The effects of shrinkage-reducing admixtures used in self-compacting concrete on its strength and durability
Source abstract
Abstract
Abstract This study explores the effects of shrinkage-reducing admixtures (SRA) used in self-compacting concrete (SCC), a specific type of concrete which is gradually receiving widespread use, yet to be improved to the desired properties and expected to replace traditional concrete in the future, on its strength and durability. In this study, SCC mixtures with and without (reference) different SRA dosages were produced to define the optimum SRA utilization rate in SCC mixtures. After deciding the SRA dosage to be used in mixtures, properties of reference and SRA-added SCC mixtures were evaluated by focusing mainly on the workability, strength and durability properties after subjected to either direct water submersion or cyclic Na2SO4 solution. As a result of the experimental program, it was concluded that the presence of SRA has adverse effects on the mechanical properties of SCC specimens although these effects are not dramatic regardless of the harshness of environmental exposure. The influence of SRA addition on fresh-state properties was also minimal so that the workability of reference and SRA-added SCC mixtures were found to be similar. Occurrence and further development of both drying and restrained shrinkage were substantially restricted with varying rates when SRA was incorporated in SCC mixtures. Overall, this study concludes that with a proper selection of SRA dosage, SCC mixtures performing well even under very hazardous environments can successfully be produced and be taken advantage of without sacrificing much of workability and/or mechanical properties and risking the occurrence and further development of shrinkage-originated cracking.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete Properties and Behavior · Concrete and Cement Materials Research · Innovative concrete reinforcement materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (47)
Show source-provided references
1. Development of self-compacting concrete
2. Shrinkage and creep of SCC–The influence of paste volume and binder composition10.1016/j.conbuildmat.2010.11.019 ↗
3. Curing cement concrete by using shrinkage reducing admixture and curing compound10.1016/j.conbuildmat.2013.07.092 ↗
4. Combined effect of expansive and shrinkage reducing admixtures to control autogenous shrinkage in self-compacting concrete10.1016/j.conbuildmat.2013.11.033 ↗
5. B.J. Pease, The role of shrinkage reducing admixtures on shrinkage, stress development, and cracking. PhD Thesis, Purdue University, 2005.
6. Influence of shrinkage reducing admixtures on distinct SCC mix compositions10.1016/j.conbuildmat.2012.02.033 ↗
7. B. Pendergrass, D Darwin, Low-Cracking High-Performance Concrete (LC-HPC) Bridge Decks: Shrinkage-Reducing Admixtures, Internal Curing, and Cracking Performance. PhD Thesis, University of Kansas, 2014.
8. Interactions between shrinkage reducing admixtures (SRA) and cement paste's pore solution10.1016/j.cemconres.2007.12.005 ↗
9. Influence of shrinkage-reducing admixtures on the reduction of plastic shrinkage cracking in concrete10.1016/j.cemconres.2008.11.011 ↗
10. Combined effect of expansive and shrinkage reducing admixtures to obtain stable and durable mortars10.1016/j.cemconres.2004.11.021 ↗
11. ABC’s of Crackless Bridge Decks with applications in accelerated bridge construction, Sonny Fereira, PE California Department of Transportation March 21,2014, Brigde Contractors / Caltrans Liaison Committee Meeting.
