Cooperative action and compatibility between Portland cement and MSWI bottom ash alkali-activated double gel system materials
Source abstract
Abstract
Abstract This study investigated the cooperative action and compatibility between Portland cement and municipal solid waste incineration (MSWI) bottom ash alkali-activated double gel system materials, focusing on the two different methods of mixed casting and layered casting. The results show that alkali-activated materials and Portland cement have a severe incompatibility problem when mixed casting is used. However, layered casting completely solves this compatibility problem in double gelled system materials. This is because liquid sodium silicate accelerates the initial setting time in alkali-activated materials and thus eliminates the influence between polymerization and hydration. Furthermore, alkali-activated materials can compensate for the lack of calcium by absorbing the Ca(OH)2 generated by the hydration of Portland cement. In this case, Calcium-Silicate-Hydrate (C-S-H) and Aluminium-Modified Calcium-Silicate-Hydrate (C-A-S-H) gels are formed, which strengthens the interface transition zone.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete and Cement Materials Research · Recycling and utilization of industrial and municipal waste in materials production · Magnesium Oxide Properties and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (56)
Show source-provided references
1. Mechanisms of cement hydration10.1016/j.cemconres.2010.09.011 ↗
2. Ki Bong Park, Analysis of the compressive strength development of concrete considering the interactions between hydration and drying10.1016/j.cemconres.2017.08.010 ↗
3. Interaction of silicate and aluminate reaction in a synthetic cement system: Implications for the process of alite hydration10.1016/j.cemconres.2016.12.006 ↗
4. Utilization of municipal solid waste incineration (MSWI) fly ash in blended cement, Part 1: Processing and characterization of MSWI fly ash10.1016/j.jhazmat.2005.12.041 ↗
5. Utilization of municipal solid waste incineration (MSWI) fly ash in blended cement, Part 2. Mechanical strength of mortars and environmental impact10.1016/j.jhazmat.2006.11.044 ↗
6. Biotoxicity evaluation of fly ash and bottom ash from different municipal solid waste incinerators10.1016/j.jhazmat.2009.02.023 ↗
7. Characteristics and application potential of municipal solid waste incineration (MSWI) bottom ashes from two waste-to-energy plants10.1016/j.conbuildmat.2015.02.033 ↗
8. Advances in understanding alkali-activated materials10.1016/j.cemconres.2015.04.013 ↗
9. New cements for the 21st century: the pursuit of an alternative to Portland cement10.1016/j.cemconres.2011.03.016 ↗
10. Durability of alkali-activated materials in aggressive environments: a review on recent studies10.1016/j.conbuildmat.2017.07.027 ↗
11. One-part alkali-activated materials: a review10.1016/j.cemconres.2017.10.001 ↗
12. Alkali-activated slag concrete: Fresh and hardened behavior10.1016/j.cemconcomp.2017.10.003 ↗
13. The role of inorganic polymer technology in the development of green concrete10.1016/j.cemconres.2007.08.018 ↗
14. Accelerated carbonation testing of alkali-activated binders significantly underestimates service life: The role of pore solution chemistry10.1016/j.cemconres.2012.07.002 ↗
15. Effect of silicate modulus and metakaolin incorporation on the carbonation of alkali silicate-activated slags10.1016/j.cemconres.2010.02.003 ↗
16. Effect of the hydration temperature on the microstructure of Class G cement: C-S-H composition and density10.1016/j.cemconres.2017.02.008 ↗
17. Effects of NaOH concentrations on physical and electrical properties of high calcium fly ash geopolymer paste10.1016/j.cemconcomp.2013.09.012 ↗
18. Effect of alkali activator concentration and curing condition on strength and microstructure of waste clay brick powder-based geopolymer10.1016/j.compositesb.2017.10.013 ↗
19. Quantitative and qualitative assessment of the amorphous phase of a Class F fly ash dissolved during alkali activation reactions-Effect of mechanical activation, solution concentration and temperature10.1016/j.compositesb.2016.08.001 ↗
20. Role of pH on the structure, composition and morphology of C-S-H–PCE nanocomposites and their effect on early strength development of Portland cement10.1016/j.cemconres.2017.09.002 ↗
21. Advances in understanding hydration of Portland cement10.1016/j.cemconres.2015.05.025 ↗
22. The influence of sodium and potassium hydroxide on alite hydration: Experiments and simulations10.1016/j.cemconres.2012.07.003 ↗
23. Effect of alkali content of cement on properties of high performance cementitious mortar10.1016/j.conbuildmat.2015.10.110 ↗
24. Alkali-activated Portland blast-furnace slag cement: Mechanical properties and hydration10.1016/j.conbuildmat.2017.02.092 ↗
25. Portland cement-blast furnace slag mortars activated using waterglass: Effect of temperature and alkali concentration10.1016/j.conbuildmat.2014.04.120 ↗
