Environmental effects on concrete using Ordinary and Pozzolana Portland cement
Source abstract
Abstract
Abstract Wastewater treatment plant consists of pipe lines and lift stations. These plants consist of concrete pipes, manholes, pump stations, interceptors and wet wells. Entire wastewater (WW) system is forced to chemical attack due to the presence of sulphate and acid available in WW. It leads to the damage in the interior wall or structure of a sewer pipe and lift station. A concrete structure when exposed to different environments, the life of the structure is drastically reduced. Main cause of the deterioration is corrosion or erosion. The defective structures are replaced periodically which leads to indirect loss in the national growth. In other words, the failure of these structures may lead to invest more on the repair and rehabilitation. In this study, the strength of the concrete in various environments has been investigated using different techniques such as compressive strength, flexural test, rapid chloride permeability, weight loss measurements, linear polarization and open circuit potential. Microbiological examinations were also analyzed. Two types of cement namely Ordinary Portland Cement (OPC) and Portland Pozzolana Cement (PPC) with one mix ratio were used for complete study. Concrete specimens exposed in three environments namely: normal water (NW Potable water), domestic sewage water (DSW) and textile wastewater (TWW). From the results, it is observed that PPC exposed in different media shows better performance than OPC in both mechanical and electrochemical studies.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Microbial Applications in Construction Materials · Concrete Corrosion and Durability · Concrete and Cement Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. Deterioration of reinforced concrete in sewer environment: a comprehensive review10.1680/muen.2006.159.1.11 ↗
2. The production and utilization of intermediary elemental sulphur during the oxidation of reduced sulphur compounds by Thiobacillus ferro-oxidans10.1007/BF00408252 ↗
3. Biochemistry of the chemolithotrophic oxidation of inorganic Sulfur10.1098/rstb.1982.0094 ↗
4. Interactions of nutrients, moisture, and pH on microbial corrosion of concrete sewer pipes10.1016/0043-1354(92)90107-F ↗
5. Effect of sludge water from ready-mixed concrete plant on properties and durability of concrete10.1016/j.cemconcomp.2006.01.001 ↗
6. Frenay JW, Zilverber H. Durability of concrete in agricultural environments-IMAG-DLO Report 93-17. Wageningen, Netherlands; 1993. p. 93–17.
7. Biogenic sulfuric acid attack on different types of commercially produced concrete sewer pipes10.1016/j.cemconres.2009.10.002 ↗
8. Ceramsite obtained from water and wastewater sludge and its characteristics affected by (Fe2O3+CaO+MgO)/(SiO2+Al2O3)10.1016/j.watres.2009.03.046 ↗
9. Microbial carbonates precipitation in construction materials: a review10.1016/j.ecoleng.2009.02.006 ↗
10. IS: 8112–1989. Specification for 43 grade ordinary Portland cement. Bureau of Indian Standards, New Delhi.
11. IS: 1489 (Part I)–1991. Specification for Portland pozzolana cements (fly ash based). Bureau of Indian standards, New Delhi.
12. ASTM C-876 1994 Standard. Standard Test Method for Half Cell Potentials of Reinforcing Steel in Concrete. West Conshohocken (PA): American Society for Testing and Materials; p. 21.
13. Long term corrosion performance of rebar embedded in blended cement concrete under macro cell corrosion condition10.1016/j.conbuildmat.2006.09.004 ↗
14. ASTM G102-89 2004. Standard practice for calculation of corrosion rates and related information from electrochemical measurements.
15. Limitations of the linear polarization method to determine stainless steel corrosion rate in concrete environment10.1016/j.cemconcomp.2006.01.007 ↗
16. Possibilities and problems of in situ techniques for measuring steel corrosion rates in large reinforced concrete, structures10.1016/j.corsci.2004.04.011 ↗
17. ASTM C1202. Standard test method for electrical indication of concrete’s ability to resist chloride ion penetration; 1997.
18. Evaluation of bagasse ash as supplementary cementitious material10.1016/j.cemconcomp.2007.03.001 ↗
19. Optimum usage of a natural pozzolan for the maximum compressive strength of concrete10.1016/j.cemconres.2004.02.008 ↗
20. Studies on the aspects of chloride ion determination in different types of concrete under macro-cell corrosion conditions10.1016/j.buildenv.2004.10.005 ↗
21. The relationship between charge passed and the chloride-ion concentration in concrete using steady-state chloride migration test10.1016/S0008-8846(01)00662-7 ↗
22. Influence of SO2 deposition on cement mortar hydration10.1016/S0008-8846(98)00183-5 ↗
23. Micro-structural characterization of leaching effects in cement pastes due to neutralization of their alkaline nature Part I: Portland cement pastes10.1016/j.cemconres.2006.10.002 ↗
24. Structure of calcium silicate hydrate (C–S–H): near-, mid-, and far-infrared spectroscopy10.1111/j.1151-2916.1999.tb01826.x ↗
25. Compositional changes in lime-based mortars exposed to different environments10.1016/j.tca.2005.03.015 ↗
26. Micro-FTIR study of the blend of humates with calcium hydroxide used to prepare smokeless fuel briquettes10.1016/S0924-2031(03)00089-4 ↗
27. Nakamoto · 1997
28. Nyquist · 1997
29. John Coates. Interpretation of infrared spectra, A practical approach. Meyers RA, editor. Encyclopedia of analytical chemistry. John Wiley & Sons Ltd.; p. 10815–10837.
30. Standard methods for examination of water & Wastewater. APHA–AWWA–WPCF. 20th ed. American public health association. American water works Association. Water pollution control federation; 2000.
31. Corrosion of biological origin observed on concrete digestors10.1016/S0950-0618(97)00041-X ↗