12. Properties of shrinkage-reducing admixture-modified pastes and mortar10.1007/s11527-005-9004-9 ↗
13. New admixture combats concrete shrinkage
14. Shrinkage-reducing admixtures
15. Shoya · 1985
16. Action mechanisms of shrinkage reducing admixture in hardened cement paste
17. Properties of high-performance concrete containing shrinkage-reducing admixture10.1016/S0008-8846(97)00135-X ↗
18. Shrinkage reduction of high strength fiber reinforced cementitious composites (HSFRCC) with various water-to-binder ratios10.1016/j.cemconcomp.2011.03.009 ↗
19. Effects of shrinkage-reducing admixtures on restrained shrinkage cracking of concrete
20. Influence of shrinkage-reducing admixture on drying shrinkage and mechanical properties of high-performance concrete
21. Combined effect of expansive, shrinkage reducing and hydrophobic admixtures for durable self-compacting concrete10.1016/j.conbuildmat.2012.04.129 ↗
22. Effects of shrinkage reducing admixture in shrinkage compensating concrete under non-wet curing conditions10.1016/j.cemconcomp.2004.09.020 ↗
23. Durability of self-consolidating concrete to sulfate attack under combined cyclic environments and flexural loading10.1016/j.cemconres.2008.12.003 ↗
24. Performance of self-compacting concrete containing different mineral admixtures10.1016/j.conbuildmat.2011.04.032 ↗
25. The effects of pozzolanic binders and polypropylene fibers on durability of SCC to magnesium sulfate attack10.1016/j.conbuildmat.2012.08.035 ↗
26. Durability of self-consolidating concrete incorporating high-volume replacement composite cements10.1016/j.cemconres.2004.03.018 ↗
27. Durability of self-consolidating concrete to different exposure regimes of sodium sulfate attack10.1617/s11527-008-9442-2 ↗
28. J. Roncero, R. Gettu, M.A. Martín, Evaluation of the influence of a shrinkage reducing admixture on the microstructure and long-term behavior of concrete, in: V.M. Malhotra (Ed.), Proc. Seventh CANMET/ACI Intnl. Conf. on Superplasticizers and Other Chemical Admixtures in Concrete (Berlin), Supplementary papers, (2003) pp. 207–226.
29. EN, TS. 934-2, Admixtures for Concrete, Mortar and Grout-Part 2: Concrete Admixtures; Definitions, Requirements, Conformity, Marking and Labelling. Turkish Standards Institute, Ankara, 2002.
30. EN, TS. 802, Design of Concrete Mixes. Turkish Standards Institute, Ankara, 2009.
31. ASTM C157/C157M-17, Standard Test Method for Length Change of Hardened Hydraulic-Cement Mortar and Concrete, ASTM International, West Conshohocken, PA, 2017.
32. C. Bibm, E. Ermco, EFNARC, The European Guidelines for Self-Compacting Concrete: Specification, Production and Use, The Self-Compacting Concrete European Project Group, 2005.
33. Influence of shrinkage-reducing admixtures on development of plastic shrinkage cracks
34. P.K. Mehta, Mechanism of sulfate attack on portland cement concrete- Another look, CCR, 13, 1983.10.1016/0008-8846(83)90040-6 ↗
35. The role of ettringite in external sulfate attack, Materials Science of Concrete: Sulfate Attack Mechanisms
36. Some aspects and mechanisms of sulphate attack
37. Self-healing capability of cementitious composites incorporating different supplementary cementitious materials10.1016/j.cemconcomp.2012.08.013 ↗
38. Deflection-hardening hybrid fiber reinforced concrete: The effect of aggregate content10.1016/j.conbuildmat.2016.08.020 ↗
39. High-early-strength ductile cementitious composites with characteristics of low early-age shrinkage for repair of infrastructures10.1617/s11527-013-0241-z ↗
40. Assessing the self-healing capability of cementitious composites under increasing sustained loading10.1680/jadcr.14.00111 ↗
41. Flexural response of steel-fiber-reinforced concrete beams: effects of strength, fiber content, and strain-rate10.1016/j.cemconcomp.2015.10.001 ↗
42. Effect of sulfate on cement mortars containing Li2SO4, LiNO3, Li2CO3 and LiBr10.1016/j.conbuildmat.2017.08.148 ↗
43. Shrinkage cracking of high-strength concrete
44. Long-term behaviour of concrete incorporating a shrinkage-reducing admixture
45. CAN3-A23.3-M84, Design of concrete structures for buildings. Ontario: Canadian Standards Association, 1984.
46. ACI 318, Building code requirements for reinforced concrete. Detroit: American Concrete Institute, 1995.
47. Self-healing performance of aged cementitious composites10.1016/j.cemconcomp.2018.01.004 ↗