26. GB/T18046-2008, Ground granulated blast furnace slag used for cement and concrete, 2008.
27. GB 175-2007, Common Portland Cement, 2007.
28. GB/T17671-1999, Method of testing cements--Determination of strength–ISO China, 1999.
29. JGJ/70-2009, Standard for test method of performance building mortar, 2009.
30. GB/T 2419-2005, Test method for fluidity of cement mortar, 1999.
31. Shi · 2006
32. Influence of activator type on hydration kinetics, hydrate assemblage and microstructural development of alkali activated blast-furnace slags10.1016/j.cemconres.2010.11.016 ↗
33. Delvasto, Effect of binder content on the performance of alkali-activated slag concretes10.1016/j.cemconres.2010.08.017 ↗
34. Enhancement in early strengths of slag-cement mortars by adjusting basicity of the slag prepared from fly-ash of MSWI10.1016/j.cemconres.2009.02.005 ↗
35. The mechanical properties of fly ash-based geopolymer concrete with alkaline activators10.1016/j.conbuildmat.2013.05.069 ↗
36. Reaction kinetics, gel character and strength of ambient temperature cured alkali activated slag–fly ash blends10.1016/j.conbuildmat.2015.01.065 ↗
37. Mechanical and microstructural properties of heat cured alkali-activated slag mortars10.1016/j.matdes.2011.10.005 ↗
38. Reactivity and reaction products of alkali-activated, fly ash/slag paste10.1016/j.conbuildmat.2015.02.022 ↗
39. Influence of calcium compounds on the mechanical properties of fly ash geopolymer pastes10.1016/j.jhazmat.2008.12.121 ↗
40. A review: The comparison between alkali-activated slag (Si+Ca) and metakaolin (Si+Al) cements10.1016/j.cemconres.2010.03.020 ↗
41. The mineralogy of the CaO-A12O3-SiO2-H2O (CASH) hydroceramie system from 200 to 350 °C10.1016/j.cemconres.2008.10.002 ↗
42. Influence of SiO2 modification on hydrogarnets formation during hydrothermal synthesis10.1016/S0008-8846(03)00200-X ↗
43. Effect of calciumon dissolution and precipitation reactions of amorphous silica at high alkalinity10.1016/j.cemconres.2016.05.004 ↗
44. Effect of calcium additions on N-A-S-H cementitious gels10.1111/j.1551-2916.2010.03668.x ↗
45. High strength geopolymer using fine high-calcium fly ash10.1061/(ASCE)MT.1943-5533.0000161 ↗
46. The influence of calcium content on the structure and thermal performance of fly ash based geopolymers10.1007/s10853-006-0532-7 ↗
47. Use of slaked lime and Portland cement to improve the resistance of MSWI bottom ash-GBFS geopolymer concrete against carbonation10.1016/j.conbuildmat.2018.01.089 ↗
48. Improving strength of calcinated coal gangue geopolymer mortars via increasing calcium content10.1016/j.conbuildmat.2018.02.005 ↗
49. Carbonation behavior of mortar produced by alkali-activation of a granulated blast furnace slag
50. Accelerated carbonation testing of alkali-activated slag/metakaolin blended concretes: effect of exposure conditions10.1617/s11527-014-0289-4 ↗
51. Bernal, Effect of the activator dose on the compressive strength and accelerated carbonation resistance of alkali silicate-activated slag/metakaolin blended materials10.1016/j.conbuildmat.2015.08.013 ↗
52. Shrinkage mitigation strategies in alkali-activated slag10.1016/j.cemconres.2017.08.025 ↗
53. Shrinkage mechanisms of alkali-activated slag10.1016/j.cemconres.2016.07.001 ↗
54. Effect of activated silica on polymerization mechanism and strength development of MSWI bottom ash alkali-activated mortars10.1016/j.conbuildmat.2018.12.125 ↗
55. The influence of curing methods on the strength of MSWI bottom ash-based alkali-activated mortars: the role of leaching of OH- and free alkali10.1016/j.conbuildmat.2018.07.224 ↗
56. Advances in understanding and analyzing the anti-diffusion behavior in complete carbonation zone of mswi bottom ash-based alkali-activated concrete10.1016/j.conbuildmat.2018.08.038 ↗