07.015 ↗
24. Investigations about the effect of aggregates on strength and microstructure of geopolymeric mine waste mud binders10.1016/j.cemconres.2007.02.006 ↗
25. Activated fly ash/slag blended cement10.1016/j.resconrec.2007.04.002 ↗
26. Higginson EC. The effect of cement fineness on concrete. Fineness of cement, ASTM STP 473; 1970. p. 71–81.10.1520/STP28620S ↗
27. Li Ying, Yang Jing. Influence of particle size distribution on microstructure and strength of cement gel. New Build Mater 2004(3):1–4 [in Chinese].
28. Francois Garcia, Nadine Le Bolay, Jean-Luc Trompette, Christin Frances. On fragmentation and agglomeration phenomena in an ultra fine wet grinding process: the role of polyelectrolyte additives. Int J Miner Process 2004; 74S (S1): S43-S54.10.1016/j.minpro.2004.07.001 ↗